IP Library Granted Patent US 11,672,883
Granted Patent B2
US 11,672,883 · App. 15/965,284 · Granted Jun 13, 2023

Shape memory articles and methods for controlling properties

Inventors: Richard Francis (Santa Rosa, CA); Brett Vegoe (Santa Rosa, CA); Curtis Goreham-Voss (Santa Rosa, CA); Dhiraj Catoor (Santa Rosa, CA); Scott Robertson (San Francisco, CA)
Assignee: MEDTRONIC, INC.
A61L27/047A61L27/06A61L27/50C22C1/02C22C14/00C22C19/03C22F1/006C22F1/10A61F2/2418A61F2/86A61F2/91A61F2210/0014A61F2210/0019A61F2240/001A61L2400/16A61L2430/20C21D2201/01
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 11,672,883
App. No.
15/965,284
Granted
Jun 13, 2023
Kind
B2
Abstract

Methods for controlling properties of structural elements of implantable medical devices, where the structural elements contain shape memory alloys (SMAs) include promoting or inhibiting in vivo formation of R-phase crystal structure or converging or separating the R-phase from the austenite phase.

Claims (7)

1. A method for enhancing displacement-controlled fatigue performance, increasing ductility or decreasing modulus of a structural element of an implantable medical device, wherein the structural element comprises a shape memory alloy material, the method comprising:

a first step consisting essentially of: heating the structural element at a temperature between 580° C. and 620° C. for a time between 30 seconds and 500 minutes to produce a heat-treated structural element; and

a second step comprising: shape setting the heat-treated structural element after the structural element is heated.

2. The method of claim 1 , wherein heating the structural element comprises heating the structural element at a temperature between 590° C. and 615° C.

3. The method of claim 1 , wherein heating the structural element comprises heating the structural element at a temperature between 595° C. and 610° C.

4. The method of claim 1 , wherein the time for which the structural element is heated is between 60 seconds and 100 minutes.

5. The method of claim 1 , wherein the shape memory alloy comprises a NiTi alloy.

Assignments (2)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Dec 24, 2022
From: FRANCIS, RICHARD
To: MEDTRONIC, INC.
Reel/Frame 062199/0470 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Dec 24, 2022
From: FRANCIS, RICHARD; VEGOE, BRETT; GOREHAM-VOSS, CURTIS; ROBERTSON, SCOTT; CATOOR, DHIRAJ
To: MEDTRONIC, INC.
Reel/Frame 062199/0472 →
Continuity (3)
Provisional Application 62529121 · Jul 6, 2017
Provisional Application 62491423 · Apr 28, 2017
Related Publication 20180311406A1 · Nov 1, 2018