IP Library Granted Patent US 9,551,421
Granted Patent B2
US 9,551,421 · App. 13/148,339 · Granted Jan 24, 2017

Sliding member and process for producing the same

Inventors: Yuhei Tabuchi (Kitaibaraki, JP); Yoshiyuki Abe (Kitaibaraki, JP); Toshiyuki Maeda (Kitaibaraki, JP)
Assignee: NOK Corporation
F16J15/102C08K7/02C08L77/00C08L77/06F16J15/3284F16J15/3496C08L77/10C08L2205/02Y10T428/24355
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 9,551,421
App. No.
13/148,339
Granted
Jan 24, 2017
Kind
B2
Abstract

Object: To provide a sliding member with a low friction coefficient in which, when fine dents are formed in a surface of the sliding member by dimpling using a laser, no hard raised portions are generated, and which does not damage a mating member; and to provide a process for producing the sliding member. Solution Means: A sliding member comprising a polyamide resin and 10 to 50 wt % of a fibrous filler selected from the group consisting of carbon fibers, aramid fibers, and whiskers, and having fine dents formed in a sliding surface thereof by dimpling using a laser; and a process for producing a sliding member comprising adding 10 to 50 wt % of a fibrous filler selected from the group consisting of carbon fibers, aramid fibers, and whiskers to a polyamide resin, and forming fine dents in a sliding surface of the sliding member by dimpling using a laser.

Claims (1)

1. A process for producing a sliding member comprising adding 10 to 50 wt % of a fibrous filler selected from the group consisting of carbon fibers, aramid fibers, and whiskers to a polyamide resin, then forming a sliding member into a predetermined shape, using a molding means, then forming fine dents having a maximum depth of 5 to 50 μm in a sliding surface of the sliding member by applying a dimpling process to the sliding member, using a laser, and forming no raised portions projecting from the same sliding surface as said sliding surface consisting of melted spheres and projections due to laser heat inside of the fine dents and around the dents at the time of the dimpling process.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Aug 8, 2011
From: TABUCHI, YUHEI; ABE, YOSHIYUKI; MAEDA, TOSHIYUKI
To: NOK CORPORATION
Reel/Frame 026714/0839 →
Priority Claims (1)
JP 2009-028286 · Feb 10, 2009 · national
Continuity (1)
Related Publication 20110305871A1 · Dec 15, 2011