Surfacing compositions and methods
Asphalt surfacing compositions and methods involving asphalt millings, water, and an amount of a polyvinyl alcohol sufficient to bind the millings such that a load-bearing asphalt paving surface is formed upon application of the composition to a material are provided.
1. A surfacing composition comprising asphalt waste millings, said waste millings containing crushed rock bound with asphalt, and further including 5%-20% by weight based on the weight of the asphalt waste millings of water and 0.4-1.2 gallons per yd 3 of said asphalt waste millings of a polyvinyl alcohol, wherein the proportion of asphalt waste millings, water, and polyvinyl alcohol is sufficient to bind said waste millings such that a load-bearing asphalt paving surface is formed upon application of the composition to a material in need thereof.
2. The composition of claim 1 , further including 0.75% to 5% by weight, based on the weight of the polyvinyl alcohol of a clay.
3. The composition of claim 2 , wherein said clay comprises a nano clay.
4. The composition of claim 1 , further including 4-10% by weight, based on the weight of the polyvinyl alcohol of a crosslinker.
5. The composition of claim 4 , wherein said crosslinker is selected from the group consisting of a carbamide, boron, and cement.
6. The composition of claim 1 , wherein said composition and said paving surface are formed free of exogenously added heat.