US 10,207,361 · App. 14/693,515 · Granted Feb 19, 2019

Method and processing machine for piercing, drilling, or cutting metal workpieces

Inventors: Martin Spiess (Gerlingen, DE); Markus Blaschka (Schoenaich, DE)
Assignee: TRUMPF Werkzeugmaschinen GmbH + Co. KG
B23K26/032B23K26/0622B23K26/0876B23K26/36B23K26/382B23K37/0235B23K37/0408B23K2101/18
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 10,207,361
App. No.
14/693,515
Granted
Feb 19, 2019
Kind
B2
Abstract

The disclosure relates to methods and systems for piercing, drilling, or cutting metal workpieces in a laser processing operation. The methods include focusing a pulsed laser beam onto a processing location on a workpiece; detecting process radiation emitted from the processing location; determining an intensity of the process radiation at a plurality of temporally sequential times during pulse pauses; determining an intensity gradient of the process radiation; comparing the intensity gradient with a gradient threshold value; and detecting a spontaneous material removal on the workpiece when the number of times the gradient threshold value has been exceeded is above a predetermined limit value. When a spontaneous material removal is detected, the system changes one or both of a laser parameter and a processing parameter of the laser processing operation. The disclosure also relates to processing machines for carrying out the methods.

Claims (22)

1. A method for piercing, drilling, or cutting metal workpieces in a laser processing operation, the method comprising:

causing a laser processing machine to generate a pulsed laser beam with a laser pulse duration of t LP and a pulse pause duration of t PP ;

focusing the pulsed laser beam onto a processing location on a workpiece;

detecting process radiation emitted from the processing location;

determining a time (t PP,S ) at which a pulse pause follows a laser pulse of the pulsed laser beam;

determining an intensity (I P1 , I P2 , I P3 ,...) of the process radiation at a plurality of temporally sequential times (t M1 , t M2 , t M3 , ...) during the pulse pause;

determining at several times a gradient (dI P1-P2 /dt, dI P2-P3 /dt,...) of the intensity (I P ) of the process radiation between two of the temporally sequential times (t M1 , t M2 ; t M2 , t M3 );

comparing the gradient (dI P1-P2 /dt, dI P2-P3 /dt,...) with a gradient threshold value (dl P,S /dt);

detecting a spontaneous material removal on the workpiece when a number of times the gradient threshold value (dl P,S /dt) has been exceeded is above a predetermined limit value;

when the spontaneous material removal is detected, changing, via a control device of the laser or of the laser processing machine, one or both of

(i) at least one laser parameter (t LP , t PP ) of the pulsed laser beam, and

(ii) at least one processing parameter of the laser processing operation; and

causing the laser processing machine to generate a subsequent pulsed laser beam pursuant to the changed one or both of the at

least one laser parameter (t LP , t PP ) and the at least one processing parameter.

2. The method according to claim 1 , further comprising continuously determining an averaged intensity (<I P >) of a detected process radiation averaged over a previous duration of the laser processing operation, and wherein detecting a spontaneous material removal comprises comparing the intensity (I P ) of the process radiation in the pulse pause with an intensity threshold value (I P,S ) that is dependent on the averaged intensity (<I P >).

3. The method according to claim 1 , wherein at least one laser parameter (t LP , t PP ) of the pulsed laser beam is changed when a spontaneous material removal is detected.

4. The method according to claim 3 , wherein changing at least onc laser parameter comprises delaying or preventing a renewed impact of the pulsed laser beam on the workpiece when a spontaneous material removal is detected.

5. The method according to claim 1 , wherein at least one processing parameter of the laser processing operation is changed when a spontaneous material removal is detected.

6. The method according claim 1 , wherein when a spontaneous material removal is detected, changing one or both of

(i) at least one laser parameter (t LP , t PP ) of the pulsed laser beam, and

(ii) at least one processing parameter of the laser processing operation

occurs only when a tolerance threshold value (dI P,DS /dt) of the gradient (dI P1-P2 /dt, dI P2-P3 /dt,...) is exceeded.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jun 12, 2015
From: SPIESS, MARTIN; BLASCHKA, MARKUS
To: TRUMPF WERKZEUGMASCHINEN GMBH + CO. KG
Reel/Frame 035826/0954 →
Priority Claims (1)
DE 10 2012 219 196 · Oct 22, 2012 · national
Continuity (2)
Continuation PCTEP2013071897 · Oct 18, 2013
Related Publication 20150224600A1 · Aug 13, 2015