IP Library Granted Patent US 9,505,083
Granted Patent B2
US 9,505,083 · App. 14/897,843 · Granted Nov 29, 2016

Method for producing a node by welding with the same width for two welds

Inventors: Sabastian Ruhl (Wetter, DE); Heiko Strobel (Munzenberg, DE); Tim Hanika (Langgoens/Oberkleen, DE)
Assignee: SCHUNK SONOSYSTEMS GMBH
B23K20/10B23K20/2333B23K2201/32B23K2203/10B23K2203/12B23K2203/18
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 9,505,083
App. No.
14/897,843
Granted
Nov 29, 2016
Kind
B2
Abstract

The invention relates to a method for producing a node by welding at least one first stranded wire comprising individual wires to at least one second stranded wire comprising individual wires, the stranded wires being of different materials, in a compression chamber with adjustable height and width of an ultrasonic welding device, the width being adjusted by means of at least one lateral slide and the height by changing the distance between a sonotrode and a counter electrode of the ultrasonic welding device, the at least one first stranded wire being welded with a higher specific energy, under a higher pressure or with a greater ultrasonic vibration amplitude than the at least one second stranded.

Claims (27)

1. A method for producing a node by welding at least one first stranded wire ( 144 ) comprising individual wires to at least one second stranded wire ( 148 ) comprising individual wires, the stranded wires being of different materials, in a compression chamber ( 122 ) with adjustable height and width of an ultrasonic welding device ( 110 ), the width being adjusted by means of at least one lateral slide ( 134 ) and the height by changing the distance between a sonotrode ( 116 ) and a counter electrode ( 118 ) of the ultrasonic welding device, the at least one first stranded wire being welded with a higher specific energy, under a higher pressure or with a greater ultrasonic vibration amplitude than the at least one second stranded wire,

characterized in that

the at least one first stranded wire ( 144 ) is inserted in the compression chamber ( 122 ) and its individual wires are welded to a partial node ( 146 ), wherein the compression chamber is set to a width B in such a manner that the partial node completely covers the bottom of the compression chamber delimited by the sonotrode ( 116 ) or a section thereof, that the at least one second stranded wire is inserted on the partial node in the compression chamber, and after closing the compression chamber the at least one second stranded wire ( 148 ) is welded to the partial node to yield an aggregate node, wherein the width of the compression chamber when welding the aggregate node is equal to the width B.

2. The method according to claim 1 ,

characterized in that

the width of the compression chamber ( 122 ) is set to the width B of the node ( 160 ) to be produced before the at least one first stranded wire ( 144 ) is inserted in said chamber.

3. The method according to claim 1 ,

characterized in that

after welding the at least one first stranded wire ( 144 ) to the partial node ( 146 ), the lateral slide ( 134 ) is depressurized and pressure is reapplied to the lateral slide such that the compression chamber has the width B before the at least one second stranded wire ( 148 ) is welded.

4. The method according to claim 1 ,

characterized in that

that such materials are selected for the at least one first and the at least on second stranded wires ( 144 , 148 ) that with respect to the material of the at least one first stranded wire at least 25% more energy must be input for welding a proper partial node ( 146 ) than for proper welding of the at least one second stranded wire.

5. The method according to claim 1 ,

characterized in that

for evaluating the proper welding of the at least one first stranded wire ( 144 ), a process parameter other than the one for monitoring proper welding of the at least one second stranded wire ( 148 ) is monitored.

6. The method according to claim 1 ,

characterized in that

the energy input required is monitored based on the specified welding time for monitoring the proper welding of the at least one stranded wire ( 144 ).

7. The method according to claim 1 ,

characterized in that

for determining proper welding of the at least one second stranded wire ( 148 ), the energy input depending on the height change of the compression chamber ( 122 ), in particular the adjustment of the counter electrode ( 118 ) in the direction of the sonotrode ( 116 ) is monitored.

8. The method according to claim 1 ,

characterized in that

copper or a copper alloy is used as the material of the at least one first stranded wire ( 144 ).

9. The method according to claim 1 ,

characterized in that

aluminum or an aluminum alloy is used as the material of the at least one second stranded wire ( 148 ).

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Sep 21, 2016
From: RÜHL, SEBASTIAN; STROBEL, HEIKO; HANIKA, TIM
To: SCHUNK SONOSYSTEMS GMBH
Reel/Frame 039817/0507 →
Priority Claims (1)
DE 10 2013 107 637 · Jul 18, 2013 · national
Continuity (1)
Related Publication 20160136753A1 · May 19, 2016