Seals and methods of making seals

Inventors: Pantcho P. Stoyanov (West Hartford, CT); Eli N. Ross (Vernon, CT)
Assignee: RTX CORPORATION
F01D11/003B23K9/04F16J15/0806F16J15/16B23K2103/10F05D2240/55F05D2300/177
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 12,055,043
App. No.
18/108,136
Filed
Feb 10, 2023
Granted
Aug 6, 2024
Kind
B2
Art Unit
3745
USPC
415/230
Abstract

A method includes providing a powdered high entropy alloy and forming the powdered high entropy alloy into a seal body with a heat source. The seal body extends between a leading edge and a trailing edge and includes a first component contact surface adjacent the leading edge and a second component contact surface adjacent the trailing edge. The seal body is operable at temperatures in excess of 700° C.

Claims (12)

1. A method comprising:

providing a powdered high entropy alloy that has a composition selected from MoNbTaW, AlCoCrFeNiTi, or CoCrFeMnNi; and

forming the powdered high entropy alloy into a seal body with a heat source, wherein the seal body extends between a leading edge and a trailing edge and includes a first component contact surface adjacent the leading edge and a second component contact surface adjacent the trailing edge and is configured to operate at temperatures in excess of 700° C.

2. A The method of claim 1 , wherein the seal body extends from a leading edge to a trailing edge and includes at least one bend.

3. A The method of claim 1 , wherein the seal body extends from a leading edge to a trailing edge and defines a piston seal.

4. A The method of claim 1 , wherein the seal body is a complete ring.

5. A The method of claim 1 , wherein the composition is MoNbTaW.

6. A The method of claim 1 , wherein the composition is AlCoCrFeNiTi.

7. A The method of claim 1 , wherein the composition is CoCrFeMnNi.

8. A The method of claim 1 , wherein the providing of the powdered high entropy alloy includes utilizing a powdered bed of the high entropy alloy and the forming of the powdered high entropy alloy into the seal body with the heat source includes welding or melting adjacent layers of the high entropy alloy in the powdered bed.

9. A The method of claim 1 , wherein the providing of the powdered high entropy alloy includes blowing streams of the powdered high entropy alloy.

10. The method of claim 9 , wherein the forming of the powdered high entropy alloy into the seal body with the heat source includes controlling the heat source to weld or melt the high entropy alloy into a desired shape of the seal body.

Assignments (1)
CHANGE OF NAME Recorded Jul 27, 2023
From: RAYTHEON TECHNOLOGIES CORPORATION
To: RTX CORPORATION
Reel/Frame 064402/0837 →
Continuity (2)
Continuation 17009907 · Sep 2, 2020
Related Publication 20230184124A1 · Jun 15, 2023