IP Library › Granted Patent US 11,081,700
Granted Patent B2
US 11,081,700 · App. 16/550,689 · Granted Aug 3, 2021

Nonaqueous electrolyte secondary battery and method for producing nonaqueous electrolyte secondary battery

Inventors: Naoki Uchida (Hyogo, JP); Haruya Nakai (Hyogo, JP); Ayumi Kochi (Osaka, JP)
Assignee: SANYO Electric Co., Ltd.
H01M4/622H01M4/0404H01M4/0435H01M4/133H01M4/1393H01M4/366H01M4/587H01M10/0525H01M2004/027
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 11,081,700
App. No.
16/550,689
Granted
Aug 3, 2021
Kind
B2
Abstract

A nonaqueous electrolyte secondary battery according to an embodiment of the present disclosure includes a negative electrode including a negative electrode core and negative electrode mixture layers formed on both surfaces of the negative electrode core. Each of the negative electrode mixture layers contains a cellulose-based binder composed of at least one of carboxymethyl cellulose and a salt thereof. When each of the negative electrode mixture layers is divided in half, at the center in the thickness direction, into a first region near the negative electrode core and a second region far from the negative electrode core, the content of the cellulose-based binder present in the first region is 35% by mass or more and less than 50% by mass of the total mass of the cellulose-based binder contained in the entire of each of the negative electrode mixture layers.

Claims (18)

1. A nonaqueous electrolyte secondary battery comprising:

an electrode body having a positive electrode, a negative electrode, and a separator; and

a nonaqueous electrolyte,

wherein the negative electrode includes a negative electrode core and negative electrode mixture layers formed on both surfaces of the negative electrode core;

each of the negative electrode mixture layers contains a cellulose-based binder composed of at least one of carboxymethyl cellulose and a salt thereof, and

when each of the negative electrode mixture layers is divided in half, at the center in the thickness direction, into a first region near the negative electrode core and a second region far from the negative electrode core, wherein the second region is located beyond the center, in the thickness direction, of at least one of the negative electrode mixture layers, the content of the cellulose-based binder present in the first region is 35% by mass or more and less than 50% by mass of the total mass of the cellulose-based binder contained in the entirety of each of the negative electrode mixture layers,

wherein each of the negative electrode mixture layers further contains a rubber-based binder composed of at least one of styrene-butadiene rubber and a modified variant of styrene-butadiene rubber that retains styrene-butadiene characteristics; and

the content of the rubber-based binder present in the first region is over 50% by mass and 70% by mass or less of the total mass of the rubber-based binder contained in the entirety of each of the negative electrode mixture layers.

2. The nonaqueous electrolyte secondary battery according to claim 1 ,

wherein the content of the cellulose-based binder present in the first region is 35% by mass or more and 45% by mass or less of the total mass of the cellulose-based binder contained in the entirety of each of the negative electrode mixture layers.

3. A nonaqueous electrolyte secondary battery comprising:

an electrode body having a positive electrode, a negative electrode, and a separator; and

a nonaqueous electrolyte,

wherein the negative electrode includes a negative electrode core and negative electrode mixture layers formed on both surfaces of the negative electrode core;

each of the negative electrode mixture layers contains a cellulose-based binder composed of at least one of carboxymethyl cellulose and a salt thereof, and

when each of the negative electrode mixture layers is divided in half, at the center in the thickness direction, into a first region near the negative electrode core and a second region far from the negative electrode core, wherein the second region is located beyond the center, in the thickness direction, of at least one of the negative electrode mixture layer, the content of the cellulose-based binder present in the first region is 35% by mass or more and less than 50% by mass of the total mass of the cellulose-based binder contained in the entirety of each of the negative electrode mixture layers,

wherein each of the negative electrode mixture layers further contains a rubber-based binder composed of at least one of styrene-butadiene rubber and a modified variant of styrene-butadiene rubber that retains styrene-butadiene characteristics; and

the content of the rubber-based binder present in the first region is over 50% by mass and 60% by mass or less of the total mass of the rubber-based binder contained in the entirety of each of the negative electrode mixture layers.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jan 10, 2020
From: UCHIDA, NAOKI; NAKAI, HARUYA; KOCHI, AYUMI
To: SANYO ELECTRIC CO., LTD.
Reel/Frame 051473/0139 →
Priority Claims (1)
JP JP2018-162113 · Aug 30, 2018 · national
Continuity (1)
Related Publication 20200075958A1 · Mar 5, 2020