IP Library › Granted Patent US 11,817,550
Granted Patent B2
US 11,817,550 · App. 17/239,593 · Granted Nov 14, 2023

Method of synthesizing a solid-state electrolyte for use in a lithium-ion battery

Inventors: Ali Sadeghi (Atherton, CA); Yuri Vorobyev (San Carlos, CA); Gene Kristul (San Francisco, CA); Leonid Velikov (San Carlos, CA)
H01M10/0562H01M10/0525H01M2300/008
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 11,817,550
App. No.
17/239,593
Granted
Nov 14, 2023
Kind
B2
Abstract

Proposed is a method of synthesizing a solid-state electrolyte of Li 3 HalO formula for use in a lithium-ion battery. The method consists of uniformly mixing at least LiOH and LiHal in a stoichiometric quantities, heating the prepared mixture to a melting temperature and causing a reaction of formula (2LiOH+LiHal=Li 3 HalO+H 2 O) between the at least LiOH and LiHal in a process free of forming a perovskite structure and at a temperature, at which H 2 O that forms at the aforementioned reaction is converted into a bound form, whereby a reaction product is obtained. According to another modification of the method, prior to the stage of melting the mixture, a reinforcement mesh is immersed into the mixture, whereby after mixture is solidified, a solid-state electrolyte reinforced with the mixture embedded into its material is obtained.

Claims (2)

1. A method of synthesizing a solid-state electrolyte for use in a lithium-ion battery, the method comprising: uniformly mixing at least LiOH and LiHal in stoichiometric quantities thus forming a uniform mixture of the at least LiOH and LiHal: heating the uniform mixture to a mixture melting temperature thus forming a mixture melt; causing a reaction of formula (2LiOH+LiHal=Li 3 HalO+H 2 O) between the at least LiOH and LiHal in a process free of forming an anti-perovskite structure and at a temperature, at which H 2 O that is formed in the aforementioned reaction is converted into a bound form, whereby a reaction product is obtained: and cooling the reaction product to a solid state, whereby a solid-state electrolyte for use in a lithium-ion battery is obtained; the Hal being selected at least from CI, Br, and/or I; the synthesizing being carried out in solid electrolyte synthesizing tools comprising a container having a container bottom and made of a heat-resistant material, a cuvette having a cuvette bottom placed onto the container bottom, and a pallet having a top surface and placed onto the cuvette bottom, and wherein, prior to the step of heating the uniform mixture, the solid electrolyte synthesizing tools being preheated to a temperature in the range of 180° C. to 220° C., and the uniform mixture is then loaded onto the top surface of the pallet, wherein the cuvette is made of a metal foil, the pallet is made of metal, and the top surface of the pallet has a polished surface.

2. A method of synthesizing a solid-state electrolyte for use in a lithium-ion battery, the method comprising: uniformly mixing at least LiOH and LiHal in stoichiometric quantities thus forming a uniform mixture of the at least LiOH and LiHal; heating the uniform mixture to a mixture melting temperature thus forming a mixture melt; causing a reaction of formula (2LiOH+LiHal=Li 3 HalO+H 2 O) between the at least LiOH and LiHal in a process free of forming an anti-perovskite structure and at a temperature, at which H 2 O that is formed in the aforementioned reaction is converted into a bound form, whereby a reaction product is obtained; and cooling the reaction product to a solid state, whereby a solid-state electrolyte of Li 3 HalO formula for use in a lithium-ion battery is obtained; the Hal being selected at least from Cl, Br, and/or I; oxides of Ca, Ba, Mg, and/or Sr being selectively added to the mixture in amounts of 0.001 wt. % to 6 wt. %, to create solid solutions in the obtained solid electrolyte; wherein the synthesizing is carried out in solid electrolyte synthesizing tools comprising a container having a container bottom and made of a heat-resistant material, a cuvette having a cuvette bottom placed onto the container bottom, and a pallet having a top surface and placed onto the cuvette bottom, wherein prior to the step of heating the uniform mixture, the solid electrolyte synthesizing tools is preheated to a temperature in the range of 180° C. to 220° C. and the uniform mixture is then loaded onto the top surface of the pallet; and wherein the cuvette is made of a metal foil, the pallet is made of metal, and the top surface of the pallet has a polished surface.

Continuity (1)
Related Publication 20220344701A1 · Oct 27, 2022