IP Library › Granted Patent US 10,833,324
Granted Patent B2
US 10,833,324 · App. 14/835,582 · Granted Nov 10, 2020

Electrodes with controlled amount of lithium attached and method of making same

Inventor: Linda Zhong (Oakland, CA)
Assignee: LICAP TECHNOLOGIES, INC.
H01M4/382H01M4/043H01M4/134H01M4/1395H01M4/366H01M10/052H01M2004/027
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 10,833,324
App. No.
14/835,582
Granted
Nov 10, 2020
Kind
B2
Abstract

A method for fabricating an electrode, includes: determining a thickness of an active layer; selecting a lithium (Li) foil having a specified thickness; determining a Li layer pattern for the Li foil based on a portion of a surface of the active layer to be covered by the Li foil; and pressing the Li layer pattern into the surface of the active layer.

Claims (11)

1. A method for fabricating an electrode, the method comprising:

determining thickness of an active layer;

selecting a lithium (Li) foil having a specified thickness;

specifying a ratio of a weight of the active layer to a weight of the Li foil;

determining a portion of a surface of the active layer to be covered by the Li foil based on the ratio, the portion being less than fifty percent of the surface of the active layer;

determining a Li layer pattern for the Li foil based on the portion of the surface of the active layer to be covered by the Li foil, said determining the Li layer pattern comprising selecting the Li layer pattern that minimizes a Li diffusion distance on the active layer from a plurality of Li foil pieces forming the Li layer pattern;

positioning the plurality of Li foil pieces on the surface of the active layer in the selected Li layer pattern; and

pressing the Li layer pattern into the surface of the active layer.

2. The method of claim 1 , wherein shapes of the plurality of Li foil pieces forming the Li layer pattern comprise one or more of squares, circles, and stripes.

3. The method of claim 1 , wherein the pressing the Li layer pattern into the surface of the active layer comprises applying pressure in a range of 110-120 kilograms per square centimeter (kg/cm 2 ) to Li foil pieces forming the Li layer pattern.

4. The method of claim 1 , wherein the portion of the surface of the active layer to be covered by the Li layer pattern is less than ten percent of the surface of the active layer.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Sep 10, 2019
From: ZHONG, LINDA
To: LICAP TECHNOLOGIES, INC.
Reel/Frame 050325/0059 →
Continuity (1)
Related Publication 20170062815A1 · Mar 2, 2017