Composite structure repair methods incorporating a lattice core material

Inventors: Jacob M. Hundley (Newbury Park, CA); Eric C. Clough (Santa Monica, CA); Zak C. Eckel (Calabasas, CA); David Page (Foothill Ranch, CA); Sophia S. Yang (Lynnwood, WA)
Assignee: HRL Laboratories, LLC
B29C73/02B29C73/10B29C73/24B29K2105/04B29L2031/608
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 10,946,600
App. No.
15/690,229
Granted
Mar 16, 2021
Kind
B1
Abstract

A method for repairing a composite structure. A damaged portion of a first facesheet of the structure is removed, forming a hole in the first facesheet. A damaged portion of the underlying core is removed to form a cavity in the sandwich. If the second facesheet is damaged, the damaged section is removed, and covered and sealed with a facesheet repair section. If the core material is an open-cell material, a dam is formed around the perimeter of the cavity, to act as a barrier between the cavity and the core material. The cavity is at least partially filled with a photomonomer resin, which then is illuminated through a mask with collimated light to form a truss structure in the cavity. Residual photomonomer resin is removed, and a facesheet repair section is bonded over the hole in the first facesheet.

Claims (34)

1. A method for repairing a composite structure comprising a core attached to a first facesheet, the method comprising:

at least partially filling a cavity in the composite structure with a photomonomer resin, the cavity including a void in the core and a hole in the first facesheet, the hole opening into the void; and

exposing the photomonomer resin to collimated light projected through a mask having a plurality of apertures to form a core repair section comprising a plurality of waveguide members that interpenetrate each other at a plurality of nodes to form a continuous material.

2. The method of claim 1 , wherein the exposing of the photomonomer resin to collimated light comprises exposing the photomonomer resin to collimated light from three sources of collimated light.

3. The method of claim 1 , further comprising, before at least partially filling the cavity in the composite structure with the photomonomer resin, forming a dam around a perimeter of the cavity to form a barrier between the cavity and the core.

4. The method of claim 3 , further comprising sealing the dam against a surface of a second facesheet that is bonded to the core opposite the first facesheet.

5. The method of claim 3 , further comprising sealing the dam against the first facesheet around a perimeter of the hole in the first facesheet.

6. The method of claim 1 , further comprising removing uncured photomonomer resin from the cavity.

7. The method of claim 6 , further comprising performing a post-curing operation on the core repair section.

8. The method of claim 7 , wherein performing the post-curing operation comprises exposing the core repair section to non-collimated ultraviolet light.

9. The method of claim 7 , wherein performing the post-curing operation comprises heating the core repair section.

10. The method of claim 9 , wherein heating the core repair section comprises exposing the core repair section to infrared light.

11. The method of claim 1 , further comprising bonding a first facesheet repair section to the first facesheet and the core repair section, covering the hole in the first facesheet.

12. The method of claim 11 , wherein bonding the first facesheet repair section to the first facesheet comprises bonding a pre-cured facesheet repair section to the first facesheet and the core repair section.

13. The method of claim 12 , wherein the pre-cured facesheet repair section is a pre-cured thermosetting polymer matrix composite facesheet repair section.

14. The method of claim 11 , wherein the bonding of the first facesheet repair section on to the first facesheet comprises:

laying an uncured thermosetting polymer matrix composite facesheet repair section on the first facesheet on the core repair section; and

curing the thermosetting polymer matrix composite facesheet repair section in place.

15. The method of claim 14 , further comprising performing a post-curing operation on the core repair section, wherein the performing of the post-curing operation and the curing of the thermosetting polymer matrix composite facesheet repair section comprise concurrently heating the core repair section and the thermosetting polymer matrix composite facesheet repair section.

16. The method of claim 1 , wherein the core comprises, as a major component, a material selected from the group consisting of honeycombs, open cell foams, and closed cell foams.

17. The method of claim 1 , further comprising, before at least partially filling the cavity in the composite structure with the photomonomer resin:

removing damaged facesheet material and removing damaged core material to form the cavity.

18. The method of claim 17 ,

wherein the core of the composite structure is sandwiched between the first facesheet and a second facesheet, and

wherein the removing of the damaged facesheet material comprises:

removing damaged facesheet material from the first facesheet;

removing damaged material from the core to form the void; and

removing damaged facesheet material from the second facesheet, to form a hole in the second facesheet opening into the void.

19. The method of claim 18 , further comprising bonding a second facesheet repair section on to the second facesheet to cover and seal the hole in the second facesheet.

20. The method of claim 19 , wherein the bonding of the second facesheet repair section on to the second facesheet comprises bonding a pre-cured facesheet repair section on to the second facesheet.

21. The method of claim 20 , wherein the pre-cured facesheet repair section is a pre-cured thermosetting polymer matrix composite facesheet repair section.

22. The method of claim 21 , wherein the bonding of the second facesheet repair section on to the second facesheet comprises:

laying an uncured thermosetting polymer matrix composite facesheet repair section on the second facesheet; and

curing the thermosetting polymer matrix composite facesheet repair section in place.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Feb 12, 2018
From: HUNDLEY, JACOB M.; CLOUGH, ERIC C.; ECKEL, ZAK C.; PAGE, DAVID; YANG, SOPHIA S.
To: HRL LABORATORIES, LLC
Reel/Frame 044900/0402 →
Cited By (1)
US 12,709,581