IP Library › Granted Patent US 10,668,595
Granted Patent B2
US 10,668,595 · App. 15/880,817 · Granted Jun 2, 2020

Method of using laminated dressing board

Inventor: Kazuma Sekiya (Tokyo, JP)
Assignee: DISCO CORPORATION
B24B53/12B24B7/228
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 10,668,595
App. No.
15/880,817
Granted
Jun 2, 2020
Kind
B2
Abstract

A method of using a laminated dressing board is provided. In the laminated dressing board, a shape adjustment dressing layer containing first abrasive grains and used for shape adjustment of a cutting blade and a setting dressing layer containing second abrasive grains and used for setting of the shape-adjusted cutting blade are laminated. The method includes a holding step of holding the shape adjustment dressing layer side of the laminated dressing board by a chuck table, a setting dressing step of causing the cutting blade to cut into the laminated dressing board from the setting dressing layer side to form a first groove in the setting dressing layer, and a shape adjustment dressing step of causing the cutting blade to cut into the bottom of the first groove along the first groove to form a second groove in the shape adjustment dressing layer.

Claims (31)

1. A method of using a laminated dressing board in which a shape adjustment dressing layer containing first abrasive grains and used for shape adjustment of a cutting blade and a setting dressing layer containing second abrasive grains and used for setting of the shape-adjusted cutting blade are laminated, the method comprising:

a holding step of holding the shape adjustment dressing layer side of the laminated dressing board by a chuck table;

a setting dressing step of causing the cutting blade to cut into the laminated dressing board from the setting dressing layer side to form a first groove in the setting dressing layer; and

a shape adjustment dressing step of causing the cutting blade to cut into a bottom of the first groove along the first groove to form a second groove in the shape adjustment dressing layer, wherein the cutting blade used in the setting dressing step is the same cutting blade used in the shape adjustment dressing step.

2. The method of using the laminated dressing board according to claim 1 , wherein:

said setting dressing step negates dulling of a cutting edge of the cutting blade; and

said shape adjustment dressing step adjusts the shape of the cutting blade to a shape concentric with a rotary shape associated with the cutting blade.

3. The method of using the laminated dressing board according to claim 1 , wherein:

said first abrasive grains of said shape adjustment dressing layer comprise white alundum; and

said second abrasive grains of said setting dressing layer comprise green carborundum.

4. A method of using a laminated dressing board in which a shape adjustment dressing layer containing first abrasive grains and used for shape adjustment of a cutting blade and a setting dressing layer containing second abrasive grains and used for setting of the shape-adjusted cutting blade are laminated, the method comprising:

a holding step of holding the shape adjustment dressing layer side of the laminated dressing board by a chuck table;

a setting dressing step of causing the cutting blade to cut into the laminated dressing board from the setting dressing layer side to form a first groove in the setting dressing layer; and

a shape adjustment dressing step of causing the cutting blade to cut into a bottom of the first groove along the first groove to form a second groove in the shape adjustment dressing layer,

wherein the method further comprises a first shape adjustment dressing step of causing the cutting blade to cut into the laminated dressing board from the setting dressing layer side to form a third groove having such a depth as to reach the shape adjustment dressing layer, prior to the setting dressing step.

5. A method of using a laminated dressing board in which a shape adjustment dressing layer containing first abrasive grains and used for shape adjustment of a cutting blade and a setting dressing layer containing second abrasive grains and used for setting of the shape-adjusted cutting blade are laminated, the method comprising:

a holding step of holding the setting dressing layer side of the laminated dressing board by a chuck table;

a shape adjustment dressing step of causing the cutting blade to cut into the laminated dressing board from the shape adjustment dressing layer side to form a first groove; and

a setting dressing step of causing the cutting blade to cut into a bottom of the first groove along the first groove to form a second groove in the setting dressing layer,

wherein the cutting blade used in the setting dressing step is the same cutting blade used in the shape adjustment dressing step.

6. The method of using the laminated dressing board according to claim 5 , wherein:

said shape adjustment dressing step adjusts the shape of the cutting blade to a shape concentric with a rotary shape associated with the cutting blade; and

said setting dressing step negates dulling of a cutting edge of the cutting blade.

7. The method of using the laminated dressing board according to claim 5 , wherein:

said first abrasive grains of said shape adjustment dressing layer comprise white alundum; and

said second abrasive grains of said setting dressing layer comprise green carborundum.

8. A method of using a laminated dressing board in which a shape adjustment dressing layer containing first abrasive grains and used for shape adjustment of a cutting blade and a setting dressing layer containing second abrasive grains and used for setting of the shape-adjusted cutting blade are laminated, the method comprising:

a holding step of holding the setting dressing layer side of the laminated dressing board by a chuck table;

a shape adjustment dressing step of causing the cutting blade to cut into the laminated dressing board from the shape adjustment dressing layer side to form a first groove; and

a setting dressing step of causing the cutting blade to cut into a bottom of the first groove along the first groove to form a second groove in the setting dressing layer,

wherein in the shape adjustment dressing step, the cutting blade is caused to cut into the laminated dressing board to such a depth that the setting dressing layer is exposed at the bottom of the first groove.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jan 26, 2018
From: SEKIYA, KAZUMA
To: DISCO CORPORATION
Reel/Frame 044739/0068 →
Priority Claims (1)
JP 2017-013181 · Jan 27, 2017 · national
Continuity (1)
Related Publication 20180215010A1 · Aug 2, 2018