Laser welding of copper with reaction materials

Inventors: James G. Schroth (Troy, MI); Thomas A. Perry (Bruce Township, MI); Hongliang Wang (Sterling Heights, MI); Chen Zhou (Troy, MI)
Assignee: GM Global Technology Operations, LLC
B23K1/0006B23K1/0056B23K1/18B23K2101/32B23K2103/12
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 10,576,565
App. No.
15/273,923
Granted
Mar 3, 2020
Kind
B2
Abstract

A method of forming a weld interface between a first workpiece and a second workpiece includes arranging a reactive braze material at a first joining surface of the first workpiece. The reactive material is selected to react upon being heated to a temperature below the solidus temperature of the first and second workpieces to form a liquid-containing reaction product. Furthermore, an assembly is prepared of the first workpiece and the second workpiece with the first joining surface of the first workpiece and a second joining surface of the second workpiece separated by the reactive material. The second workpiece is then heated with a first laser beam following a first path and with a second laser beam following a second path.

Claims (31)

1. A method of forming a weld interface between a first workpiece and a second workpiece, the method comprising:

arranging a reactive braze material at a first joining surface of the first workpiece, the reactive braze material being selected to react upon being heated to a temperature below the solidus temperature of the first and second workpieces to form a liquid-containing reaction product;

preparing an assembly of the first workpiece and the second workpiece by placing the first workpiece into a rectangular opening in the second workpiece so that the first joining surface of the first workpiece and a second joining surface of the second workpiece are separated by the reactive braze material, and so that the first workpiece is provided in a perpendicular arrangement with the second workpiece;

directly heating the second workpiece at an upper surface thereof with a first, green laser beam and directly heating only the second workpiece at a lower surface of the second workpiece with a second, green laser beam, wherein the first green laser beam follows a first weld path and the second green laser beam follows a second weld path, the second weld path has a greater weld path length than the first weld path; and

delaying solidification of the liquid-containing reaction product at the lower surface of the second workpiece by adjusting an input energy of one or more of the first green laser beam and the second green laser beam, and

wherein the first workpiece is an insulated wire.

2. The method of claim 1 , wherein the first and second workpieces are metal or metal alloys of copper.

3. The method of claim 1 , wherein the reactive material is at least one metal element of copper, silicon, zinc, aluminum, or magnesium, or alloys thereof.

4. The method of claim 1 , further comprising forming a solid-state welded joint between the first and second joining surfaces.

5. The method of claim 1 , wherein the first workpiece is joined at a T-joint with the second workpiece.

6. The method of claim 5 , further comprising arranging the first workpiece to extend from the lower surface of the second workpiece, such that only the first weld path of the first laser beam directly heats the first workpiece.

7. A method of forming a weld interface between a first workpiece and a second workpiece, the method comprising:

arranging a reactive braze material at a first joining surface of the first workpiece, the reactive braze material being selected to react upon being heated to a temperature below the solidus temperature of the first and second workpieces to form a liquid-containing reaction product;

preparing an assembly of the first workpiece and the second workpiece placing the first workpiece into a rectangular opening in the second workpiece so that the first joining surface of the first workpiece and a second joining surface of the second workpiece are separated by the reactive braze material, and so that the first workpiece is provided in a perpendicular arrangement with the second workpiece;

directly heating the second workpiece at an upper surface thereof with a first, green laser beam and with a second, infrared laser beam, wherein the first green laser beam follows a first weld path and the second infrared laser beam subsequently follows the first weld path, and wherein a weld bead is formed at a lower surface of the second workpiece in response to heat energy from the second infrared laser beam; and

delaying solidification of the liquid-containing reaction product at the lower surface of the second workpiece by adjusting an input energy of one or more of the first green laser beam and the second infrared laser beam, and

wherein the first workpiece is an insulated wire.

8. The method of claim 7 , wherein the first and second workpieces are metal or metal alloys of copper.

9. The method of claim 7 , wherein the reactive braze material includes at least one metal element of copper, silicon, zinc, aluminum, or magnesium, or alloys thereof.

10. The method of claim 7 , further comprising forming a solid-state welded joint between the first and second joining surfaces.

11. The method of claim 7 , further comprising arranging the first workpiece to extend from the lower surface of the second workpiece and into the opening in the second workpiece, such that both the first and second laser beams approach the assembly from the upper surface of the second workpiece.

12. A method of forming a weld interface between a first workpiece and a second workpiece, the method comprising:

arranging a reactive braze material at a first joining surface of the first workpiece, the reactive braze material being selected to react upon being heated to a temperature below the solidus temperature of the first and second workpieces to form a liquid-containing reaction product;

preparing an assembly of the first workpiece and the second workpiece by placing the first workpiece into a rectangular opening in the second workpiece so that the first joining surface of the first workpiece and a second joining surface of the second workpiece are separated by the reactive braze material, and so that the first workpiece is provided in a perpendicular arrangement with the second workpiece;

directly heating the second workpiece with a first laser beam following a first weld path and with a second laser beam following a second weld path, wherein the first and second workpieces are metal or metal alloys of copper, and wherein the first laser beam is a green laser beam; and

delaying solidification of the liquid-containing reaction product at a lower surface of the second workpiece by adjusting an input energy of one or more of the first laser beam and the second laser beam, and

wherein the first workpiece is an insulated wire.

13. The method of claim 12 , wherein the reactive braze material includes at least one metal element of copper, silicon, zinc, aluminum, or magnesium, or alloys thereof.

14. The method of claim 12 , further comprising forming a solid-state welded joint between the first and second joining surfaces.

15. The method of claim 12 , further comprising arranging the first workpiece to perpendicularly extend from the lower surface of the second workpiece, and wherein the first laser beam approaches the assembly from the upper surface of the second workpiece and the second laser beam approaches the assembly from the lower surface of the second workpiece.

16. The method of claim 12 , further comprising arranging the first workpiece to perpendicularly extend from the lower surface of the second workpiece, and wherein both the first and second laser beams approach the assembly from the upper surface of the second workpiece.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Sep 27, 2016
From: SCHROTH, JAMES G.; PERRY, THOMAS A.; WANG, HONGLIANG; ZHOU, CHEN
To: GM GLOBAL TECHNOLOGY OPERATIONS LLC
Reel/Frame 039865/0324 →
Continuity (1)
Related Publication 20180085855A1 · Mar 29, 2018
Cited By (1)
US 12,420,360