Method for producing a laminate consisting of a backing sheet and decorative paper

Inventor: Norbert Kalwa (Horn-Bad Meinberg, DE)
Assignee: Flooring Technologies Ltd.
B32B37/1284B27N7/005B32B7/12B32B21/02B32B21/06B32B37/24B44C5/04B44C5/0492B29C65/481B29C65/486B29C65/522B29C65/64B32B2250/02B32B2317/125B32B2317/16B32B2451/00
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 10,981,370
App. No.
15/741,561
Granted
Apr 20, 2021
Kind
B2
Abstract

The present invention relates to a method for producing a laminate having a backing sheet and a decorative paper arranged on the backing sheet, including the steps of: a) providing the backing sheet, b) scattering at least one layer of at least one powdered resin onto at least one side of the backing sheet, the surface of the side of the backing sheet that is to be scattered with the powdered resin being unsmoothed, c) placing at least one decorative paper onto the side of the backing sheet that is provided with the powdered resin, and d) pressing the layered structure including the backing sheet, the powdered resin and the decorative paper. The present invention likewise relates to a laminate that can be produced by this method.

Claims (56)

1. A method for producing a laminate comprising a wooden composite board and a decorative paper disposed on the wooden composite board,

comprising the steps of:

a) providing the wooden composite board,

b) scattering at least one layer of at least one pulverulent resin onto at least one side of the wooden composite board, where a surface of the at least one side of the wooden composite board on which the at least one pulverulent resin is to be scattered is unsanded and bears a press skin or rotting layer;

c) placing at least one decorative paper onto the at least one side of the wooden composite board that bears the at least one pulverulent resin, and

d) compressing the wooden composite board, the at least one pulverulent resin and decorative paper,

wherein the at least one side of the wooden composite board on which the at least one pulverulent resin is to be scattered is pretreated, before the scattering of the at least one pulverulent resin, to improve an adhesion of the at least one pulverulent resin,

wherein the pretreatment of the at least one side on which scattering is to take place comprises subjecting the wooden composite board to moisture or comprises electrostatically charging the wooden composite board,

wherein the at least one pulverulent resin has a scatter density of 0.5 to 1.5 kg/l and an average particle size of 10 to 50 μm and is applied in an amount of 3 to 20 g/m 2 to the wooden composite board, and

wherein the decorative paper is an at least partially impregnated decorative paper.

2. The method according to claim 1 , wherein the pretreatment of the at least one side on which scattering is to take place comprises subjecting the wooden composite board to 0.5-5 g/m 2 of water.

3. The method according to claim 2 , wherein the pretreatment comprises subjecting the wooden composite board to 1 to 2 g/m 2 of water.

4. The method according to claim 1 , wherein the at least one pulverulent resin is a formaldehyde resin, a urea resin, a melamine resin, a phenolic resin, or a melamine-formaldehyde resin.

5. The method according to claim 4 , wherein the at least one pulverulent resin is a melamine-formaldehyde resin or a urea resin.

6. The method according to claim 1 , wherein the at least one pulverulent resin is scattered onto at least one side of at least one backing paper, and the at least one backing paper scattered with the at least one pulverulent resin is disposed with the at least one pulverulent resin in a direction of the at least one side of the wooden composite board.

7. The method according to claim 6 , wherein at least one side of the wooden composite board is coated with the at least one backing paper, and/or the at least one side of the at least one backing paper that is to be scattered with the at least one pulverulent resin, is pretreated, before scattering of the at least one pulverulent resin, to improve the adhesion of the at least one pulverulent resin.

8. The method according to claim 7 , wherein the at least one side of the wooden composite board that is to be coated with the at least one backing paper, and/or the at least one side of the at least one backing paper that is to be scattered with the at least one pulverulent resin, is pretreated by being subjected to moisture or being electrostatically charged.

9. The method according to claim 1 , wherein the at least one pulverulent resin is applied using a scattering apparatus.

10. The method according to claim 1 , wherein at least one backing paper is an at least partially impregnated backing paper.

11. The method according to claim 1 , wherein the wooden composite board consists of a wood-based material or a wood-based material/polymer mixture.

12. The method according to claim 11 , wherein the wooden composite board is a particle board, medium density fibre (MDF) board, high-density fibre (HDF) board or oriented strand board (OSB), or plywood board.

13. The method according to claim 1 , wherein the at least one pulverulent resin has a scatter density of 0.8 to 1.0 kg/l and an average particle size of 20 to 30 μm.

14. The method according to claim 1 , wherein the at least one pulverulent resin is applied in an amount of 6 to 10 g/m 2 to the wooden composite board.

