Composition for car interior trim and preparation method using the same

Inventors: Soo-Ho Moon (Chungcheongnam-do, KR); Jin-Bae Cho (Incheon, KR); Man-Ho Lee (Gyeonggi-do, KR); Ki-Pyoung Yang (Daegu, KR); Seoung-Jee Lee (Gyeongsangbuk-do, KR); Chong Hoon Lee (Ulsan, KR)
Assignee: S&B CO., LTD.
C09D175/08C08J9/0038C08J9/365C08K5/521C08L33/08C08J2375/04C08J2433/08C08J2475/04C08K5/0066
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 10,035,925
App. No.
15/062,216
Granted
Jul 31, 2018
Kind
B2
Abstract

A composition for a car interior trim including: a polyurethane sponge layer for a car interior trim; and a water-soluble resin layer formed on the polyurethane sponge layer and comprising 20 to 50 parts by weight of a phosphorus-based flame retardant and 1 to 5 parts by weight of a thickener, based on 100 parts by weight of a coating agent blend of one or two more of a water-dispersed polyurethane or an aqueous acrylic resin.

Claims (11)

1. A method of preparing a composition for a car interior trim comprising:

adding a phosphorus-based flame retardant into a resin and dispersing it, thereby preparing a coating agent (step 1);

adding water into the dispersed coating agent and dispersing it at less than 2000 rpm, thereby preparing an aqueous resin (step 2);

adding a thickener into the aqueous resin to control viscosity (step 3)

rotating a polyurethane sponge layer on a roller and coating the aqueous resin thereon (step 4); and

drying the polyurethane sponge layer coated with the aqueous resin (step 5).

2. The method of preparing a composition for a car interior trim according to claim 1 , wherein the step 1 comprises dispersing at high speed of 2000 to 5000 rpm for 20 to 30 minutes.

3. The method of preparing a composition for a car interior trim according to claim 1 , wherein the step 3 comprises adding 1 to 3 parts by weight of the thickener, based on 100 parts by weight of the dispersed aqueous resin.

4. The method of preparing a composition for a car interior trim according to claim 1 , wherein the step 3 comprises adding the thickener into the resin to control viscosity to 3,000 to 6,000 CPS.

5. The method of preparing a composition for a car interior trim according to claim 1 , wherein the step 4 comprises rotating the roller at 10 to 30 m/min and coating the aqueous resin with an amount of 20 to 50 g/m 2 .

6. The method of preparing a composition for a car interior trim according to claim 1 , wherein the step 5 comprises drying at temperature of 130 to 160° C.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Mar 7, 2016
From: MOON, SOO-HO; CHO, JIN-BAE; LEE, MAN-HO; YANG, KI-PYOUNG; LEE, SEOUNG-JEE; LEE, CHONG HOON