Method of repairing a damaged spar cap of a wind turbine blade of a wind turbine
A method of repairing a damaged spar cap of a wind turbine blade of a wind turbine, the damaged spar cap including carbon fiber-reinforced plastic and the method having the steps of: removing a damaged carbon fiber-reinforced plastic part from the damaged spar cap to obtain a corresponding recess in the damaged spar cap, applying an adhesive to the recess, and fitting at least one patch including carbon fiber-reinforced plastic into the recess, is provided.
1. A method of repairing a damaged spar cap of a wind turbine blade of a wind turbine, the damaged spar cap comprising carbon fiber-reinforced plastic, the method comprising:
removing a damaged carbon fiber-reinforced plastic part from the damaged spar cap to obtain a corresponding recess in the damaged spar cap;
applying an adhesive to the corresponding recess;
fitting at least one patch comprising carbon fiber-reinforced plastic into the corresponding recess, wherein the carbon fiber-reinforced plastic of the at least one patch are pultruded carbon elements; and
joining the at least one patch with the spar cap to obtain a repaired spar cap.
2. The method according to claim 1 , wherein the corresponding recess is tapered in at least one direction with a tapering angle and at least one of the at least one patches is chamfered in at least one direction with a chamfering angle.
3. The method according to claim 2 , wherein at least one of the at least one direction of the tapering and/or at least one of the at least one direction of the chamfering is a fiber direction of the carbon fiber-reinforced plastic.
4. The method according to claim 2 , wherein the tapering angle corresponds to the chamfering angle.
5. The method according to claim 1 , wherein the adhesive is applied continuously on at least 80% of a surface of the corresponding recess.
6. The method according to claim 1 , wherein the adhesive is an electrically conductive adhesive film.
7. The method according to claim 1 , wherein the at least one patch is provided with a peel-ply on a top surface and/or a bottom surface of the patch, whereby the peel-ply is removed prior to fitting the at least one patch into the corresponding recess.
8. The method according to claim 1 , wherein the carbon fiber-reinforced plastic of the damaged spar cap are provided as pultruded carbon elements.
9. The method according to claim 8 , wherein the damaged spar cap and/or the at least one patch are provided with an array of at least two pultruded carbon elements arranged parallel to each other in a fiber direction of the carbon fiber-reinforced plastic.
10. The method according to claim 8 , wherein the damaged spar cap and/or the at least one patch are provided with a stack of at least two pultruded carbon elements arranged stacked on top of each other.
11. The method according to claim 1 , wherein at least two patches are being fitted into the corresponding recess, whereby the adhesive is applied on top of at least one of the at least two patches.
12. The method according to claim 1 , wherein the damaged carbon fiber-reinforced plastic is removed from the damaged spar cap by means of abrasion and/or sanding.
13. The method according to claim 1 , wherein the at least one patch is joined with the damaged spar cap by means of vacuum bagging using a vacuum bagging assembly.
14. The method according to claim 1 , wherein the at least one patch is joined with the damaged spar cap by applying heat to the at least one patch by means of a heating blanket.
15. The method according to claim 1 , wherein at least one doubler plate is being arranged on top of the at least one patch and the damaged spar cap and the at least one doubler plate is being joined with the at least one patch and the damaged spar cap.