Halogen-containing polymer and production method for same

Inventors: Takeshi Kanbara (Yamaguchi, JP); Tomohiro Arita (Yamaguchi, JP)
Assignee: TOSOH CORPORATION
C08G65/42
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 11,555,093
App. No.
16/628,799
Granted
Jan 17, 2023
Kind
B2
Abstract

To provide a highly heat resistant flame retardant. A polymer having repeating units represented by the following formula (1), which has a weight average molecular weight as calculated as standard polystyrene of at least 6,000: wherein R is a C 1-6 alkylene group, —S— or —SO 2 —.

Claims (10)

1. A method for producing a polymer having repeating units represented by the following formula (1)

wherein R is a C 1-6 alkylene group, —S— or —SO 2 —, which comprises reacting a compound represented by the following formula (2) and a compound represented by the following formula (3):

wherein R is a C 1-6 alkylene group, —S— or —SO 2 —, and X is a halogen atom;

wherein R is a C 1-6 alkylene group, —S— or —SO 2 —, and M is an alkali metal ion or a substituted or non-substituted ammonium ion;

wherein the polymer has a weight average molecular weight as calculated as standard polystyrene of at least 6,000.

2. The method of claim 1 , wherein the polymer has a weight average molecular weight as calculated as standard polystyrene of at least 7,500.

3. The method of claim 1 , wherein the content of a monomer represented by the following formula (2) is at most 3% in the entire polymer having repeating units represented by the formula (1), as measured by GPC:

wherein R is a C 1-6 alkylene group, —S— or —SO 2 —, and X is a halogen atom.

4. The method of claim 1 , wherein the polymer has a melting point of at least 255° C.

5. The method of claim 1 , wherein the 20 wt % weight loss temperature of the polymer is at least 365° C. at a temperature-raising rate of 10° C/min.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jan 6, 2020
From: KANBARA, TAKESHI; ARITA, TOMOHIRO
To: TOSOH CORPORATION
Reel/Frame 051425/0212 →
Priority Claims (2)
JP JP2017-133921 · Jul 7, 2017 · national
JP JP2017-219687 · Nov 15, 2017 · national
Continuity (1)
Related Publication 20200199296A1 · Jun 25, 2020