Additive manufacturing

Inventors: Joseph Gwilliam Crabtree (Sheffield, GB); Konstantin Rybalcenko (Sheffield, GB); Andre Gaio (Sheffield, GB); Giorgio Ioannides (Sheffield, GB); Rory Evan Charlesworth (Sheffield, GB); Viktor Pap-Kovacs (Veszprem, HU)
Assignee: SHAWBROOK BANK LIMITED
B29C64/30B05D1/02B05D1/60B05D5/06B05D7/02B33Y40/20C23C14/24
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 11,628,623
App. No.
16/754,352
Granted
Apr 18, 2023
Kind
B2
Abstract

The present application describes apparatus ( 100 ) for colouring an additively manufactured polymer part, comprising a chamber ( 106 ) for locating at least one additively manufactured polymer part ( 105 ) to be coloured, a first reservoir ( 102 ) for containing dye pigment particles to be suspended in a gas, and fluidly coupled to the chamber, and a further reservoir ( 104 ) for containing a solvent vapour, and fluidly coupled to the chamber. A method of colouring an additively manufactured polymer part is also described.

Claims (28)

1. A method of colouring an additively manufactured polymer part, comprising:

locating an additively manufactured polymer part in a chamber;

providing a liquid solvent in a solvent reservoir;

heating the liquid solvent in the solvent reservoir to cause the liquid solvent to vaporise to produce a solvent vapour within the solvent reservoir;

introducing the solvent vapour from the solvent reservoir into the chamber;

dissolving or softening a surface of the additively manufactured polymer part located within the chamber using the solvent vapour to create a dissolved or softened surface;

introducing dye pigment particles into the chamber, wherein the dye pigment particles introduced into the chamber are suspended in a gas or in said solvent vapour; and

adhering the dye pigment particles onto the dissolved or softened surface of the additively manufactured polymer part whereby, upon adhering to the dissolved or softened surface, the dye pigment particles serve to colour the dissolved or softened surface of the additively manufactured part.

2. The method according to claim 1 , comprising providing a particle reservoir, said particle reservoir being fluidly coupled to the chamber, and suspending the dye pigment particles in a gas within the particle reservoir prior to said dye pigment particles being introduced into the chamber.

3. The method according to claim 2 , wherein the step of introducing dye pigment particles into the chamber comprises selectively pressurising the particle reservoir so as to cause the dye pigment particles contained therein to transfer into the chamber.

4. The method according to claim 2 , wherein the chamber and the particle reservoir are each held at a respective pressure, and wherein the method further comprises reducing the pressure in the chamber such that the pressure in the chamber is less than the pressure in the particle reservoir so as to cause the dye pigment particles contained within the particle reservoir to transfer into the chamber.

5. The method according to claim 1 , wherein, after the introduction of the solvent vapour and the dye pigment particles into the chamber, the chamber contains a mixture of air, the solvent vapour, and the dye pigment particles; and wherein the method further comprises passing said mixture through a recovery system so as to recover the solvent vapour and the dye pigment particles from the mixture, and then, after the solvent vapour and the dye pigment particles have been recovered, releasing the remaining air into the atmosphere.

6. The method according to claim 1 , wherein the chamber and the solvent reservoir are each held at a respective pressure, and wherein the method further comprises reducing the pressure in the chamber such that the pressure in the chamber is less than the pressure in the solvent reservoir so as to cause the solvent vapour contained within the solvent reservoir to transfer into the chamber.

7. The method according to claim 1 , wherein the solvent comprises at least one of the following: 1,1,1,3,3,3-hexafluoro-2-propanol (HFIP), dimethylformamide, sulphuric acid, m-cresol, formic acid, trifluoroacetic acid, 2-Methyltetrahydrofuran (Me-THF), Dimethyl sulfoxide and benzyl alcohol.

8. A method of disposing dye pigment particles onto a surface of an additively manufactured polymer part, comprising:

locating an additively manufactured polymer part in a chamber;

introducing a solvent vapour into the chamber;

dissolving or softening a surface of the additively manufactured polymer part located within the chamber using the solvent vapour to create a dissolved or softened surface; and

introducing dye pigment particles into the chamber, wherein the dye pigment particles introduced into the chamber are suspended in a gas or in said solvent vapour; and

adhering the dye pigment particles onto the dissolved or softened surface of the additively manufactured polymer part whereby, upon adhering to the dissolved or softened surface, the dye pigment particles serve to colour the dissolved or softened surface of the additively manufactured part.

9. A method of aligning particles on a surface of an additively manufactured polymer part, comprising:

locating an additively manufactured polymer part in a chamber;

introducing a solvent vapour into the chamber to dissolve/soften a surface of the additively manufactured polymer part;

introducing at least partially magnetic particles suspended in a gas into the chamber to adhere the at least partially magnetic particles onto the surface of the additively manufactured polymer part,

wherein the at least partially magnetic particles are initially deposited onto the surface of the additively manufactured polymer part in a random orientation;

applying a magnetic field across the chamber whilst the particles are suspended in the softened surface of the additively manufactured polymer part so as to align the randomly orientated particles into a desired orientation in the direction of the magnetic field; and

allowing the softened surface of the additively manufactured polymer part to solidify so as to fix the at least partially magnetic particles in the desired orientation.

10. The method according to claim 9 , comprising selectively moving at least one magnet with respect to the chamber to thereby orient the magnetic field in a desired direction across the chamber and a part located therein.

Assignments (2)
SECURITY INTEREST Recorded Jul 21, 2022
From: ADDITIVE MANUFACTURING TECHNOLOGIES LTD
To: SHAWBROOK BANK LIMITED
Reel/Frame 060583/0182 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Aug 31, 2021
From: CRABTREE, JOSEPH GWILLIAM; RYBALCENKO, KONSTANTIN; GAIO, ANDRE; IOANNIDES, GIORGIO; CHARLESWORTH, RORY EVAN; PAP-KOVACS, VIKTOR
To: ADDITIVE MANUFACTURING TECHNOLOGIES LIMITED
Reel/Frame 057345/0336 →
Priority Claims (1)
GB 1812476.8 · Jul 31, 2018 · national
Continuity (1)
Related Publication 20200238620A1 · Jul 30, 2020