IP Library › Granted Patent US 10,695,381
Granted Patent B2
US 10,695,381 · App. 16/179,221 · Granted Jun 30, 2020

Tissue repair material derived from fish skin and manufacturing method thereof

Inventors: Horng-Ji Lai (Taipei, TW); Min-Chang Huang (Taipei, TW); Jui-Min Ho (Taipei, TW); Yun-Ting Hsu (Taipei, TW); Yu-Chi Lin (Taipei, TW); Ta-Wei Su (Taipei, TW); Kuan-Hao Huang (Taipei, TW); Yu-Wei Chang (Taipei, TW)
Assignee: BODY ORGAN BIOMEDICAL CORP.
A61K35/60A61L15/40A61L27/3604A61L27/3687A61L27/3691A61L27/52A61L2430/16A61L2430/40
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 10,695,381
App. No.
16/179,221
Granted
Jun 30, 2020
Kind
B2
Abstract

A tissue repair material derived from fish skin and manufacturing method thereof is applied to provide the tissue repair material suitable for use as a patch, a cover, a carrier, a scaffold, an implant or a reagent in various tissues. The tissue repair material has collagens to improve the wounded tissue repair, and has particular characters for desired tissue repair application. Furthermore, so far the factors of the terrestrial animal transmitted disease (caused by virus) do not survive on the tissue repair material derived from fish skin.

Claims (17)

1. A manufacturing method of a tissue repair material derived from fish skin, comprises:

obtaining a fish skin without a fish flesh;

removing fish scales, oil, cells, chromatophores and pocket structures from the fish skin to obtain a purified fish skin;

treating the purified fish skin with acidic solution to obtain a shapeable flake without breakdown; and

shaping the shapeable fish skin to obtain a shaped flake in a particular form, wherein the shaping step comprises cutting the shapeable flake to obtain the shaped flake, wherein a surface of the shaped flake is a cross section of the shapeable flake.

2. The manufacturing method according to claim 1 , further comprising washing the shaped flake with water.

3. The manufacturing method according to claim 2 , further comprising dehydrating the shaped flake before the washing step.

4. The manufacturing method according to claim 2 , further comprising dehydrating the shaped flake after the washing step.

5. The manufacturing method according to claim 4 , further comprising backwatering the shaped flake after the dehydrating steps.

6. The manufacturing method according to claim 5 , further comprising dehydrating the shaped flake after the backwatering step.

7. The manufacturing method according to claim 1 , further comprising:

extracting a collagen solution from the shapeable flake.

8. The manufacturing method according to claim 1 , further comprising:

lyophilizing the shapeable flake.

9. The manufacturing method according to claim 1 , wherein the treating step comprises:

treating the purified fish skin with acidic solution more than two times to obtain the shapeable flake without breakdown;

removing at least one outer layer of the shapeable flake between any two acid-treating steps.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Nov 2, 2018
From: LAI, HORNG-JI; HUANG, MIN-CHANG; HO, JUI-MIN; HSU, YUN-TING; LIN, YU-CHI; SU, TA-WEI; HUANG, KUAN-HAO; CHANG, YU-WEI
To: BODY ORGAN BIOMEDICAL CORP.
Reel/Frame 047396/0593 →
Continuity (3)
Division 15082441 · Mar 28, 2016
Provisional Application 62140508 · Mar 31, 2015
Related Publication 20190070224A1 · Mar 7, 2019