Sintered metal friction material

Inventors: Makoto Yasuda (Tokyo, JP); Takuya Kinomura (Tokyo, JP)
Assignee: TOKAI CARBON CO., LTD.
F16D69/027B22F7/04B22F9/082B22F9/30C22C1/05C22C38/002C22C38/008C22C38/08C22C38/16B22F2301/35F16D2200/0008F16D2200/0086
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 11,644,076
App. No.
16/476,652
Granted
May 9, 2023
Kind
B2
Abstract

The present invention provides a sintered metal friction material that has excellent wear resistance, heat resistance even at high load and has a higher friction coefficient while maintaining a friction coefficient and wear resistance that are hard to decrease, and has a reduced content of copper of less than 5 mass %. There is provided a sintered metal friction material characterized in that the sintered metal friction material comprises a sintered material of a friction material composition, the friction material composition comprises matrix metals and a friction modifier, the matrix metals comprise following 20 to 40 mass % of iron powder, 20 to 40 mass % of nickel powder, 0.5 to 10 mass % of zinc powder, 0.5 to 5 mass, of tin powder, 0.5 to 4 mass % of copper powder and 0.5 to 5 mass % of sintering assist powder.

Claims (16)

1. A sintered metal friction material wherein the sintered metal friction material comprises a sintered material of a friction material composition,

the friction material composition comprises matrix metals and a friction modifier,

the matrix metals consist of

20 to 40 mass % of iron powder,

20 to 40 mass % of nickel powder,

0.5 to 10 mass % of zinc powder,

0.5 to 5 mass % of tin powder,

0.5 to 4 mass % of copper powder and

0.5 to 5 mass % of sintering assist powder,

wherein the total content of the matrix metals in the friction material composition is 42 to 95 mass % and the content of the friction modifier in the friction material composition is 5 to 58 mass %.

2. The sintered metal friction material according to claim 1 , wherein the total content of the iron powder and the nickel powder in the friction material composition is 40 to 80 mass %.

3. The sintered metal friction material according to claim 1 , wherein the sintering assist powder is one or more selected from iron boride powder, iron phosphide powder, copper phosphide powder and phosphor bronze powder.

4. The sintered metal friction material according to claim 1 , wherein

the friction modifier comprises a lubricant material and a hard material,

the lubricant material is one or more selected from graphite powder, coke powder, calcium fluoride powder, barium fluoride powder, boron nitride powder and molybdenum disulfide powder, and

the hard material is one or more selected from alumina powder, mullite powder, zircon sand powder and silica powder.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jul 29, 2019
From: YASUDA, MAKOTO
To: TOKAI CARBON CO., LTD.
Reel/Frame 049889/0384 →
Priority Claims (1)
JP JP2017-001898 · Jan 10, 2017 · national
Continuity (1)
Related Publication 20210041002A1 · Feb 11, 2021