IP Library › Granted Patent US 9,822,426
Granted Patent B2
US 9,822,426 · App. 14/813,389 · Granted Nov 21, 2017

Method for recovery of metals from sulfide ores

Inventor: Jody Kelso (Tucson, AZ)
C22B3/18C22B1/16C22B11/04C22B15/0067C22B19/22C22B23/0415Y02P10/234
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 9,822,426
App. No.
14/813,389
Granted
Nov 21, 2017
Kind
B2
Abstract

A process for bio-oxidation of sulfides in mineral ore having a metal such as gold occluded or dispersed within the ore as a sulfide is disclosed. The first step comminutes the ore into particles with a size distribution having a P80 of less than 0.25 inch with minus 106 micron particles in the range of 15% to 40% by weight. Agglomerates are formed by adding to the comminuted ore particles an acidic inoculate solution including water, with the solution further including microorganisms capable of bio-oxidizing the sulfides. The agglomerates are then placed in at least one bio-reactor containment vessel to form an ore bed. The process continues by bio-oxidizing the sulfides in the ore bed; then re-circulating the solution through the ore bed, and continuing the bio-oxidation until a desired bio-oxidation level is achieved. Thereafter, the metal is recovered from the ore.

Claims (32)

1. A process for bio-oxidation of sulfides in mineral ore having a metal occluded or dispersed within said ore as a sulfide, comprising the steps of:

comminuting said ore into particles with a size distribution having a P80 of less than 0.25 inch, and minus 106 micron particles in the range of 15% to 40% by weight;

forming agglomerates by adding to said comminuted ore particles an acidic inoculate solution including water, said solution further including microorganisms capable of bio-oxidizing said sulfides;

placing said agglomerates in at least one bio-reactor containment vessel to form an ore bed;

bio-oxidizing said sulfides in said ore bed; and

re-circulating said solution through said ore bed and continuing said bio-oxidation until a desired bio-oxidation level is achieved; and

thereafter recovering said metal from said ore.

2. A process for bio-oxidation as claimed in claim 1 , wherein said metal is selected from the group consisting of gold, silver, copper, zinc, nickel and cobalt.

3. A process for bio-oxidation as claimed in claim 2 , wherein said metal is gold.

4. A process for bio-oxidation as claimed in claim 1 wherein the agglomerates formed have a micropore to macropore volume ratio of about 1:1.

5. A process for bio-oxidation as claimed in claim 1 wherein the agglomerates formed have a micropore to macropore volume ratio of greater than 3:7.

6. A process for bio-oxidation as claimed in claim 1 wherein the agglomerates formed have a micropore to macropore volume ratio ranging from 1:2 to 2:1.

7. A process for bio-oxidation as claimed in claim 1 wherein said ore has a dry weight before said inoculate solution is added to said comminuted ore particles and wherein said agglomerates have spaces between them referred to as macropores and wherein the amount of said inoculate solution in the macropores of the agglomerates is about 1% of the dry weight of the ore when a steady state bio-oxidation condition is achieved.

8. A process for bio-oxidation as claimed in claim 1 wherein said ore has a dry weight before said inoculate solution is added to said comminuted ore particles and wherein said agglomerates have spaces between them referred to as macropores and wherein the amount of said inoculate solution in the macropores of the agglomerates is less than 2% of the dry weight of the ore when a steady state bio-oxidation condition is achieved.

9. A process for bio-oxidation as claimed in claim 1 further comprising supplying the ore bed with oxygen to enhance the bio-oxidation process.

10. A process for bio-oxidation as claimed in claim 9 wherein the oxygen is supplied to the ore bed via air.

11. A process for bio-oxidation as claimed in claim 9 wherein the ore bed has a surface and wherein the oxygen supplied to the ore bed is supplied at a rate which is adjusted to maintain the oxygen content of the air exiting the surface of the ore bed at a predetermined threshold level.

12. A process for bio-oxidation as claimed in claim 1 wherein the solution has an iron concentration which is maintained so that it less than or equal to 100 grams per liter of solution.

13. A process for bio-oxidation as claimed in claim 1 wherein said ore bed has a bottom layer of agglomerates and wherein said step of bio-oxidizing said sulfides in said ore bed is carried out in a free drained mode to ensure that the bottom layer of agglomerates is permeable.

14. A process for bio-oxidation as claimed in claim 1 wherein said microorganisms include mesophilic microorganisms.

15. A process for bio-oxidation as claimed in claim 14 wherein said microorganisms further include thermophilic microorganisms.

16. A process for bio-oxidation as claimed in claim 15 wherein said thermophilic microorganisms include moderate and extreme thermophilic organisms.

17. A process for bio-oxidation of sulfides in mineral ore having a metal occluded or dispersed within said ore as a sulfide, comprising the steps of:

comminuting said ore into particles with a size distribution having a P80 in the approximate range of 340 to 950 microns, and minus 106 micron particles in the range of 15% to 40% by weight;

forming agglomerates by adding to said comminuted ore particles an acidic inoculate solution including water, said solution further including microorganisms capable of bio-oxidizing said sulfides;

placing said agglomerates in at least one bio-reactor containment vessel to form an ore bed;

bio-oxidizing said sulfides in said ore bed; and

re-circulating said solution through said ore bed and continuing said bio-oxidation until a desired bio-oxidation level is achieved; and

thereafter recovering said metal from said ore.

18. A process for bio-oxidation as claimed in claim 17 , wherein said metal is selected from the group consisting of gold, silver, copper, zinc, nickel and cobalt.

19. A process for bio-oxidation as claimed in claim 17 , wherein said agglomerates are placed in a plurality of containment vessels.

20. A process for bio-oxidation proccss as claimed in claim 19 , wherein said metal is selected from the group consisting of gold, silver, copper, zinc, nickel and cobalt.

Continuity (3)
Continuation PCTUS2014014324 · Jan 31, 2014
Provisional Application 61759929 · Feb 1, 2013
Related Publication 20150329936A1 · Nov 19, 2015