Method of fabricating a friction part out of composite material

Inventors: Patrice Brender (Charvieu-Chavagneux, FR); Floriane Demeyer (Bordeaux, FR); Sylvain Jacques (Talence, FR)
Assignee: SAFRAN LANDING SYSTEMS
C04B41/4531C04B35/52C04B35/5622C04B35/80C04B35/806C04B35/83C04B41/0072C04B41/4584C04B41/5001C04B41/5057C23C16/32F16D69/023F16D69/028C04B2235/3839C04B2235/441C04B2235/48C04B2235/5248C04B2235/614C04B2235/79C04B2235/80F16D65/126F16D2200/006F16D2200/0052F16D2200/0091
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 10,836,684
App. No.
16/161,814
Granted
Nov 17, 2020
Kind
B2
Abstract

A method of fabricating a friction part out of composite material, the method including densifying a carbon yarn fiber preform with a matrix including at least pyrolytic carbon and a ZrO x C y phase, where 1≤x≤2 and 0≤y≤1, the matrix being formed by film-boiling or by chemical vapor infiltration from a first precursor for pyrolytic carbon and a second precursor that includes zirconium, the second precursor being a zirconium complex including an alcoxy or carboxylate ligand bonded to zirconium.

Claims (8)

1. A method of fabricating a friction part out of composite material, the method comprising:

densifying a carbon yarn fiber preform with a matrix comprising at least pyrolytic carbon and a ZrO x C y phase, where 1≤x≤2 and 0≤y≤1, the matrix being formed by film-boiling from a film-boiling bath comprising a first precursor for pyrolytic carbon and a second precursor that includes zirconium, the second precursor being a zirconium complex comprising an alkoxy or carboxylate ligand bonded to zirconium, wherein the ZrO x C y phase is formed by film-boiling from the second precursor, and wherein the content by weight of the second precursor in the film-boiling bath lies in the range 3% to 30%.

2. The method according to claim 1 , wherein the alcoxy or carboxylate ligand is a C 2 to C 10 ligand.

3. The method according to claim 2 , wherein the alcoxy or carboxylate ligand is selected from: propoxy ligand; butoxy ligand; or 2-ethylhexanoate ligand.

4. The method according to claim 3 , wherein the second precursor is selected from: zirconium propoxide; zirconium butoxide; zirconium ethyl-2-hexanoate; and mixtures thereof.

5. The method according to claim 1 , further comprising deoxygenation heat treatment of the ZrO x C y phase that has been formed.

6. The method according to claim 1 , wherein the optionally deoxygenated ZrO x C y phase is present in the final part at a content by weight lying in the range 0.5% to 25%.

7. The method according to claim 1 , wherein the friction part is a brake disk.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Nov 7, 2018
From: BRENDER, PATRICE; DEMEYER, FLORIANE; JACQUES, SYLVAIN
To: SAFRAN LANDING SYSTEMS