IP Library › Granted Patent US 9,636,775
Granted Patent B2
US 9,636,775 · App. 14/583,398 · Granted May 2, 2017

Composite beam generator and powder melting or sintering method using the same

Inventors: Wei-Chin Huang (Tainan, TW); Ping-Han Wu (Tainan, TW); Kuang-Po Chang (Taichung, TW)
Assignee: INDUSTRIAL TECHNOLOGY RESEARCH INSTITUTE
B23K26/0608B22F3/1055B23K26/0626B23K26/0648B23K26/342B28B1/001B28B17/0063B29C67/0077B29C67/0088B22F2003/1057B33Y10/00B33Y30/00
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 9,636,775
App. No.
14/583,398
Granted
May 2, 2017
Kind
B2
Abstract

This disclosure provides a composite beam generator and a method of performing powder melting or sintering in additive manufacturing process using the same. The composite beam generator comprises: a beam splitter for splitting a beam into a first directed beam and a second directed beam; a beam shaper for shaping a transverse energy distribution profile of the second directed beam to non-circular; at least one beam delivery unit for guiding the first directed beam or the second directed beam; and a beam combiner for receiving the first directed beam and the second directed beam, and respectively generating a first output beam and a second output beam, and combining them into the composite beam.

Claims (38)

1. A composite beam generator for performing powder melting or sintering in additive manufacturing process, comprising:

a first directed beam having a first transverse energy distribution profile for melting or sintering a powder;

a second directed beam having a second transverse energy distribution profile of non-circular for adjusting the temperature variation of the melted powder to control the solidification; and

a beam combiner for receiving the first directed beam and the second directed beam, and combining them into the composite beam.

2. The composite beam generator according to claim 1 , wherein the beam combiner is selected from a group consisting of a non-polarizing beam combiner, a polarizing beam combiner, and an optical fiber coupler.

3. The composite beam generator according to claim 1 , wherein the second directed beam comprising a shape of line, rectangle, oval, triangle, teardrop, or dumbbell.

4. The composite beam generator according to claim 1 , wherein each of the first and second directed beam is a continuous-wave laser beam or a pulsed laser beam to control the solidification to control the solidification.

5. A composite beam generator for performing powder melting or sintering in additive manufacturing process, comprising:

a beam splitter for splitting a beam into a first directed beam and a second directed beam;

a beam shaper for shaping a transverse energy distribution profile of the second directed beam to non-circular;

at least one beam delivery unit for guiding the first directed beam or the second directed beam; and

a beam combiner for receiving the first directed beam and the second directed beam, and respectively generating a first output beam and a second output beam, and combining them into the composite beam.

6. The composite beam generator for performing powder melting or sintering according to claim 5 , further comprising a laser source for generating an optical beam to be provided for the beam splitter.

7. The composite beam generator for performing powder melting or sintering according to claim 5 , wherein the beam delivery unit comprises a mirror, an optical fiber, a prism, or the combination thereof.

8. The composite beam generator for performing powder melting or sintering according to claim 5 , wherein the second directed beam has a transverse energy distribution profile comprising a shape of line, rectangle, oval, triangle, teardrop, or dumbbell.

9. The composite beam generator for performing powder melting or sintering according to claim 5 , further comprising an energy regulator for regulating energy ratios of the first output beam to the first directed beam and the second output beam to the second directed beam.

10. The composite beam generator for performing powder melting or sintering according to claim 9 , wherein the second directed beam after split from the beam splitter is directed to a polarization regulator, so that the second directed beam is regulated by the polarization regulator.

11. The composite beam generator for performing powder melting or sintering according to claim 9 , wherein the energy regulator is selected from a group consisting of a polarization regulator, an energy attenuator, and an energy amplifier.

12. The composite beam generator for performing powder melting or sintering according to claim 5 , wherein the beam splitter is selected from a group consisting of a non-polarizing beam splitter, a polarizing beam splitter and an optical fiber coupler.

13. The composite beam generator for performing powder melting or sintering according to claim 5 , wherein the beam shaper is comprising a cylindrical lens, a diffractive optical element, and a spatial light modulator.

14. The composite beam generator for performing powder melting or sintering according to claim 5 , wherein the beam combiner is selected from a group consisting of a non-polarizing beam combiner, a polarizing beam combiner, and an optical fiber coupler.

15. The composite beam generator for performing powder melting or sintering according to claim 6 , wherein the laser source has a wavelength between 0.2 μm and 100 μm.

16. The composite beam generator for performing powder melting or sintering according to claim 6 , wherein the laser source is comprising a continuous-wave laser, a pulsed laser, or the combination thereof.

17. A method for performing powder melting or sintering in additive manufacturing process, comprising the following steps of:

providing a powder layer on a surface; and

selectively irradiating the powder layer with a moving composite energy beam which includes a first directed beam and a second directed beam;

wherein the first directed beam has a first transverse energy distribution profile for melting or sintering the powder; and

wherein the second directed beam has a second transverse energy distribution profile with non-circular shape for adjusting the temperature variation of the melted powder layer to control the solidification.

18. The method according to claim 17 , wherein the first transverse energy distribution profile has an area between 1 μm 2 and 100 mm 2 .

19. The method according to claim 17 , wherein the second directed beam has a absorbed energy density of the powder layer being from 0.01 to 0.99 times that of the first directed beam.

20. The method according to claim 17 , wherein the second transverse energy distribution profile is comprising a shape of line, rectangle, oval, triangle, teardrop, or dumbbell.

21. The method according to claim 17 , further comprising a step of adjusting an energy magnitude of the second directed beam.

22. The method according to claim 17 , further comprising a step of adjusting an energy distribution of the second directed beam.

23. The method according to claim 17 , wherein an energy source of the composite energy beam is comprising a continuous-wave laser beam, a pulsed laser beam, an electron beam, an electric arc, or the combination thereof.

24. The method according to claim 17 , further comprising a step of dynamically regulating the propagation direction of the composite energy beam.

25. The method according to claim 17 , wherein the second directed beam has a second transverse energy distribution profile of non-circular for adjusting the temperature variation of the powder layer before and after the powder is melted to control the solidification.

26. The method according to claim 17 , wherein the second directed beam has a second transverse energy distribution profile of non-circular for adjusting the temperature variation of the powder layer before or after the powder is melted to control the solidification.

27. The method according to claim 17 , wherein the powder is selective from group consisting of metal, ceramic, polymer, or the mixture thereof.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Mar 20, 2015
From: HUANG, WEI-CHIN; WU, PING-HAN; CHANG, KUANG-PO
To: INDUSTRIAL TECHNOLOGY RESEARCH INSTITUTE
Reel/Frame 035217/0703 →
Priority Claims (1)
TW 103145237 A · Dec 24, 2014 · national
Continuity (1)
Related Publication 20160184925A1 · Jun 30, 2016