Method for producing a pyrolytic carbon with predetermined microstructure
A process for manufacturing pyrocarbon, includes forming pyrocarbon by a calefaction process from at least one C 2 to C 6 alcohol or polyalcohol precursor, the precursor being ethanol, rough laminar pyrocarbon being obtained by imposing a temperature of between 1250° C. and 1325° C. during calefaction.
1. A process for manufacturing pyrocarbon, comprising a step of forming pyrocarbon by a calefaction process from at least one C 2 to C 6 alcohol or polyalcohol precursor, the precursor being ethanol, rough laminar pyrocarbon being obtained by imposing a temperature of between 1250° C. and 1325° C. during calefaction.
2. A process for coating a substrate, comprising at least the following step:
forming a pyrocarbon coating on a surface of a substrate by carrying out a process as claimed in claim 1 .
3. A process for densifying a fiber preform, comprising at least the following step:
forming a pyrocarbon matrix in the porosity of the fiber preform by carrying out a process as claimed in claim 1 .