IP Library Granted Patent US 11,161,201
Granted Patent B2
US 11,161,201 · App. 15/609,121 · Granted Nov 2, 2021

System and methods for fabricating a component with a laser device

Inventors: Victor Petrovich Ostroverkhov (Ballston Lake, NY); Jason Harris Karp (Niskayuna, NY); Mark Marshall Meyers (Halfmoon, NY); William Thomas Carter (Galway, NY)
Assignee: General Electric Company
B23K26/073B22F12/00B23K26/342B33Y30/00B33Y50/02B22F10/10B22F2203/00B33Y10/00
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 11,161,201
App. No.
15/609,121
Granted
Nov 2, 2021
Kind
B2
Abstract

A powder melting device for an additive manufacturing system is provided. The powder melting device includes at least one laser device configured to generate at least one energy beam for forming at least one melt pool in a layer of powdered material. The powder melting device also includes at least two optical elements configured to dynamically induce beam distortion in the at least one energy beam to modify a beam spot incident on the layer of powdered material. The at least two optical elements are configured to induce at least one of an aspect ratio adjustment of the at least one energy beam, an optical powder redistribution between a periphery and a center of the at least one energy beam, and a rotation of the at least one energy beam.

Claims (36)

1. A powder melting device for an additive manufacturing system, said powder melting device comprising:

at least one laser device configured to generate at least one energy beam for forming at least one melt pool in a melt plane defined by a layer of powdered material;

at least three optical elements configured to dynamically induce beam distortion in the at least one energy beam to modify a beam spot incident on the layer of powdered material, said at least three optical elements comprising an adjustable cylindrical beam expander disposed between a deformable mirror and a beam rotation prism configured to collectively induce:

an adjustment of an aspect ratio of the at least one energy beam in the melt plane; and

an optical power redistribution between a periphery and a center of the at least one energy beam.

2. The powder melting device in accordance with claim 1 , wherein said at least three optical elements are further configured to rotate an orientation of the at least one energy beam.

3. The powder melting device in accordance with claim 1 , wherein said adjustable cylindrical beam expander is configured to:

perform the adjustment of the aspect ratio of the at least one energy beam; and

rotate an orientation of the at least one energy beam.

4. The powder melting device in accordance with claim 1 , wherein said beam rotation prism is configured to rotate an orientation of the at least one energy beam.

5. The powder melting device in accordance with claim 1 , wherein said powder melting device is configured to generate a non-uniform energy intensity profile for at least one scan path of said at least one energy beam.

6. An additive manufacturing system comprising:

a powder bed; and

a powder melting device comprising:

at least one laser device configured to generate at least one energy beam for forming at least one melt pool in a melt plane defined by a layer of powdered material in said powder bed; and

at least three optical elements configured to dynamically induce beam distortion in the at least one energy beam to modify a beam spot incident on the layer of powdered material, said at least three optical elements comprising an adjustable cylindrical beam expander disposed between a deformable mirror and a beam rotation prism configured to collectively induce:

an adjustment of an aspect ratio of the at least one energy beam in the melt plane; and

an optical power redistribution between a periphery and a center of the at least one energy beam.

7. The additive manufacturing system of claim 6 , wherein said at least three optical elements are further configured to rotate an orientation of the at least one energy beam.

8. The additive manufacturing system of claim 6 , wherein said adjustable cylindrical beam expander is configured to:

perform the adjustment of the aspect ratio of the at least one energy beam in the melt plane; and

rotate an orientation of the at least one energy beam.

9. The additive manufacturing system of claim 6 , wherein said beam rotation prism is configured to rotate an orientation of the at least one energy beam.

10. The additive manufacturing system of claim 6 , wherein said powder melting device is configured to generate a non-uniform energy intensity profile for at least one scan path of said at least one energy beam.

11. A method of fabricating a component in a powder bed, said method comprising:

moving at least one laser device through at least one scan path across the powder bed;

emitting at least one energy beam from the at least one laser device;

dynamically inducing beam distortion in the at least one energy beam using at least three optical elements to modify a beam spot incident in a melt plane on a layer of powdered material in the powder bed, the at least three optical elements comprising an adjustable cylindrical beam expander disposed between a deformable mirror and a beam rotation prism for modifying the beam spot by collectively:

performing an adjustment of an aspect ratio of the at least one energy beam in the melt plane; and

redistributing optical power between a periphery and a center of the at least one energy beam; and

generating at least one melt pool in the powder bed.

12. The method in accordance with claim 11 , wherein dynamically inducing beam distortion comprises rotating an orientation of the at least one energy beam.

13. The powder melting device in accordance with claim 1 , wherein the at least one energy beam has a first dimension and a second, perpendicular, dimension in the melt plane, and wherein the adjustment of an aspect ratio of the at least one energy beam causes the first dimension to be greater than the second dimension.

14. The powder melting device in accordance with claim 1 , wherein the beam rotation prism is optically downstream the adjustable cylindrical beam expander.

15. The additive manufacturing system of claim 6 , wherein the beam rotation prism is optically downstream the adjustable cylindrical beam expander.

16. The method in accordance with claim 11 , wherein the beam rotation prism is optically downstream the adjustable cylindrical beam expander.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded May 31, 2017
From: OSTROVERKHOV, VICTOR PETROVICH; KARP, JASON HARRIS; MEYERS, MARK MARSHALL; CARTER, WILLIAM THOMAS
To: GENERAL ELECTRIC COMPANY
Reel/Frame 042538/0032 →
Continuity (1)
Related Publication 20180345405A1 · Dec 6, 2018
Cited By (2)
US 12,280,538 US 12,403,650