15. A method for producing a laminate comprising a wooden composite board and a decorative paper disposed on the wood composite board, comprising the steps of:

a) providing the wooden composite board,

b) scattering at least one layer of at least one pulverulent resin onto at least one side of the wooden composite board, where a surface of that side of the wooden composite board on which the at least one pulverulent resin is to be scattered is unsanded and bears a press skin or rotting layer,

c) placing at least one decorative paper onto a side of the wooden composite board that bears the pulverulent resin,

c2) applying at least one overlay onto the at least one decorative paper, and

d) compressing the wooden composite board, the at least one pulverulent resin and the at least one decorative paper,

wherein the at least one pulverulent resin has a scatter density of 0.5 to 1.5 kg/l and an average particle size of 10 to 50 μm and is applied in an amount of 3 to 20 g/m 2 to the wooden composite board, and

wherein the decorative paper is an at least partially impregnated decorative paper.

16. The method according to claim 15 , wherein the at least one overlay applied in step c2) is a resin-impregnated overlay.

17. A method for producing a laminate comprising a wooden composite board and a decorative paper disposed on the wood composite board,

comprising the steps of:

a) providing the wooden composite board,

b) scattering at least one layer of at least one pulverulent resin onto at least one side of the wooden composite board, where a surface of at least one side of the wooden composite board on which the at least one pulverulent resin is to be scattered is unsanded and bears a press skin or rotting layer,

c) placing at least one decorative paper onto the at least one side of the wooden composite board that bears the at least one pulverulent resin,

c1) applying at least one further layer of a pulverulent resin onto the top side of the decorative paper, and

d) compressing the wooden composite board, the at least one pulverulent resin and the at least one decorative paper,

wherein the at least one pulverulent resin has a scatter density of 0.5 to 1.5 kg/l and an average particle size of 10 to 50 μm and is applied in an amount of 3 to 20 g/m 2 to the wooden composite board, and

wherein the decorative paper is an at least partially impregnated decorative paper.

18. The method according to claim 17 , wherein a further layer to be applied in step c1) consists of a mixture comprising the at least one pulverulent resin, natural and/or synthetic fibers, wear-reducing particles, and, optionally, at least one further additive.

19. The method according to claim 18 , wherein as further additives at least one additive is selected from a group consisting of conductive substances, flame retardants, luminescent substances, and metals.

20. The method according to claim 18 , wherein the at least one further additive comprises a conductive substance.

21. The method according to claim 18 , wherein the natural and/or synthetic fibers comprise bleached cellulose fibers or organic polymer fibers.

22. The method according to claim 18 , wherein wear-reducing particles comprise at least one of the following: aluminum oxides, corundum, boron carbides, silicon dioxides, silicon carbides and glass beads.

23. The method according to claim 18 , wherein the at least one side of the wooden composite board on which the at least one pulverulent resin is to be scattered in step b) is pretreated, before the scattering of the at least one pulverulent resin, to improve an adhesion of the at least one pulverulent resin.

24. The method according to claim 23 , wherein the pretreatment of the at least one side on which scattering is to take place in step b) comprises subjecting the wooden composite board to moisture or comprises electrostatically charging the wooden composite board.

25. The method according to claim 23 , wherein the pretreatment of the side on which scattering is to take place in step b) comprises subjecting the wooden composite board to 0.5-5 g/m 2 of water.

26. The method according to claim 18 , wherein the at least one pulverulent resin is a formaldehyde resin, a urea resin, a melamine resin or a phenolic resin.

27. The method according to claim 18 , wherein the at least one pulverulent resin has a scatter density of 0.5 to 1.5 kg/l, and an average particle size of 10 to 50 μm.

28. The method according to claim 18 , wherein the at least one pulverulent resin is scattered onto at least one side of at least one backing paper, and the at least one backing paper scattered with the at least one pulverulent resin is disposed with the at least one pulverulent resin in a direction of the at least one side of the wooden composite board.

29. The method according to claim 28 , wherein the at least one side of the wooden composite board on which the at least one backing paper is disposed, and/or the at least one side of the at least one backing paper that is to be scattered with the pulverulent resin, is pretreated, before scattering of the pulverulent resin, to improve an adhesion of the at least one pulverulent resin.

30. The method according to claim 18 , wherein the at least one pulverulent resin is applied using a scattering apparatus.

31. The method according to claim 18 , wherein the at least one backing paper is an at least partially impregnated backing paper.

32. The method according to claim 18 , wherein the wooden composite board consists of a wood-based material or a wood-based material/polymer mixture.

Priority Claims (1)
EP 15177033 · Jul 16, 2015 · regional
Continuity (1)
Related Publication 20180194123A1 · Jul 12, 2018
Cited By (1)
US 12,296,499