IP Library › Granted Patent US 11,435,610
Granted Patent B2
US 11,435,610 · App. 17/169,961 · Granted Sep 6, 2022

Method for producing a flexible electro-optic cell

Inventors: Roy E. Miller, IV (Stow, OH); Christine Baker (Munroe Falls, OH); Ludmila Sukhomlinova (Kent, OH); Eui-Yeul Park (Hudson, OH); William Ryan (Kent, OH); Bahman Taheri (Shaker Heights, OH); Paul Luchette (Kent, OH)
Assignee: ALPHAMICRON INCORPORATED
G02F1/133305G02F1/1303G02F1/1679G02F2202/28
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 11,435,610
App. No.
17/169,961
Granted
Sep 6, 2022
Kind
B2
Abstract

Provided is a flexible cell unit and a method of manufacturing the same. The cell unit includes first and second substrates separated by a controlled distance maintained by spacers, filled with an electro-optic material and enclosed by a border seal. The method includes providing two sheets to form the first and second substrates, where at least one of the sheets is flexible, depositing an electro-optic material on at least one substrate, and roll-filling the cell by using one or more lamination rollers to pair the first and second substrates to within the controlled distance of each other and filling the controlled distance with the electro-optic material.

Claims (49)

1. A cell unit comprising:

first and second substrates separated by a controlled distance maintained by spacers within the cell unit, filled with an electro-optic material and enclosed by a border seal, said cell unit produced using a method of manufacture comprising:

providing two sheets of material to form the first and second substrates wherein at least one of the sheets is flexible,

depositing the electro-optic material on at least one said substrate, and

roll-filling the cell by using one or more lamination rollers to pair the first and second substrates to within the controlled distance of each other and filling said controlled distance with said electro-optic material

wherein the cell unit is an optical device suitable for a user to look through, and

wherein the cell unit does not include periodic structures that cause diffraction.

2. The cell unit of claim 1 , wherein the electro-optic material is non-discrete: non-encapsulated non-polymerizable and contains less than 20% polymerizable material.

3. The cell unit of claim 1 wherein the electro-optic material is deposited in an area outside the perimeter of the border seal before roll-filling the cell.

4. The cell unit of claim 1 , wherein the spacers are unpatterned.

5. The cell unit of claim 4 , wherein the unpatterned spacers have a density of more than 80 per square mm.

6. The cell unit of claim 1 , wherein one or both of the substrates further comprise an alignment layer and the spacers are deposited inside the alignment layer.

7. The cell unit of claim 1 , wherein the cell further comprises adhesive gap control (AGC) means comprising one or more elements selected from polymeric or adhesive bridges, partition walls, pillars, or a combination thereof.

8. The cell unit of claim 1 , wherein the cell is an optical device having a haze value less than 10% in at least one state.

9. The cell unit of claim 1 , wherein the electro-optic material is a guest-host dichroic dye-liquid crystal mixture.

10. The cell unit of claim 9 , wherein the guest-host mixture has a clear state with a maximal light transmission of 30% or above and a transmission swing of 35% or more.

11. The cell unit of claim 1 , wherein said border seal is formed by applying a border sealant and wherein the ratio of border sealant viscosity to the electro-optic material viscosity is greater than 10.

12. A method of producing a cell unit comprising first and second substrates separated by a controlled distance maintained by spacers within the cell unit, filled with an electro-optic material and enclosed by a border seal, the method comprising:

providing two sheets of material to form the first and second substrates wherein at least one said sheet is flexible,

depositing the electro-optic material on at least one said substrate, and

roll-filling the cell unit by using one or more lamination rollers to pair the first and second substrates to within the controlled distance of each other and tilling said controlled distance with said electro-optic material

wherein the cell unit is an optical device suitable for a user to look through, and

wherein the cell unit does not include periodic structures that cause diffraction.

13. The method of claim 12 , wherein the electro-optic material is non-discrete non-encapsulated non-polymerizable and contains less than 20% polymerizable material.

