IP Library Granted Patent US 10,371,213
Granted Patent B2
US 10,371,213 · App. 14/563,849 · Granted Aug 6, 2019

System, method and apparatus for tolerance ring control of slip interface sliding forces

Inventors: Andrew R. Slayne (Bristol, GB); Parag Natu (Neuss, DE)
Assignee: SAINT-GOBAIN PERFORMANCE PLASTICS RENCOL LIMITED
F16D1/0835F16C27/02F16D3/06F16D7/021Y10T156/1041Y10T403/7058Y10T403/7061
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 10,371,213
App. No.
14/563,849
Granted
Aug 6, 2019
Kind
B2
Abstract

A tolerance ring comprising a metallic band for spring features and a complementary low friction material for frictional considerations is disclosed. The tolerance ring is designed to operate within a precisely controlled torque or axial force band to provide a defined amount of resistance and sliding force control between components that move relative to each other. Isolated portions of the tolerance ring form regions of contact with adjacent ones of the components. Other surfaces of the tolerance ring comprise portions with spring features that have geometry suitable for their spring rate, rather than conforming to mating surfaces of the adjacent components.

Claims (31)

1. A method of forming a tolerance ring comprising:

providing a strip of resilient material comprising spring steel having a radial thickness of 0.1 to 0.7 mm;

laminating a low friction layer comprising a fluoropolymer to the strip of resilient material to form a layered structure; and

forming projections in the layered structure, wherein the projection are axially-elongated ridges with rounded peaks, wherein the tolerance ring comprises a rim disposed at an axial end, and wherein the tolerance ring is adapted to provide at least one of: a radial stiffness that is greater than 20,000 N/mm, a axial sliding force in a range of 10 to 600 N, or a slip torque in a range of 1 to 25 Nm, wherein the coefficient of friction provided by the low friction layer is in a range of about 0.04 to 0.25, wherein the projections are adapted to be compressed between inner and outer components such that the tolerance ring operates in a flattened portion of a compression/retention force characteristic whereby the projections initially exhibit elastic behavior and are plastically deformed.

2. The method of claim 1 , further comprising:

bending the layered structure into a curved shape.

3. The method of claim 2 , wherein bending the layered structure is performed so as to define a ring including an axial gap.

4. The method of claim 1 , wherein the step of forming the projections is performed by stamping.

5. The method of claim 1 , wherein the low friction layer comprises a flexible material.

6. The method of claim 1 , wherein forming the projections is performed such that each projection is spaced apart from a neighboring projection by a flat section.

7. The method of claim 6 , wherein the rim is contiguous with the flat sections.

8. The method of claim 1 , wherein the step of laminating the low friction layer is performed with an adhesive disposed between the low friction layer and the strip of resilient material.

9. The method of claim 1 , wherein corrosion resistant coating is applied to a surface of the resilient material, wherein the corrosion resistant coating comprises an epoxy layer.

10. A method of forming a tolerance ring comprising:

providing a layered structure including laminating a strip of resilient material comprising spring steel having a radial thickness of 0.1 to 0.7 mm and a low friction layer comprising a fluoropolymer;

forming projections in the layered structure; and

bending the layered structure into a curved shape, wherein the projections are axially-elongated ridges with rounded peaks, wherein the tolerance ring comprises a rim disposed at an axial end, and wherein the tolerance ring is adapted to provide at least one of: a radial stiffness that is greater than 20,000 N/mm, a axial sliding force in a range of 10 to 600 N, or a slip torque in a range of 1 to 25 Nm, wherein the coefficient of friction provided by the low friction layer is in a range of about 0.04 to 0.25, wherein the projections are adapted to be compressed between inner and outer components such that the tolerance ring operates in a flattened portion of a compression/retention force characteristic whereby the projections initially exhibit elastic behavior and are plastically deformed.

11. The method of claim 10 , wherein the step of forming the projections is performed by stamping.

12. The method of claim 10 , wherein bending the layered structure is performed so as to define a ring including an axial gap.

13. The method of claim 10 , wherein the step of forming the projections is performed such that each projection comprises tapered shoulders.

14. The method of claim 10 , wherein the step of providing a layered structure is performed by:

providing a strip of resilient material; and

laminating a low friction layer to the strip of resilient material to form a layered structure.

15. The method of claim 14 , wherein the step of laminating the low friction layer is performed with an adhesive disposed between the low friction layer and the strip of resilient material.

16. A method of forming a tolerance ring comprising:

providing a strip of resilient material comprising spring steel having a radial thickness of 0.1 to 0.7 mm;

laminating a low friction layer comprising a fluoropolymer to the strip of resilient material to form a layered structure;

forming projections in the layered structure, wherein the projections are axially-elongated ridges with rounded peaks; and

bending the layered structure into a curved shape such that the low friction layer is disposed radially inside of the strip of resilient material, wherein the tolerance ring comprises a rim disposed at an axial end, and wherein the tolerance ring is adapted to provide at least one of: a radial stiffness that is greater than 20,000 N/mm, a axial sliding force in a range of 10 to 600 N, or a slip torque in a range of 1 to 25 Nm, wherein the coefficient of friction provided by the low friction layer is in a range of about 0.04 to 0.25, wherein the projections are adapted to be compressed between inner and outer components such that the tolerance ring operates in a flattened portion of a compression/retention force characteristic whereby the projections initially exhibit elastic behavior and are plastically deformed.

17. The method of claim 16 , wherein the step of laminating the low friction layer is performed with an adhesive disposed between the low friction layer and the strip of resilient material.

18. The method of claim 16 , wherein laminating the corrosion resistant coating is performed prior to forming the projections.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Feb 18, 2016
From: SLAYNE, ANDREW R; NATU, PARAG
To: SAINT-GOBAIN PERFORMANCE PLASTICS RENCOL LIMITED
Reel/Frame 037761/0744 →
Continuity (4)
Continuation 13947789 · Jul 22, 2013
Continuation 12884383 · Sep 17, 2010
Provisional Application 61245883 · Sep 25, 2009
Related Publication 20150114549A1 · Apr 30, 2015
Cited By (1)
US 12,247,618