IP Library › Granted Patent US 11,168,214
Granted Patent B2
US 11,168,214 · App. 16/308,367 · Granted Nov 9, 2021

Method for identifying the extent of aging in an asphalt

Inventors: Gerald H. Reinke (La Crosse, WI); Gaylon L. Baumgardner (Arkadelphia, AR); Andrew Hanz (La Crosse, WI)
Assignees: A.L.M. Holding Company; Ergon Asphalt & Emulsions, Inc.
C08L95/00A61K31/56C04B18/16C04B26/26C08K5/05E01C1/00G01N33/42C08K2201/00C08L2555/10C08L2555/22C08L2555/60C08L2555/64E01C7/18G01Q60/24
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 11,168,214
App. No.
16/308,367
Granted
Nov 9, 2021
Kind
B2
Abstract

Disclosed are asphalt and asphalt binders and methods for making such compositions with sterols. The sterols improve various rheological properties. Also disclosed are methods of determining the changes or improvements of various rheoloical properties.

Claims (22)

1. A method for identifying the extent of aging in an aged asphalt binder and slowing the aging of the aged asphalt binder comprising:

analyzing the aged asphalt binder for surface defects using atomic force microscopy; and

adding amounts of an anti-aging additive comprising sterol or stanol and a virgin asphalt binder to the aged asphalt binder, wherein the anti-aging additive slows the aging rate of the asphalt binder composition compared to an asphalt binder composition without the age-retarding additive.

2. The method according to claim 1 , wherein the asphalt binder is derived from asphalt comprising re-refined engine oil bottoms or vacuum tower asphalt extender.

3. The method according to claim 1 , wherein the asphalt binder is derived from asphalt comprising drain oil product or waste engine oil material with or without post-consumer processing.

4. The method according to claim 1 , wherein the asphalt binder is derived from asphalt comprising paraffinic processing oil.

5. The method according to claim 1 , wherein the asphalt binder is derived from asphalt comprising lubricating base oil.

6. The method according to claim 1 , wherein the asphalt binder is derived from a paving mixture containing reclaimed asphalt pavement (RAP) and the RAP is present in an amount of 0.1% to 100% of the asphalt binder weight.

7. The method according to claim 1 , wherein the asphalt binder is derived from a paving mixture containing reclaimed asphalt shingles (RAS) and the RAS is present in binder in an amount of 0.1% to 50% of the total asphalt binder weight.

8. The method according to claim 1 , wherein the asphalt binder is derived from a paving mixture containing RAP and RAS, and wherein a combination of RAP and RAS is present in an amount of 0.1% to 100% of the total binder weight.

9. The method according to claim 1 , wherein the asphalt binder is derived from the upper 13 mm (½ inch) of a pavement sample obtained from a road.

10. The method according to claim 1 , wherein the asphalt binder is derived from a pavement sample aged in place from 1 day to 10 years.

11. The method according to claim 1 , wherein the asphalt binder is derived from any depth of a pavement layer including a full pavement layer.

12. The method according to claim 1 , wherein the asphalt binder comprises a virgin asphalt binder prior to paving.

13. The method according to claim 1 , wherein the anti-aging additive comprises 0.5 to 15 wt. % of the anti-aging additive based on the virgin asphalt binder weight.

14. The method according to claim 1 , wherein the sterol or stanol comprises a plant sterol or plant stanol.

15. The method according to claim 1 , wherein the anti-aging additive is present in an amount effective to provide a decreased R value after aging the asphalt binder compared to the similarly-aged asphalt binder without the anti-aging additive.

16. The method according to claim 1 , wherein the anti-aging additive is present in an amount effective to provide a less negative ΔTc value after aging the asphalt binder compared to the similarly-aged asphalt binder without the anti-aging additive.

17. The method according to claim 1 , wherein the anti-aging additive is present in an amount effective to provide a ΔTc of greater than or equal to −5.0° C.

18. The method according to claim 1 , wherein the asphalt binder is derived from a pavement aged for more than five years.

19. The method according to claim 1 , wherein the sterol or stanol is derived from a tall oil pitch.

20. The method according to claim 1 , wherein the sterol or stanol is derived from soybean oil or corn oil.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Dec 10, 2018
From: REINKE, GERALD H.; BAUMGARDNER, GAYLON L.; HANZ, ANDREW
To: A.L.M. HOLDING COMPANY; ERGON ASPHALT & EMULSIONS, INC.
Reel/Frame 047725/0402 →
Continuity (4)
Continuation In Part PCTUS2016037077 · Jun 10, 2016
Provisional Application 62385905 · Sep 9, 2016
Provisional Application 62385899 · Sep 9, 2016
Related Publication 20190265221A1 · Aug 29, 2019
Cited By (3)
US 12,234,189 US 12,692,395 US 12,703,796