IP Library Granted Patent US 10,156,002
Granted Patent B2
US 10,156,002 · App. 15/546,038 · Granted Dec 18, 2018

Method for recovering scandium

Inventors: Ryoma Yamaguma (Niihama, JP); Tatsuya Higaki (Niihama, JP); Hidemasa Nagai (Niihama, JP); Satoshi Asano (Niihama, JP); Hiroshi Kobayashi (Niihama, JP)
Assignee: SUMITOMO METAL MINING CO., LTD.
C22B3/42C22B3/22C22B3/44C22B59/00Y02P10/234
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 10,156,002
App. No.
15/546,038
Granted
Dec 18, 2018
Kind
B2
Abstract

Provided is a method for recovering scandium with which scandium can be efficiently recovered as high purity scandium oxide from a scandium-containing solution containing impurities such as iron without causing problems such as increased cost and safety problems. According to the method for recovering scandium according to the present invention, the pH of a solution containing scandium and iron (scandium-containing solution) is adjusted within the range of not less than −0.5 and less than 1, then scandium oxalate is obtained by adding the pH adjusted solution to an oxalic acid solution, and the scandium oxalate is roasted into scandium oxide.

Claims (6)

1. A method for recovering scandium, comprising:

adjusting pH of a solution containing scandium and iron to a range of 0.5 to less than 1 wherein the scandium-containing solution contains divalent iron ions;

adding the solution after the pH adjustment to an oxalic acid solution filled in a reaction vessel to obtain scandium oxalate; and

roasting the scandium oxalate to convert the scandium oxalate into scandium oxide.

2. The method for recovering scandium according to claim 1 , wherein the scandium-containing solution before the pH adjustment is obtained by subjecting a solution containing scandium to an ion exchange treatment and a solvent extraction treatment.

3. The method of recovering scandium according to claim 1 , wherein in adding the solution after the pH adjustment to the oxalic acid solution, when the amount of oxalic acid required to convert scandium into scandium oxalate is defined as 1 equivalence, the amount of the oxalic acid solution is set to be in the range of 1.4 equivalence to 2.0 equivalences of scandium contained in the scandium-containing solution.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jul 25, 2017
From: HIGAKI, TATSUYA; NAGAI, HIDEMASA; ASANO, SATOSHI; KOBAYASHI, HIROSHI