IP Library › Granted Patent US 10,561,405
Granted Patent B2
US 10,561,405 · App. 15/487,046 · Granted Feb 18, 2020

Method for manufacturing a biological fluid sensor

Inventors: Adam Pizer (Jeffersonville, IN); Dalton Pont (Sterling, VA); John V. Chiochetti (Annapolis, MD)
Assignee: CORESYTE, INC.
A61B10/0064A61B5/1477A61B5/14517A61B5/4266A61B5/6833B23K1/008B23K1/0016B23K26/38B23K26/384B23K26/389B23K26/402B29C69/00G01N33/48707A61B2562/0295A61B2562/12A61B2562/125A61B2562/164A61B2562/166B23K2101/36B23K2101/42B23K2103/172B23K2103/42B29K2027/06B29K2995/0005B29L2009/008B29L2031/34B29L2031/753H05K1/16H05K2201/10151
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 10,561,405
App. No.
15/487,046
Granted
Feb 18, 2020
Kind
B2
Abstract

The present invention presents a method of fabrication for a physiological sensor with electronic, electrochemical, and chemical components. The fabrication method comprises steps for manufacturing an apparatus comprising at least one electrochemical sensor, a microcontroller, and a transceiver. The fabrication process includes the steps of substrate fabrication, circuit fabrication, pick and place, reflow soldering, electrode fabrication, membrane fabrication, sealing and curing, layer bonding, and dressing. The physiological sensor is operable to analyze biological fluids such as sweat.

Claims (71)

1. A method of fabrication for a biological fluid sensor for analyzing at least one analyte in human biological fluid, said biological fluid sensor comprising electronic components, electrochemical components, and chemical components, the method comprising:

fabricating at least one substrate;

fabricating at least one circuit on the at least one substrate;

picking and placing the electronic components onto the at least one circuit, wherein the electronic components include at least one microcontroller and at least one transceiver;

reflow soldering of the at least one circuit;

fabricating at least two electrodes, wherein the at least two electrodes are comprised of at least one active electrode and at least one reference electrode;

applying an ionophore coating on the at least one active electrode;

sealing the at least one active electrode to create an electronic layer; and

integrating the electronic layer with a top cover layer, a microfluidic management layer, and a double-sided adhesive layer;

wherein the step of fabricating the at least two electrodes further comprises:

fabricating a metallization paste;

constructing the least one reference electrode by applying the metallization paste on top of at least one first trace metal of the at least one circuit and annealing; and

constructing the least one active electrode by applying the metallization paste on top of at least one second trace metal of the at least one circuit and annealing; and

wherein the step of integrating the electronic layer with the top cover layer, the microfluidic management layer, and the double-sided adhesive layer further comprises:

cutting the top cover layer, wherein the top cover layer has an adhesive side;

placing the electronic layer on top of the adhesive side of the top cover layer, wherein the at least two electrodes are facing up;

cutting the microfluidic management layer;

surrounding the at least two electrodes with the microfluidic management layer;

cutting a sheet of double-sided adhesive to create the double-sided adhesive layer;

placing the double-sided adhesive layer on top of the electronic layer such that the double-sided adhesive layer covers the electronic layer; and

pressing the top cover layer, the microfluidic management layer, the electronic layer, and the double-sided adhesive layer for permanent bond;

wherein the at least one substrate includes an active electrode substrate and a reference electrode substrate,

wherein the active electrode substrate includes the at least one active electrode and the reference electrode substrate includes the at least one reference electrode, and

wherein the step of applying the ionophore coating on the at least one active electrode is performed using a multilayer substrate approach comprising:

casting an ionophore in a well of the reference electrode substrate;

placing an adhesive layer or a bonding film layer on top of the active electrode substrate; and

attaching the reference electrode substrate to the active electrode substrate using the adhesive layer or the bonding film layer.

2. The method of claim 1 , wherein the biological fluid is sweat.

3. The method of claim 1 , wherein the metallization paste is made of at least one stable metal selected from the group consisting of silver, gold, platinum, and palladium.

4. The method of claim 1 , wherein the at least one reference electrode and the at least one active electrode include silver, zinc, copper, gold, platinum, rhodium, carbon, and a combination thereof.

5. The method of claim 1 , wherein applying the ionophore coating on the at least one active electrode is performed via an automated dispenser.

6. The method of claim 1 , further including curing the ionophore coating using heat and light.

7. The method of claim 1 , wherein a conductive trace is in a ring around the well, wherein the conductive trace does not contact the well, wherein the at least one active electrode is within the well.

8. The method of claim 1 , wherein the ionophore coating is fabricated by dissolving an ion selective material in a polyvinylchloride (PVC) solution.

9. The method of claim 1 , wherein the ionophore coating is cast in a shape and placed on a carrier or a film to facilitate application on the at least one electrode.

