Method for manufacturing slurry for positive electrode of nonaqueous electrolyte secondary battery and apparatus therefor
A method for manufacturing a slurry for a positive electrode of a nonaqueous electrolyte secondary battery using an aqueous solvent containing an alkali metal complex oxide, includes: while causing a raw material slurry containing a solid content and the solvent as slurry raw materials for a positive electrode of the nonaqueous electrolyte secondary battery to flow along a path, performing a neutralization treatment on an alkali component in the raw material slurry by inorganic carbon supplied to the raw material slurry flowing along the path.
1. A method for manufacturing a slurry for a positive electrode of a nonaqueous electrolyte secondary battery using an aqueous solvent containing an alkali metal complex oxide, comprising:
while causing a raw material slurry containing a solid content and the solvent as slurry raw materials for a positive electrode of the nonaqueous electrolyte secondary battery to flow along a path, performing a neutralization treatment on an alkali component in the raw material slurry by inorganic carbon supplied to the raw material slurry flowing along the path.
2. The method for manufacturing a slurry for a positive electrode of a nonaqueous electrolyte secondary battery according to claim 1 , further comprising:
a pre-process of producing the raw material slurry by supplying, while causing the solvent as the slurry raw material for a positive electrode of the nonaqueous electrolyte secondary battery to flow along the path, the solid content as the slurry raw material for a positive electrode of the nonaqueous electrolyte secondary battery to the solvent flowing along the path,
wherein the neutralization treatment is performed on the alkali component in the raw material slurry by supplying the inorganic carbon to the raw material slurry flowing along the path.
3. The method for manufacturing a slurry for a positive electrode of a nonaqueous electrolyte secondary battery according to claim 1 ,
wherein the neutralization treatment is performed on the alkali component in the raw material slurry while producing the raw material slurry by supplying, while causing the solvent as the slurry raw material for a positive electrode of the nonaqueous electrolyte secondary battery to flow along the path, the solid content as the slurry raw material for a positive electrode of the nonaqueous electrolyte secondary battery and the inorganic carbon to the solvent flowing along the path.
4. The method for manufacturing a slurry for a positive electrode of a nonaqueous electrolyte secondary battery according to claim 1 , further comprising:
a pre-process of dissolving the inorganic carbon in the solvent by supplying, while causing the solvent as the slurry raw material for a positive electrode of the nonaqueous electrolyte secondary battery to flow along the path, the inorganic carbon to the solvent flowing along the path,
wherein the neutralization treatment is performed on the alkali component in the raw material slurry while producing the raw material slurry by supplying the solid content as the slurry raw material for a positive electrode of the nonaqueous electrolyte secondary battery to the solvent flowing along the path and containing dissolved inorganic carbon.
5. The method for manufacturing a slurry for a positive electrode of a nonaqueous electrolyte secondary battery according to claim 1 ,
wherein the inorganic carbon is supplied to the path at a negative pressure.
6. The method for manufacturing a slurry for a positive electrode of a nonaqueous electrolyte secondary battery according to claim 1 ,
wherein the neutralization treatment is performed while causing cavitation by causing the raw material slurry, to which the inorganic carbon is supplied, to flow through a cavitation causing portion.
7. An apparatus for manufacturing a slurry for a positive electrode of a nonaqueous electrolyte secondary battery using an aqueous solvent containing an alkali metal complex oxide, comprising:
a path on which a raw material slurry containing a solid content and a solvent as slurry raw materials for a positive electrode of the nonaqueous electrolyte secondary battery flows; and
an inorganic carbon supply portion supplying inorganic carbon to the raw material slurry flowing along the path,
wherein a neutralization treatment is performed on an alkali component in the raw material slurry while causing the raw material slurry to flow along the path.
8. The apparatus for manufacturing a slurry for a positive electrode of a nonaqueous electrolyte secondary battery according to claim 7 further comprising:
unit that causes the path to be at a negative pressure,
wherein the inorganic carbon is supplied to the path at the negative pressure.
9. The apparatus for manufacturing a slurry for a positive electrode of a nonaqueous electrolyte secondary battery according to claim 8 further comprising:
a cavitation causing portion which performs the neutralization treatment while causing cavitation by causing the raw material slurry to which the inorganic carbon is supplied to flow.