Method for engineered geothermal system treatment using brines
A method of repairing a well is provided. The method includes injecting a brine solution into the well, injecting carbon dioxide into the well, and reacting the brine solution in the reservoir rock with the carbon dioxide to form calcite such that calcite precipitates into the desired flow path between a cold well and a hot well to effectively repair short circuits within the EGS reservoir.
1. A method of fracturing rock comprising:
drilling a well;
super-cooling a brine solution;
injecting the brine solution into the well;
contacting rock in the well with the brine solution; and
fracturing the rock responsive to contacting the rock with the brine solution.
2. The method of claim 1 , further comprising:
removing heat from the rock in the well responsive to contacting the rock with the brine solution.
3. The method of claim 1 , further comprising:
cooling and contracting the rock responsive to contacting the rock with the brine solution.
4. The method of claim 1 , wherein super-cooling the brine solution comprises super-cooling the brine solution to a temperature less than 20° F.
5. The method of claim 1 , wherein super-cooling the brine solution comprises super-cooling the brine solution to a temperature less than −0° F.
6. The method of claim 1 , wherein super-cooling the brine solution comprises super-cooling the brine solution to a temperature less than −20° F.
7. The method of claim 1 , wherein the brine solution is a rich calcium brine solution.
8. The method of claim 1 , wherein the brine solution is a supersaturated brine solution.
9. The method of claim 1 , wherein the brine solution is a supersaturated calcium brine solution.
10. The method of claim 9 , wherein the supersaturated calcium brine solution includes approximately 30% to 40% by wt. calcium chloride.
11. The method of claim 1 , wherein the brine solution is a calcium brine solution.
12. The method of claim 11 , wherein a freezing point of the calcium brine solution is approximately 28° F. to approximately 12° F.
13. The method of claim 11 , wherein a freezing point of the calcium brine solution is approximately 12° F. to approximately −22° F.
14. The method of claim 11 , wherein a freezing point of the calcium brine solution is approximately −22° F. to approximately −35° F.
15. The method of claim 11 , wherein the calcium brine solution includes at least one of approximately 5% to 15% by wt. calcium chloride, approximately 15% to 25% by wt. calcium chloride, and approximately 25% to 38% by wt. calcium chloride.
16. The method of claim 11 , wherein the calcium brine solution absorbs heat from the rock.
17. The method of claim 11 , wherein the calcium brine solution reduces the temperature of the well.
18. The method of claim 1 , further comprising:
creating a conductive flow path for subsequent brine injection for heat transfer.
19. The method of claim 1 , further comprising:
preparing a brine solution.
20. The method of claim 19 , wherein preparing the brine solution comprises preparing a calcium brine solution, a rich calcium brine solution, a supersaturated brine solution, or a supersaturated calcium brine solution.