Lithium containing nano powders, mechanical alloys, or combinations thereof; methods, and systems for manufacturing the same

Inventors: Zhuo Chen (Ontario, CA); Shizhu Chen (Ontario, CA); Hui Li (Sugarland, TX); Pufang Xiao (Ontario, CA)
Assignee: ABM Nano LLC
B02C17/1815B02C17/18H01M4/485
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 11,998,923
App. No.
17/664,044
Granted
Jun 4, 2024
Kind
B2
Abstract

One general aspect of the present disclosure is directed to a method of manufacturing a lithium containing nano powder. An additional general aspect of the present disclosure relates to a system for manufacturing the lithium containing nano powder. A further general aspect of the present disclosure pertains to the lithium containing nano powder. A further general aspect of the present disclosure relates to converting a plurality of metals, a plurality of metal oxides, or a combination thereof into a mechanical alloy using the manufacturing method and system of the present disclosure. The mechanical alloy may be a powder, e.g., a nano powder, and may or may not include the lithium containing nano powder.

Claims (28)

1. A method comprising:

milling microscopic lithium lanthanum zirconium oxide (LLZO) powder with a milling device while the milling device is in a first position;

turning the milling device, so that the milling device is in a second position;

agitating the microscopic LLZO powder while the milling device is in the second position;

cooling the microscopic LLZO powder while the milling device is in the second position;

returning the milling device to the first position; and

repeating the milling, turning, agitating, cooling, and returning steps until the microscopic LLZO powder is converted into LLZO nano powder.

2. The method of claim 1 , where the milling device is a ball mill comprising:

a milling chamber; and

a plurality of milling balls.

3. The method of claim 1 , where the microscopic LLZO powder has an average particle size of 1 to 1000 microns.

4. The method of claim 1 , further comprising synthesizing the microscopic LLZO powder within the milling device using a plurality of metals, a plurality of metal oxides, or a combination thereof.

5. The method of claim 1 , where milling the microscopic LLZO powder comprises rotating the milling device about an axis of the milling device at a rotational speed of 100 rpm to 3000 rpm.

6. The method of claim 1 , where the first position is a vertical position.

7. The method of claim 1 , where the second position is a horizontal position.

8. The method of claim 1 , where turning the milling device to the second position comprises turning the milling device 90°.

9. The method of claim 1 , where returning the milling device to the first position comprises turning the milling device 90° in an opposite direction.

10. The method of claim 1 , where the LLZO nano powder has an average particle size of 1 nm to 500 nm.

11. The method of claim 1 , where a temperature inside the milling device ranges from 20° C. to 180° C.

12. The method of claim 1 , where agitating the microscopic LLZO powder inside the milling device comprises striking the milling device with an impact rod.

13. The method of claim 1 , where agitating the microscopic LLZO powder comprises rotating the milling device about an axis of the milling device at a rotational speed of 5 rpm to 500 rpm.

14. The method of claim 1 , where cooling the microscopic LLZO powder comprises directly contacting the milling device with a cooling medium by dispersing a cooling medium to an area surrounding the milling device using a nozzle.

15. The method of claim 1 , where cooling the microscopic LLZO powder comprises indirectly contacting the milling device with a cooling medium by running the cooling medium through a cooling jacket that surrounds the milling device.

16. The method of claim 1 , where the method does not comprise contacting the microscopic LLZO powder with a liquid.

17. The method of claim 1 , where the method does not comprise contacting the microscopic LLZO powder with a solvent.

18. The method of claim 1 , where the method results in a production yield, of the LLZO nano powder, of 98% to 100%.

19. The method of claim 1 where the LLZO nano powder has an average particle size of 1 nanometers to 500 nanometers.

20. The method of claim 1 where the LLZO powder has the lithium containing nano powder has a particle density of 0.1 g/cm 3 to 5 g/cm 3 .

Continuity (2)
Provisional Application 63190732 · May 19, 2021
Related Publication 20220371023A1 · Nov 24, 2022