IP Library › Granted Patent US 10,335,894
Granted Patent B2
US 10,335,894 · App. 14/605,638 · Granted Jul 2, 2019

Joining method

Inventors: Hisashi Hori (Shizuoka, JP); Nobushiro Seo (Shizuoka, JP)
Assignee: NIPPON LIGHT METAL COMPANY, LTD.
B23K20/1225B23K20/122B23K20/1265B23K2103/04
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 10,335,894
App. No.
14/605,638
Granted
Jul 2, 2019
Kind
B2
Abstract

A joining method includes a butting process configured to butt a first metal member and a second metal member each having a front surface with various heights to form therebetween a butt portion with various heights; and a welding process configured to apply a friction stirring to the butt portion by a stirring pin of a rotation tool while only the stirring pin of the rotation tool contacts with the first metal member and the second metal member of the butt portion. The welding process may be configured to insert the stirring pin of the rotation tool into the butt portion from front surfaces of the first metal member and the second metal member and apply the friction stirring to the butt portion while an insertion depth of only the stirring pin is kept approximately constant.

Claims (14)

1. A joining method comprising:

a butting process configured to butt a first metal member and a second metal member each having a front surface with various heights against each other to form therebetween a butt portion with varying heights, wherein the butt portion includes at least two flat sections, at least one upward inclined section and at least one downward inclined section; and

a welding process configured to apply a friction stirring to the butt portion by a stirring pin of a rotation tool, the stirring pin being maintained at a constant insertion depth with respect to at least one of the first and the second metal member across the flat sections and said upward and downward inclined sections of the butt portion,

wherein only the stirring pin contacts both the first metal member and the second metal member at the insertion depth generating only frictional heat and the stirring pin has a tapered shape so as to have a smaller diameter in a hanging down direction and includes only one outer circumferential surface having only one continuous spiral groove engraved only in the outer circumferential surface engaging the first metal member and the second metal member, and

wherein the spiral groove extends counterclockwise from a proximal end side to a distal end side of the outer circumferential surface of the stirring pin, while the rotation tool rotates clockwise, and the spiral groove extends clockwise from a proximal end side to a distal end side of the outer circumferential surface of the stirring pin, while the rotation tool rotates counterclockwise.

2. A joining method comprising:

a stacking process configured to stack a first metal member on a second metal member, with a back surface of the first metal member in contact with a front surface of the second metal member, to form a lap portion therebetween, the first metal member having various heights at least at the back surface thereof, the second metal member having various heights at least at the front surface thereof, wherein the lap portion includes at least two flat sections, at least one upward inclined section and at least one downward inclined section; and

a welding process configured to insert a stirring pin of a rotation tool into the first metal member from a front surface of the first metal member toward the lap portion and apply a friction stirring to the lap portion by the stirring pin of the rotation tool, the stirring pin being maintained at a constant insertion depth with respect to at least one of the first and the second metal member across the flat sections and said upward and downward inclined sections of the lap portion,

wherein only the stirring pin contacts both the first metal member and the second metal member at the insertion depth generating only frictional heat and the stirring pin has a tapered shape so as to have a smaller diameter in a hanging down direction and includes only one outer circumferential surface having only one continuous spiral groove engraved only in the outer circumferential surface engaging the first metal member and the second metal member, and

wherein the spiral groove extends counterclockwise from a proximal end side to a distal end side of the outer circumferential surface of the stirring pin, while the rotation tool rotates clockwise, and the spiral groove extends clockwise from a proximal end side to a distal end side of the outer circumferential surface of the stirring pin, while the rotation tool rotates counterclockwise.

3. The joining method according to claim 1 , wherein a friction stirring is performed with a rotation center axis of the rotation tool always disposed in parallel with the vertical axis.

4. The joining method according to claim 2 , wherein a friction stirring is performed with a rotation center axis of the rotation tool always disposed in parallel with the vertical axis.

5. The joining method according to claim 1 , wherein a friction stirring is performed with a rotation center axis of the rotation tool always disposed perpendicularly to joint surfaces.

6. The joining method according to claim 2 , wherein a friction stirring is performed with a rotation center axis of the rotation tool always disposed perpendicularly to a boundary surface of the lap portion.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jan 27, 2015
From: HORI, HISASHI; SEO, NOBUSHIRO
To: NIPPON LIGHT METAL COMPANY, LTD.
Reel/Frame 034816/0828 →
Priority Claims (3)
JP 2014-012551 · Jan 27, 2014 · national
JP 2014-075625 · Apr 1, 2014 · national
JP 2014-107666 · May 26, 2014 · national
Continuity (1)
Related Publication 20150209893A1 · Jul 30, 2015