IP Library › Granted Patent US 9,425,091
Granted Patent B2
US 9,425,091 · App. 14/797,234 · Granted Aug 23, 2016

Method for forming semiconductor structure

Inventors: Yi-Nien Su (Hsinchu, TW); Hsiang-Wei Lin (New Taipei, TW)
Assignee: Taiwan Semiconductor Manufacturing Company Limited
H01L21/76877H01L21/768H01L21/7682H01L21/76802H01L21/76819H01L23/528H01L23/5222H01L23/53228H01L23/53295H01L23/5226H01L2924/0002
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 9,425,091
App. No.
14/797,234
Granted
Aug 23, 2016
Kind
B2
Abstract

One or more techniques or systems for forming a semiconductor structure having a gap are provided herein. In some embodiments, a gap is formed between a first etch stop layer (ESL) and an ESL seal region. For example, the gap is formed by removing a portion of a low-k (LK) dielectric region above an oxide region and removing the oxide region. In some embodiments, the oxide region below the LK dielectric region facilitates removal of the LK dielectric region, at least because the oxide region enhances a bottom etch rate of a bottom of the LK dielectric region such that the bottom etch rate is similar to a wall etch rate of a wall of the LK dielectric region.

Claims (68)

1. A method for forming a semiconductor structure, comprising:

forming a first etch stop layer (ESL);

forming an oxide region above the first ESL;

forming a low-k (LK) dielectric region above the oxide region;

forming a first metal line through at least one of the first ESL, the oxide region, or the LK dielectric region;

forming a second metal line through at least one of the first ESL, the oxide region, or the LK dielectric region;

forming a second ESL over at least one of the first metal line, the second metal line, or the LK dielectric region;

removing at least a portion of the second ESL at least one of:

over at least one of the first metal line or the second metal line; or

between the first metal line and the second metal line;

forming a gap by removing at least one of:

at least a portion of the oxide region between the first metal line and the second metal line; or

at least a portion of the LK dielectric region between the first metal line and the second metal line; and

forming an ESL seal region over at least one of the second ESL, the first metal line, the second metal line, or the gap.

2. The method of claim 1 , forming the first metal line comprising performing chemical-mechanical planarization (CMP) on at least one of the LK dielectric region or the first metal line.

3. The method of claim 1 , forming the second metal line comprising performing chemical-mechanical planarization (CMP) on at least one of the LK dielectric region or the second metal line.

4. The method of claim 1 , comprising removing at least a portion of the second ESL based on photo resist (PR) patterning.

5. The method of claim 1 , comprising forming the first metal line of copper.

6. The method of claim 1 , comprising forming the second metal line of copper.

7. The method of claim 1 , comprising forming the first ESL of a dielectric material.

8. The method of claim 1 , comprising forming the second ESL of a dielectric material.

9. The method of claim 1 , comprising forming a third metal line between the first metal line and the second metal line.

10. A method for forming a semiconductor structure, comprising:

forming a first etch stop layer (ESL);

forming an oxide region above the first ESL;

forming a low-k (LK) dielectric region above the oxide region;

forming a hard mask (HM) region above the LK dielectric region;

patterning the HM region;

etching at least one of a first trench, a second trench, or a contact space based on the patterned HM region:

the first trench formed through at least one of the first ESL, the oxide region, or the LK dielectric region;

the second trench formed through at least one of the first ESL, the oxide region, or the LK dielectric region; or

the contact space formed through at least one of the first ESL, the oxide region, the LK dielectric region, or one or more additional regions;

forming a first metal line by filling the first trench with metal;

forming a second metal line by filling the second trench with metal;

forming a via by filling the contact space with metal;

forming a second ESL over at least one of the first metal line, the second metal line, the via, or the LK dielectric region;

removing at least a portion of the second ESL at least one of:

over at least one of the first metal line or the second metal line; or

between the first metal line and the second metal line;

forming a gap by removing at least one of:

at least a portion of the oxide region between the first metal line and the second metal line; or

at least a portion of the LK dielectric region between the first metal line and the second metal line; and

forming an ESL seal region over at least one of the second ESL, the first metal line, the second metal line, the via, or the gap.

11. The method of claim 10 , comprising removing the patterned HM region prior to the forming a second ESL.

12. The method of claim 11 , the removing the patterned HM region comprising planarizing a top surface of the semiconductor structure.

13. The method of claim 10 , the forming an ESL seal region comprising forming the ESL seal region to contact the first metal line and the second metal line.

14. The method of claim 10 , comprising:

removing a portion of the ESL seal region over the via; and

removing a second portion of the second ESL over the via to form a second contact space over the via.

15. The method of claim 14 , comprising filling the second contact space with metal.

16. The method of claim 14 , the removing a second portion of the second ESL comprising removing the second portion of the second ESL after forming the ESL seal region.

17. A method for forming a semiconductor structure, comprising:

forming a first etch stop layer (ESL);

forming an oxide region above the first ESL;

forming a dielectric region above the oxide region;

etching the first ESL, the oxide region, and the dielectric region to form a first trench and a second trench;

forming a first metal line in the first trench;

forming a second metal line in the second trench;

forming a second ESL over the first metal line, the second metal line, and the dielectric region;

removing a portion of the second ESL between the first metal line and the second metal line;

removing a portion of the oxide region and a portion of the dielectric region between the first metal line and the second metal line to form a gap; and

forming an ESL seal region over the first metal line, the second metal line, and the gap.

18. The method of claim 17 , the removing a portion of the second ESL comprising exposing at least a portion of a top surface of the first metal line and a portion of a top surface of the second metal line.

19. The method of claim 18 , the forming an ESL seal region comprising forming the ESL seal region to contact at least a portion of a top surface of the second ESL, the portion of the top surface of the first metal line, and the portion of the top surface of the second metal line.

20. The method of claim 17 , comprising:

removing a portion of the ESL seal region;

removing a second portion of the second ESL to form a contact space; and

filling the contact space with metal.