Method for repairing ceramic matrix composite and ceramic matrix composite member

Inventors: Masahiko Mega (Tokyo, JP); Takayuki Kurimura (Tokyo, JP); Taiji Torigoe (Tokyo, JP); Mineaki Matsumoto (Tokyo, JP)
Assignee: MITSUBISHI HEAVY INDUSTRIES, LTD.
B29C73/245B29C73/04B29C73/26C04B35/62625C04B35/76C04B35/80C04B41/009C04B41/0018C04B41/52C04B41/89B29C2073/264B29C2073/268C04B2235/616C04B2235/77C04B2235/96
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 11,034,106
App. No.
16/029,117
Granted
Jun 15, 2021
Kind
B2
Abstract

A method for repairing a target member including a ceramic matrix composite reinforced by ceramic fiber includes: a removal step of removing at least a part of a surface of the target member; an arrangement step of arranging a green body for repair which includes the ceramic fiber on a portion where the surface is removed in the removal step; an impregnation step of impregnating at least the portion of the target member where the green body for repair is disposed with slurry; and a sintering step of sintering the target member on which the green body for repair is disposed, after the impregnation step.

Claims (21)

1. A method for repairing a target member including a ceramic matrix composite reinforced by ceramic fiber, the method comprising:

a removal step of removing at least a part of a surface of the target member;

a hole-forming step of forming at least one hole on the portion where the surface is removed after the removal step;

an arrangement step of arranging a green body for repair which includes the ceramic fiber on a portion where the surface is removed in the removal step;

an impregnation step of impregnating at least the portion of the target member where the green body for repair is disposed with slurry; and

a sintering step of sintering the target member on which the green body for repair is disposed, after the impregnation step wherein the portion where the surface is removed in the removal step includes a first region where a density of the ceramic fiber is relatively high and a second region where the density of the ceramic fiber is lower than that in the first region, and wherein the hole-forming step includes forming the at least one hole by drilling the at least one hole in the second region.

2. The method for repairing a ceramic matrix composite according to claim 1 ,

wherein the ceramic fiber includes a layer including a first bundle of the ceramic fiber extending in a first direction, a second bundle of the ceramic fiber extending in the first direction adjacent to the first bundle, a third bundle of the ceramic fiber extending in a second direction interesting with the first direction, and a fourth bundle of the ceramic fiber extending in the second direction adjacent to the third bundle, the first bundle and the second bundle intersecting with the third bundle and the fourth bundle, respectively, and

wherein the hole-forming step includes forming the at least one hole in a position between the first bundle and the second bundle, and the hole formed is also in a position between the third bundle and the fourth bundle.

3. The method for repairing a ceramic matrix composite according to claim 1 , further comprising, after the removal step, a hole-forming position determination step of capturing an image of a layer of the ceramic fiber remaining on the target member, performing an image processing on the image obtained by the capturing, and determining a position for forming the at least one hole on the basis of a result of the image processing.

4. The method for repairing a ceramic matrix composite according to claim 2 ,

wherein a depth of the at least one hole is smaller than a thickness of a single layer of the ceramic fiber.

5. The method for repairing a ceramic matrix composite according to claim 1 ,

wherein the impregnation step includes:

a deaeration step of deaerating at least a portion of the target member where the green body for repair is disposed; and

an immersion step of immersing at least the portion of the target member where the green body for repair is disposed in the slurry, after the deaeration step.

6. The method for repairing a ceramic matrix composite according to claim 1 ,

wherein the impregnation step comprises;

a step of covering the target member on which the green body for repair is disposed with a bag or a sheet, and injecting the slurry into an inside of the bag or the sheet covering a portion of the target member; and

a step of vacuuming and depressurizing the inside of the bag or the sheet covering the portion of the target member, after the step of injecting the slurry.

7. The method for repairing a ceramic matrix composite according to claim 1 , wherein the impregnation step includes a step of arranging, inside a pressurizing device, the target member on which the green body for repair is disposed, and pressurizing the slurry.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Sep 26, 2018
From: MEGA, MASAHIKO; KURIMURA, TAKAYUKI; TORIGOE, TAIJI; MATSUMOTO, MINEAKI
To: MITSUBISHI HEAVY INDUSTRIES, LTD.
Reel/Frame 046980/0009 →
Priority Claims (1)
JP JP2017-135495 · Jul 11, 2017 · national
Continuity (1)
Related Publication 20190016072A1 · Jan 17, 2019