IP Library › Granted Patent US 10,843,856
Granted Patent B2
US 10,843,856 · App. 16/004,264 · Granted Nov 24, 2020

Oxo-degradable rigid and flexible packaging

Inventor: Russell Petrie (Irvine, CA)
Assignee: Okeanos Group, LLC
B65D65/466B65B31/04B32B2307/7163B32B2307/7244B32B2323/043B32B2323/046B32B2329/04B32B2367/00B32B2439/70B65D85/80B65D2565/388C09C1/021
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 10,843,856
App. No.
16/004,264
Granted
Nov 24, 2020
Kind
B2
Abstract

A container is formed from a composition including: calcium carbonate (CaCO 3 ); a polymer; and an oxo-degradable additive. The container may be sealed and an interior defined by the container may include a liquid or gas having a concentration of oxygen in a range of 0 volume percent (vol %) to 21 vol %, based on the total volume of the liquid or gas. The container may have a set oxo-biodegradation rate.

Claims (26)

1. A container formed from a composition comprising:

calcium carbonate (CaCO 3 );

a polymer; and

an oxo-degradable additive,

wherein the container comprises a side comprising at least one layer formed from the composition, and

wherein the oxo-degradable additive in said at least one layer of the side has a concentration that varies along a concentration gradient.

2. The container of claim 1 , wherein the polymer comprises polyethylene, polypropylene, polystyrene, polyethylene terephthalate, biodegradable polylactic acid polymer, polyvinyl alcohol, or any combination thereof.

3. The container of claim 1 , wherein the container is sealed and an interior defined by the container comprises a liquid or gas having a concentration of oxygen in a range of 0 volume percent (vol %) to 21 vol %, based on the total volume of the liquid or gas.

4. The container of claim 3 , wherein the container is hermetically sealed.

5. The container of claim 1 , wherein an exterior surface of the container is substantially free of the oxo-degradable additive.

6. The container of claim 1 , wherein the container has a long-term stability of 6 months or more when an interior defined by the container comprises a liquid or gas having a concentration of oxygen in a range of 0 volume percent (vol %) to 21 vol %, based on the total volume of the liquid or gas.

7. The container of claim 1 , wherein the container oxo-biodegrades in a time period of 45 years or less.

8. The container of claim 1 , wherein the composition comprises the oxo-degradable additive in an amount of 0.01 wt % to 20 wt %, based on the total weight of the composition.

9. The container of claim 1 , wherein the composition comprises the polymer in an amount of 5 wt % to 45 wt %, based on the total weight of the composition.

10. The container of claim 1 , wherein the composition comprises the calcium carbonate in an amount of 35 wt % to 94.99 wt %, based on the total weight of the composition.

11. The container of claim 1 , wherein the container has a side formed from the composition, and the side has a thickness of 1 nm to 20.32 cm.

12. The container of claim 1 , wherein the container is a food container.

13. The food container of claim 12 , wherein the food container contains potato chips.

14. The container of claim 1 , wherein the container contains a liquid.

15. The container of claim 14 , wherein the liquid is chosen from milk, orange juice, and a carbonated beverage.

16. The container of claim 1 , wherein the container is a non-food container.

17. The container of claim 1 , wherein the composition further comprises a filler comprising carbon nanotubes, graphene, cotton, cellulose, a non-nylon fiber, and/or a non-polyester fiber.

18. The container of claim 1 , wherein the side comprises a plurality of layers.

19. The container of claim 18 , wherein the plurality of layers comprises an outer layer facing an exterior of the container and an inner layer facing an interior of the container, and

wherein at least one of the outer layer and the inner layer is the at least one layer formed from the composition.

20. The container of claim 19 , wherein a degradation rate of the outer layer upon exposure to oxygen is slower than that of the inner layer.

Assignments (2)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Oct 21, 2020
From: HEDGEHOG GROUP LLC
To: OKEANOS GROUP, LLC
Reel/Frame 054131/0877 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jun 11, 2018
From: PETRIE, RUSSELL
To: HEDGEHOG GROUP LLC
Reel/Frame 046048/0903 →
Continuity (2)
Provisional Application 62517563 · Jun 9, 2017
Related Publication 20180354691A1 · Dec 13, 2018