US 9,999,941 · App. 15/111,191 · Granted Jun 19, 2018

Method of manufacturing liquid-cooled jacket

Inventors: Hisashi Hori (Shizuoka, JP); Nobushiro Seo (Shizuoka, JP)
Assignee: NIPPON LIGHT METAL COMPANY, LTD.
B23K20/1235B23K20/124B23K20/126B23K20/1255B23K2201/045
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 9,999,941
App. No.
15/111,191
Granted
Jun 19, 2018
Kind
B2
Abstract

A method of manufacturing a liquid-cooled jacket, includes a preparation step which includes placing a sealing body on a stepped portion to allow a step side surface and a sealing-body side surface of the sealing body to butt each other, and a primary joining step which includes allowing a primary joining rotary tool to move once around the sealing body, while moving the rotary tool along a butted portion formed in the preparation step, to carry out friction stir welding. The primary joining step includes employing the primary joining rotary tool provided with a stirring pin having a length dimension greater than a thickness dimension of the sealing body, and carrying out friction stirring with only the stirring pin being brought into contact with a jacket body and the sealing body.

Claims (13)

1. A method of manufacturing a liquid-cooled jacket which is composed of a jacket body having a bottom portion and a frame-shaped side wall portion provided to stand on the bottom portion, and a sealing body which seals an opening of the jacket body, and allows heat transport fluid to flow in a hollow portion formed by the jacket body and the sealing body, the method comprising:

a preparation step which includes forming, on a peripheral edge of the opening of the jacket body, a step bottom surface located below by one step from an end surface of the side wall portion, and a step side surface rising from the step bottom surface, and

placing the sealing body on the step bottom surface to allow the step side surface and a sealing-body side surface of the sealing body to butt each other; and

a primary joining step which includes allowing a rotary tool to move once around the sealing body, while moving the rotary tool along a butted portion formed in the preparation step, to carry out friction stir welding, wherein

the primary joining step includes employing the rotary tool provided with a stirring pin having a length dimension greater than a thickness dimension of the sealing body, and carrying out friction stirring with only the stirring pin being brought into contact with the jacket body and the sealing body, and

wherein the primary joining step includes carrying out friction stir welding in a state in which a front surface side of the jacket body and a front surface side of the sealing body are in a convex shape.

2. A method of manufacturing a liquid-cooled jacket which is composed of a jacket body having a bottom portion and a frame-shaped side wall portion provided to stand on the bottom portion, and a sealing body which seals an opening of the jacket body, and allows heat transport fluid to flow in a hollow portion formed by the jacket body and the sealing body, the method comprising:

a preparation step which includes forming, on a peripheral edge of the opening of the jacket body, a step bottom surface located below by one step from an end surface of the side wall portion, and a step side surface rising from the step bottom surface, and

placing the sealing body on the step bottom surface to allow the step side surface and a sealing-body side surface of the sealing body to butt each other; and

a primary joining step which includes allowing a rotary tool to move once around the sealing body, while moving the rotary tool along a butted portion formed in the preparation step, to carry out friction stir welding, wherein

the primary joining step includes employing the rotary tool provided with a stirring pin having a length dimension greater than a thickness dimension of the sealing body, and carrying out friction stirring with only the stirring pin being brought into contact with the jacket body and the sealing body,

wherein the primary joining step includes carrying out friction stir welding in a state in which a front surface side of the jacket body and a front surface side of the sealing body are in a convex shape, and

wherein the primary joining step includes measuring beforehand an amount of deformation of at least one of the jacket body and the sealing body, and carrying out friction stir welding while adjusting an insertion depth of the stirring pin according to the amount of deformation.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jul 13, 2016
From: HORI, HISASHI; SEO, NOBUSHIRO
To: NIPPON LIGHT METAL COMPANY, LTD.
Reel/Frame 039140/0349 →
Priority Claims (2)
JP 2014-004267 · Jan 14, 2014 · national
JP 2014-004280 · Jan 14, 2014 · national
Continuity (1)
Related Publication 20160325374A1 · Nov 10, 2016