IP Library › Granted Patent US 10,087,105
Granted Patent B2
US 10,087,105 · App. 15/821,141 · Granted Oct 2, 2018

Lightweight concrete formulations

Inventors: Chris Calvin (Bradford, CA); Matthew Boehler (Markham, CA)
Assignee: 2581776 Ontario Inc.
C04B18/027C04B14/06C04B14/106C04B14/24C04B28/04C04B2111/2023C04B2111/40C04B2111/70
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 10,087,105
App. No.
15/821,141
Granted
Oct 2, 2018
Kind
B2
Abstract

A lightweight concrete formulation containing Portland cement, aggregate, glass particles, water and metakaolin. At least 80% of the glass particles have a grain size of less than 2 mm. The glass particles contribute between 3% and 20% of the total weight of the concrete formulation. The metakaolin contributes between 4% and 12% of the total weight of the concrete formulation. The glass particles are preferably expanded glass particles. Also provided is a lightweight grout formulation containing Portland cement, glass particles, water and metakaolin. At least 80% of the glass particles have a grain size of less than 2 mm. The glass particles contribute between 3% and 15% of the total weight of the grout formulation. The metakaolin contributes between 7% and 15% of the total weight of the grout formulation.

Claims (19)

1. A concrete formulation comprising Portland cement, aggregate, expanded glass particles, water and metakaolin, wherein at least 80% of the expanded glass particles have a grain size of between 0.25 mm and 0.5 mm, the expanded glass particles contribute between 3% and 20% of the total weight of the concrete formulation, the Portland cement contributes at least 30% of the total weight of the concrete formulation, and the metakaolin contributes between 7% and 15% of the total weight of the concrete formulation, and wherein the compressive strength of the concrete formulation is at least 30 MPa after curing.

2. The concrete formulation of claim 1 , wherein the expanded glass particles contribute between 6% and 15% of the total weight of the concrete formulation.

3. The concrete formulation of claim 1 , wherein the expanded glass particles contribute at least 12% of the total weight of the concrete formulation.

4. The concrete formulation of claim 1 , wherein the metakaolin contributes between 8% and 12% of the total weight of the concrete formulation.

5. The concrete formulation of claim 1 , wherein the metakaolin contributes between 8% and 10% of the total weight of the concrete formulation.

6. The concrete formulation of claim 1 , wherein the expanded glass particles contribute between 12% and 15% of the total weight of the concrete formulation.

7. The concrete formulation of claim 1 , wherein the Portland cement contributes between 30% and 38% of the total weight of the concrete formulation, the aggregate contributes between 16% and 24% of the total weight of the concrete formulation, and the metakaolin contributes between 6% and 12% of the total weight of the concrete formulation.

8. The concrete formulation of claim 7 , wherein the Portland cement contributes between 32% and 36% of the total weight of the concrete formulation, the aggregate contributes between 19% and 23% of the total weight of the concrete formulation, and the metakaolin contributes between 8% and 10% of the total weight of the concrete formulation.

9. A concrete formulation comprising Portland cement, aggregate, expanded glass particles, sand, water and metakaolin, wherein at least 80% of the expanded glass particles have a grain size of between 0.25 mm and 0.5 mm, the expanded glass particles contribute between 3% and 20% of the total weight of the concrete formulation, the Portland cement contributes at least 21% of the total weight of the concrete formulation, and the metakaolin contributes between 5% and 15% of the total weight of the concrete formulation, and wherein the compressive strength of the concrete formulation is at least 30 MPa after curing.

10. The concrete formulation of claim 9 , wherein the Portland cement contributes between 20% and 35% of the total weight of the concrete formulation, the aggregate contributes between 16% and 24% of the total weight of the concrete formulation, the sand contributes between 22% and 32% of the total weight of the concrete formulation, the expanded glass particles contribute between 3% and 9% of the total weight of the concrete formulation, and the metakaolin contributes between 5% and 11% of the total weight of the concrete formulation.

11. The concrete formulation of claim 10 , wherein the Portland cement contributes between 21% and 25% of the total weight of the concrete formulation, the aggregate contributes between 18% and 22% of the total weight of the concrete formulation, the sand contributes between 25% and 29% of the total weight of the concrete formulation, the expanded glass particles contribute between 5% and 7% of the total weight of the concrete formulation, and the metakaolin contributes between 6% and 8% of the total weight of the concrete formulation.

12. A grout formulation comprising Portland cement, expanded glass particles, water and metakaolin, wherein at least 80% of the expanded glass particles have a grain size of between 0.25 mm and 0.5 mm, the expanded glass particles contribute between 3% and 15% of the total weight of the grout formulation, the Portland cement contributes at least 32% of the total weight of the concrete formulation, and the metakaolin contributes between 7% and 15% of the total weight of the grout formulation, and wherein the compressive strength of the grout formulation is at least 30 MPa after curing.

13. The grout formulation of claim 12 , wherein the expanded glass particles contribute between 8% and 13% of the total weight of the grout formulation.

14. The grout formulation of claim 12 , wherein the metakaolin contributes between 8% and 11% of the total weight of the grout formulation.

15. The grout formulation of claim 12 , wherein the expanded glass particles contribute between 8.5% and 10.5% of the total weight of the grout formulation.

16. The grout formulation of claim 12 , wherein the Portland cement contributes between 44% and 52% of the total weight of the grout formulation, and the metakaolin contributes between 8% and 13% of the total weight of the grout formulation.

17. The grout formulation of claim 16 , wherein the Portland cement contributes between 45.5% and 49.5% of the total weight of the grout formulation, and the metakaolin contributes between 9.5% and 11.5% of the total weight of the grout formulation.

18. The grout formulation of claim 12 further comprising sand, wherein the Portland cement contributes between 32% and 37% of the total weight of the grout formulation, the sand contributes between 20% and 28% of the total weight of the grout formulation, the expanded glass particles contribute between 3% and 9% of the total weight of the grout formulation, and the metakaolin contributes between 8% and 14% of the total weight of the grout formulation.

19. The grout formulation of claim 18 , wherein the Portland cement contributes between 33.5% and 35.5% of the total weight of the grout formulation, the sand contributes between 22% and 24% of the total weight of the grout formulation, the expanded glass particles contribute between 5% and 7% of the total weight of the grout formulation, and the metakaolin contributes between 9% and 11% of the total weight of the grout formulation.

Assignments (1)
NUNC PRO TUNC ASSIGNMENT Recorded May 22, 2018
From: CALVIN, CHRIS; BOEHLER, MATTHEW
To: 2581776 ONTARIO INC.
Reel/Frame 046207/0417 →
Continuity (3)
Continuation PCTCA2017000130 · May 23, 2017
Provisional Application 62340801 · May 24, 2016
Related Publication 20180093920A1 · Apr 5, 2018
Cited By (1)
US 12,595,207