Method for forming TE to TM mode converter of heat-assisted magnetic recording head

Inventors: Aidan Dominic Goggin (Donnegal, IE); Kelly Elizabeth Hamilton (Derry, GB); Paula Frances McElhinney (Derry, GB); Fadi El Hallak (Derry, GB)
Assignee: Seagate Technology LLC
G11B5/4866G02B6/126G02B6/1228G02B6/132G02B6/136G02B6/2726G02B6/2766G11B5/6088G11B7/1387G11B11/1051G11B11/10506G11B2005/0021
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 10,127,938
App. No.
15/784,429
Granted
Nov 13, 2018
Kind
B2
Abstract

An apparatus includes an input coupler configured to receive light excited by a light source. A near-field transducer (NFT) is positioned at a media-facing surface of a write head. A layered waveguide is positioned between the input coupler and the NFT and configured to receive the light output from the input coupler in a transverse electric (TE) mode and deliver the light to the NFT in a transverse magnetic (TM) mode. The layered waveguide comprises a first layer extending along a light-propagation direction. The first layer is configured to receive light from the input coupler. The first layer tapers from a first cross track width to a second cross track width where the second cross track width is narrower than the first cross track width. The layered waveguide includes a second layer that is disposed on the first layer. The second layer has a cross sectional area in a plane perpendicular to the light propagation direction that increases along the light propagation direction. The cross sectional area of the second layer is smaller proximate to the input coupler and larger proximate to the NFT.

Claims (37)

1. A method for forming a write head, comprising:

depositing a first waveguide layer;

depositing a second waveguide layer adjacent to the first waveguide layer;

applying a first mask to a substrate parallel surface of the second waveguide layer creating a masked portion and an exposed portion of the second waveguide layer;

etching the exposed portion of the second waveguide layer;

applying a second mask to the substrate parallel surface of the second waveguide layer creating masked sections and exposed sections of the first and second waveguide layers; and

milling the exposed sections of both the first and the second waveguide layers, wherein the second layer has a cross sectional area in a plane perpendicular to the light propagation direction that increases along the light propagation direction, the cross sectional area being smaller proximate to an input coupler and larger proximate to a near field transducer (NFT).

2. The method of claim 1 , further comprising forming a stop layer on the first waveguide layer before depositing the second waveguide layer.

3. The method of claim 2 , wherein the stop layer comprises Yttria.

4. The method of claim 1 , further comprising after the etching, filling the etched portion with a cladding material.

5. The method of claim 1 , further comprising, after the milling, filling the milled sections with a cladding material.

6. The method of claim 1 , wherein at least one of the first waveguide layer and the second waveguide layer comprises NbO x .

7. The method of claim 1 , wherein at least one of the first mask and the second mask is applied with a tolerance of 50 nm.

8. A method for forming a write head, comprising:

depositing a first waveguide layer;

depositing a second waveguide layer adjacent to the first waveguide layer;

applying a first mask to a substrate parallel surface of the second waveguide layer creating masked portions and exposed portions of the first and second waveguide layers;

etching the exposed portions of the first and second waveguide layers;

applying a second mask to the substrate parallel surface of the second waveguide layer, the second mask creating a masked section and an exposed section of the second waveguide layer; and

milling the exposed section of the second waveguide layer, wherein the second layer has a cross sectional area in a plane perpendicular to the light propagation direction that increases along the light propagation direction, the cross sectional area being smaller proximate to an input coupler and larger proximate to a near field transducer (NFT).

9. The method of claim 8 , further comprising, after the milling, filling the milled section with a cladding material.

10. The method of claim 8 , further comprising, after the etching, filling the etched portion with a cladding material.

11. The method of claim 8 , wherein at least one of the first mask and the second mask is applied with a tolerance of 50 nm.

12. A method for forming a write head, comprising:

depositing a waveguide layer;

applying a first mask to a substrate parallel surface of the waveguide layer creating a first masked portion and a first exposed portion of the waveguide layer;

etching the first exposed portion of the waveguide layer;

applying a second mask to the substrate parallel surface of the waveguide layer, the second mask creating a second masked portion and a second exposed portion; and

milling the second exposed portion of the waveguide layer, wherein the waveguide layer has a cross sectional area in a plane perpendicular to the light propagation direction that increases along the light propagation direction, the cross sectional area being smaller proximate to an input coupler and larger proximate to a near field transducer (NFT).

13. The method of claim 12 , wherein etching the first exposed portion of the waveguide layer comprises etching the first exposed portion of the waveguide layer to a predetermined thickness.

14. The method of claim 13 , wherein the predetermined thickness is about half of a total thickness of the waveguide layer.

15. The method of claim 13 , wherein milling the second exposed portion of the waveguide layer comprises milling the second exposed portion to a total thickness of the waveguide layer.

16. The method of claim 12 , wherein etching the first exposed portion of the waveguide layer comprises etching the first exposed portion of the waveguide layer to a total thickness of the waveguide layer.

17. The method of claim 16 , wherein milling the second exposed portion of the waveguide layer comprises milling the second exposed portion to a predetermined thickness of the waveguide layer.

18. The method of claim 17 , wherein the predetermined thickness is about half of the total thickness of the waveguide layer.

19. The method of claim 12 , further comprising, after the etching, filling the milled portion with a cladding material.

20. The method of claim 12 , after the etching, filling the etched portion with a cladding material.