Alkaline battery including cathode can with coating composed of nickel-cobalt alloy

Inventors: Shigeyuki Kuniya (Kosai, JP); Yoshiaki Ishitani (Kosai, JP)
Assignee: FDK Energy Co., Ltd.
H01M2/0257H01M2/026H01M2/0235H01M2/0272H01M2/0285H01M2/0287H01M6/08H01M6/085
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 9,728,752
App. No.
13/818,475
Granted
Aug 8, 2017
Kind
B2
Abstract

There is provided An inside-out alkaline battery, including: a cylindrical cathode can that has a bottom, that performs a function of a cathode current collector, that has a nickel-plated layer on an inner surface of the cathode can, and that has a coating on a surface layer of the nickel-plated layer, the coating being composed of nickel-cobalt alloy, a thickness of the coating being between 0.15 μm and 0.25 μm (both inclusive), a ratio of cobalt in the nickel-cobalt alloy being between 40% and 60% (both inclusive); and a cathode mixture that is disposed in the cathode can, that is annular in shape, and that contains a cathode active material.

Claims (17)

1. An inside-out alkaline battery, comprising:

a cylindrical cathode can

that has a bottom,

that performs a function of a cathode current collector,

that uses a can formed by multistage deep drawing of a steel sheet, the steel sheet including a nickel-plated layer having a thickness of 1.0 μm,

that does not include an electro-conductive paint in which volatile organic compound or water is used as solvent being applied to an inner surface of the cathode can,

that has the nickel-plated layer on the inner surface of the cathode can, and

that has a coating on a surface layer of the nickel-plated layer,

the coating being composed of nickel-cobalt alloy that contains only nickel-cobalt alloy,

a thickness of the coating being between 0.15 μm and 0.25 μm (both inclusive),

a ratio of cobalt in the nickel-cobalt alloy being between 40% and 60% (both inclusive); and

a cathode mixture

that is disposed in the cathode can,

that is annular in shape, and

that contains a cathode active material.

2. An alkaline battery according to claim 1 , wherein

the inner surface of the cylindrical cathode can has a roughness Ra value between 1.0 μm and 1.5 μm (both inclusive) in a circumferential direction.

Assignments (2)
MERGER AND CHANGE OF NAME Recorded Sep 17, 2018
From: FDK ENERGY CO., LTD.; FDK CORPORATION
To: FDK CORPORATION
Reel/Frame 047095/0493 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Apr 3, 2013
From: KUNIYA, SHIGEYUKI; ISHITANI, YOSHIAKI
To: FDK ENERGY CO., LTD.
Reel/Frame 030142/0619 →
Priority Claims (1)
JP 2010-189769 · Aug 26, 2010 · national
Continuity (1)
Related Publication 20130209864A1 · Aug 15, 2013