IP Library Granted Patent US 10,024,135
Granted Patent B2
US 10,024,135 · App. 15/349,621 · Granted Jul 17, 2018

Electrically activated adhesive for strengthening of a subterranean wellbore

Inventors: Beathe Mariero Pettersen (Sandnes, NO); Anders Grinrod (Sandnes, NO); Anne Myrvold Fosse (Sandnes, NO)
Assignee: SCHLUMBERGER NORGE AS
E21B33/138C08G83/003C08G83/004C09K8/035C09K8/42C09K8/428C09K8/44C09K8/502C09K8/508C09K8/565C09K8/5751E21B21/003
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 10,024,135
App. No.
15/349,621
Granted
Jul 17, 2018
Kind
B2
Abstract

A wellbore strengthening composition may include a base fluid and at least one polymer functionalized with electrochemically activated groups. A method of treating a wellbore may include emplacing, in at least a selected region of the wellbore, a wellbore strengthening composition including a base fluid and at least one polymer functionalized with electrochemically activated groups. The method may also include emplacing a downhole tool capable of generating a voltage potential in the wellbore and applying a voltage potential in the wellbore with the downhole tool.

Claims (14)

1. A method of treating a wellbore, the method comprising:

emplacing in at least a selected region of the wellbore, a wellbore strengthening composition comprising:

a base fluid; and

at least one polymer functionalized with electrochemically activated groups;

emplacing a downhole tool capable of generating a voltage potential in the wellbore; and

applying a voltage potential in the wellbore with the downhole tool.

2. The method of claim 1 , wherein the voltage potential is applied near a wall of the wellbore.

3. The method of claim 1 , wherein the voltage potential is applied at multiple distinct zones of the wellbore.

4. The method of claim 1 , wherein the voltage potential applied is at least about−0.5V.

5. The method of claim 1 , wherein the voltage potential is applied for at least one minute.

6. The method of claim 1 , wherein the voltage potential is applied for at most one hour.

7. The method of claim 1 , wherein the at least one polymer functionalized with electrochemically activated groups is a dendrimer.

8. The method of claim 1 , wherein the at least one polymer functionalized with electrochemically activated groups is a poly(amidoamine) dendrimer.

9. The method of claim 1 , wherein the electrochemically activated groups are carbene precursors.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jul 10, 2018
From: PETTERSEN, BEATHE MARIERO; GRINROD, ANDERS; FOSSE, ANNE MYRVOLD
To: SCHLUMBERGER NORGE AS
Reel/Frame 046301/0165 →
Continuity (2)
Provisional Application 62255001 · Nov 13, 2015
Related Publication 20170137693A1 · May 18, 2017