14. The method of claim 12 , wherein the electro-optic material is deposited in an area outside the perimeter of the border seal before roll-filling the cell.

15. The method of claim 12 . wherein the spacers are unpatterned and have a diameter of 3-100 μm in size and a density of more than 80 per square mm.

16. The method of claim. 12 , wherein the method further comprises applying a plurality of unpatterned spacers to the first substrate, the second substrate or both.

17. The method of claim 12 , wherein one or both of the substrates further comprise an alignment layer and the method further comprises depositing the spacers inside or as part of the alignment layer.

18. The method of claim 12 , wherein the method further comprises placing adhesive gap control (AGC) means on at least one said substrate, wherein the AGC means comprise one or more elements selected from polymeric or adhesive bridges, partition walls, pillars, or a combination thereof.

19. The method of claim 12 , wherein the cell is an optical device having a haze value less than 10% in at least one state.

20. The method of claim 12 , wherein the electro-optic material is a guest-host dichroic dye-liquid crystal mixture.

21. The method of claim 12 , wherein the guest-host mixture has a clear state with a maximal light transmission of 30% or above and a transmission swing of 35% or more.

22. The method of claim 12 , wherein the border seal perimeter has at least one opening during the roll-filling step.

23. The method of claim 12 , wherein the border seal perimeter is created after the roll-filling step.

24. The method of claim 12 , wherein the method is vacuum-less.

25. A method of producing a flexible cell unit enclosed by a border seal and filled with an electro-optic material, the flexible cell unit having a first substrate and a second substrate separated by a controlled distance maintained by a plurality of unpatterned spacers within the flexible cell unit, the method comprising:

providing two sheets of flexible material as the first and second substrates,

depositing an electro-optic material on at least one substrate, wherein the electro-optic material is non-discrete non-encapsulated, non-polymeric, and contains less than 20% polymerizabie material; and

pairing the first and second substrates while roll-filling the flexible cell unit with the electro-optic material using one or more lamination rollers while the electro-optic material maintains its ability to be altered by application of an electric current or voltage so that the electro-optic material completely fills the controlled distance between the first and second substrates, wherein the controlled distance is maintained by the unpatterned spacers

wherein the cell unit is an optical device suitable for a user to look through, and

wherein the cell unit does not include periodic structures that cause diffraction.

26. The method of claim 25 . wherein the method further comprises applying a plurality of unpatterned spacers to the first substrate, the second substrate or both.

27. The method of claim 25 wherein one or both of the substrates further comprise an alignment layer and the method further comprises depositing the spacers inside or as part of the alignment layer.

28. The method of claim 25 , wherein the method further comprises placing adhesive gap control (AGC) means on at least one said substrate, wherein the AOC means comprise one or more elements selected from polymeric or adhesive bridges, partition walls, pillars, or a combination thereof.

29. The method of claim 25 , wherein the elects-optic material is a guest-host dichroic dye-liquid crystal mixture.

30. The method of claim 25 , wherein the electro-optic material is deposited on an area outside the perimeter of the border sealant, an area inside the perimeter of the border sealant, or one or more areas both inside and outside the perimeter of the border sealant.

31. The method of claim 25 , wherein the border seal perimeter has at least one opening during the roll-filling step.

32. The method of claim 25 , wherein the method is vacuum-less.

33. A cell unit manufactured according to the method in claim 25 .

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Feb 19, 2021
From: MILLER, ROY E., IV; BAKER, CHRISTINE; SUKHOMLINOVA, LUDMILA; PARK, EUI-YEUL; RYAN, WILLIAM; TAHERI, BAHMAN; LUCHETTE, PAUL
To: ALPHAMICRON INCORPORATED
Reel/Frame 055330/0531 →
Continuity (4)
Continuation In Part 16557235 · Aug 30, 2019
Continuation In Part 15526023
Provisional Application 62080630 · Nov 17, 2014
Related Publication 20210157197A1 · May 27, 2021
Cited By (5)
US 12,204,222 US 12,222,623 US 12,332,524 US 12,468,198 US 12,736,845