10. The method of claim 9 , wherein the carrier or the film becomes an integral part of the biological fluid sensor.

11. The method of claim 1 , wherein the ionophore coating has an embedded glass or plastic fiber.

12. The method of claim 1 , wherein the microfluidic layer is comprised of one or more of wicking paper, fabric, and crystal fibers.

13. The method of claim 1 , wherein the at least one analyte is one or more of sodium, potassium, chloride, oxygen, glucose, calcium, ammonium, copper, magnesium, iron, zinc, lactate, creatinine, uric acid, urea, ethanol, amino acids, hormones, steroids, proteins, catecholamines, and interleukins.

14. The method of claim 1 , wherein the double-sided adhesive layer further contains laser cut macrofluidic pores.

15. The method of claim 1 , wherein the step of integrating the electronic layer with the top cover layer, the microfluidic management layer, and the double-sided adhesive layer further includes:

mechanically separating an individual unit; and

automatically packaging the individual unit into an individualized wrapper to create an individually wrapped unit.

16. A method of fabrication for a biological fluid sensor for analyzing at least one analyte in human biological fluid, said biological fluid sensor comprising electronic components, electrochemical components, and chemical components, the method comprising:

fabricating at least one substrate;

fabricating at least one circuit on the at least one substrate;

picking and placing the electronic components onto the at least one circuit, wherein the electronic components include at least one microcontroller and at least one transceiver;

reflow soldering of the at least one circuit;

fabricating at least two electrodes, wherein the at least two electrodes are comprised of at least one active electrode and at least one reference electrode;

applying an ionophore coating on the at least one active electrode;

sealing the at least one active electrode to create an electronic layer; and

integrating the electronic layer with a top cover layer, a microfluidic management layer, and a double-sided adhesive layer;

wherein the step of fabricating the at least two electrodes further comprises:

fabricating a metallization paste;

constructing the least one reference electrode by applying the metallization paste on top of at least one first trace metal of the at least one circuit and annealing; and

constructing the least one active electrode by applying the metallization paste on top of at least one second trace metal of the at least one circuit and annealing; and

wherein the step of integrating the electronic layer with the top cover layer, the microfluidic management layer, and the double-sided adhesive layer further comprises:

cutting the top cover layer, wherein the top cover layer has an adhesive side;

placing the electronic layer on top of the adhesive side of the top cover layer, wherein the at least two electrodes are facing up;

cutting the microfluidic management layer;

surrounding the at least two electrodes with the microfluidic management layer;

cutting a sheet of double-sided adhesive to create the double-sided adhesive layer;

placing the double-sided adhesive layer on top of the electronic layer such that the double-sided adhesive layer covers the electronic layer; and

pressing the top cover layer, the microfluidic management layer, the electronic layer, and the double-sided adhesive layer for permanent bond;

wherein a conductive trace is in a first ring around the at least one active electrode, wherein the conductive trace in the first ring around the at least one active electrode does not contact the at least one active electrode, and wherein the step of applying the ionophore coating on the at least one active electrode is performed using a surface tension dam approach comprising:

printing, depositing, or adhering a soldermask, a printed ink, or a non-conductive material on the at least one substrate in a second ring around the at least one active electrode, wherein the second ring around the at least one active electrode is inside the first ring around the at least one active electrode, and wherein the first ring around the at least one active electrode does not contact the second ring around the at least one active electrode; and

applying the ionophore coating on the at least one active electrode via liquid deposition such that the ionophore coating completely covers the at least one active electrode and is contained within the second ring formed by the soldermask, the printed ink, or the non-conductive material; and

wherein the non-conductive material is a different material than the at least one substrate.

17. The method of claim 16 , wherein the biological fluid is sweat.

18. The method of claim 16 , wherein the double-sided adhesive layer further contains laser cut macrofluidic pores.

19. The method of claim 16 , wherein the ionophore coating is fabricated by dissolving an ion selective material in a polyvinylchloride (PVC) solution.

Assignments (4)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Apr 13, 2017
From: CHIOCHETTI, JOHN V.
To: CORESYTE, INC.
Reel/Frame 042003/0387 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Apr 13, 2017
From: PONT, DALTON
To: CORESYTE, INC.
Reel/Frame 042003/0496 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Apr 13, 2017
From: PIZER, ADAM
To: KEY ELECTRONICS, INC.
Reel/Frame 042003/0543 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Apr 13, 2017
From: KEY ELECTRONICS, INC.
To: CORESYTE, INC.
Reel/Frame 042003/0581 →
Continuity (4)
Continuation In Part 15177703 · Jun 9, 2016
Continuation 15019006 · Feb 9, 2016
Provisional Application 62130047 · Mar 9, 2015
Related Publication 20170223844A1 · Aug 3, 2017
Cited By (1)