IP Library Granted Patent US 10,090,527
Granted Patent B2
US 10,090,527 · App. 14/773,333 · Granted Oct 2, 2018

Binder composition for secondary battery, slurry composition for secondary battery, negative electrode for secondary battery, and secondary battery

Inventor: Kenya Sonobe (Tokyo, JP)
Assignee: ZEON CORPORATION
H01M4/622C08F236/10H01M10/0525H01M2004/8684
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 10,090,527
App. No.
14/773,333
Granted
Oct 2, 2018
Kind
B2
Abstract

A binder composition for a secondary battery includes: a water-soluble thickener (A) having a hydroxy group or a carboxy group; a cross-linking agent (B) having a functional group reacting with the hydroxy group or the carboxy group of the water-soluble thickener (A); and a particulate polymer (C). The particulate polymer (C) has a functional group reacting with the cross-linking agent (B) and includes an aliphatic conjugated diene monomer unit and an aromatic vinyl monomer unit. The binder composition contains 0.001 part by mass or more and less than 100 parts by mass of the cross-linking agent (B) and 10 parts by mass or more and less than 500 parts by mass of the particulate polymer (C), each per 100 parts by mass of the water-soluble thickener (A).

Claims (15)

1. A binder composition for a secondary battery, comprising: a water-soluble thickener (A) having a hydroxy group or a carboxy group; a cross-linking agent (B) having a functional group reacting with the hydroxy group or the carboxy group of the water-soluble thickener (A); and a particulate polymer (C), wherein the particulate polymer (C) has a functional group reacting with the cross-linking agent (B) and includes an aliphatic conjugated diene monomer unit and an aromatic vinyl monomer unit, and the binder composition contains 0.001 part by mass or more and less than 100 parts by mass of the cross-linking agent (B) and 10 parts by mass or more and less than 500 parts by mass of the particulate polymer (C), each per 100 parts by mass of the water-soluble thickener (A).

2. The binder composition for a secondary battery, according to claim 1 , wherein a water solubility of the cross-linking agent (B) is 80% by mass or more.

3. The binder composition for a secondary battery, according to claim 1 , wherein the cross-linking agent (B) is a multifunctional epoxy compound.

4. The binder composition for a secondary battery, according to claim 1 , wherein the water-soluble thickener (A) is at least one selected from the group consisting of carboxymethyl cellulose, methyl cellulose, hydroxypropyl methylcellulose, hydroxyethyl methylcellulose, polyvinyl alcohol, and polyacrylic acid, and salts thereof.

5. The binder composition for a secondary battery, according to claim 1 , wherein the functional group in the particulate polymer (C) that reacts with the cross-linking agent (B) is at least one selected from the group consisting of a carboxy group, a hydroxy group, a glycidyl ether group, and a thiol group.

6. A slurry composition for a secondary battery, comprising: a water-soluble thickener (A) having a hydroxy group or a carboxy group; a cross-linking agent (B) having a functional group reacting with the hydroxy group or the carboxy group of the water-soluble thickener (A); a particulate polymer (C); an electrode active material; and water, wherein the particulate polymer (C) has a functional group reacting with the cross-linking agent (B) and includes an aliphatic conjugated diene monomer unit and an aromatic vinyl monomer unit, and the binder composition contains 0.001 part by mass or more and less than 100 parts by mass of the cross-linking agent (B) and 10 parts by mass or more and less than 500 parts by mass of the particulate polymer (C), each per 100 parts by mass of the water-soluble thickener (A).

7. A negative electrode for a secondary battery, comprising a negative electrode mix layer obtained from the slurry composition for a secondary battery, according to claim 6 , wherein the electrode active material is a negative electrode active material.

8. A negative electrode for a secondary battery, according to claim 7 , wherein the negative electrode mix layer has a crosslinking structure formed from the water-soluble thickener (A), the cross-linking agent (B), and the particulate polymer (C).

9. A secondary battery comprising: the negative electrode according to claim 7 ; a positive electrode; an electrolyte solution; and a separator.

10. The binder composition for a secondary battery, according to claim 1 , wherein an aliphatic conjugated diene monomer that constitutes the aliphatic conjugated diene monomer units of the particulate polymer (C) is at least one selected from the group consisting of 1,3-butadiene, 2-methyl-1,3-butadiene, 2,3-dimethyl-1,3-butadiene, 2-chloro-1,3-butadiene, substituted straight-chain conjugated pentadienes, and substituted and side chain conjugated hexadienes.

11. The binder composition for a secondary battery, according to claim 1 , wherein content percentage of the aliphatic conjugated diene monomer units contained in the particulate polymer (C) is 20% by mass or more and 70% by mass or less.

12. The slurry composition for a secondary battery, according to claim 6 , wherein an aliphatic conjugated diene monomer that constitutes the aliphatic conjugated diene monomer units of the particulate polymer (C) is at least one selected from the group consisting of 1,3-butadiene, 2-methyl-1,3-butadiene, 2,3-dimethyl-1,3-butadiene, 2-chloro-1,3-butadiene, substituted straight-chain conjugated pentadienes, and substituted and side chain conjugated hexadienes.

13. The slurry composition for a secondary battery, according to claim 6 , wherein content percentage of the aliphatic conjugated diene monomer units contained in the particulate polymer (C) is 20% by mass or more and 70% by mass or less.

14. The binder composition for a secondary battery, according to claim 1 , wherein the gel content of the particulate polymer (C) is 50% by mass or more.

15. The slurry composition for a secondary battery, according to claim 6 , wherein the gel content of the particulate polymer (C) is 50% by mass or more.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Sep 8, 2015
From: SONOBE, KENYA
To: ZEON CORPORATION
Reel/Frame 036506/0607 →
Priority Claims (1)
JP 2013-053612 · Mar 15, 2013 · national
Continuity (1)
Related Publication 20160028087A1 · Jan 28, 2016