IP Library › Granted Patent US 12,071,677
Granted Patent B2
US 12,071,677 · App. 17/879,059 · Granted Aug 27, 2024

Lithium iron phosphate (LFP) battery recycling

Inventors: Eric Gratz (Worcester, MA); Kee-Chan Kim (Worcester, MA)
Assignee: Ascend Elements, Inc.
C22B26/12C22B1/005C22B3/06
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 12,071,677
App. No.
17/879,059
Filed
Aug 2, 2022
Granted
Aug 27, 2024
Kind
B2
Art Unit
1738
USPC
75/743
Abstract

The inventions described herein provide methods and systems for recycling lithium iron phosphate batteries, including: adding an oxidizing agent to a recycling stream of lithium iron phosphate (LiFePO 4 ) batteries to form a leach solution; filtering the leach solution to remove a residue and obtain a lithium rich solution; modifying pH of the lithium rich solution for filtering impurities and obtaining a purified Li solution; and adding a precipitant to the purified Li solution thereby precipitating a lithium compound.

Claims (42)

1. A method for recycling lithium iron phosphate batteries, the method comprising:

shredding a recycling stream of lithium iron phosphate batteries to obtain granular powder comprising cathodes and anodes of batteries including lithium iron phosphate;

adding an oxidizing agent to the granular powder from the recycling stream of lithium iron phosphate (LiFePO 4 ) batteries to form a leach solution;

filtering the leach solution to remove a residue including FePO 4 and graphite and obtain a lithium rich solution;

modifying pH of the lithium rich solution for filtering impurities and obtaining a purified Li solution;

adding a precipitant to the purified Li solution thereby precipitating a lithium compound; and

after filtering, purifying the graphite by at least one process selected from acid leaching and froth flotation.

2. The method according to claim 1 , wherein prior to filtering further comprising heating the leach solution to a temperature in a range between 20° C. to 100° C.

3. The method according to claim 1 , wherein the residue comprises at least one of: graphite and FePO 4 .

4. The method according to claim 1 , wherein modifying the pH of the lithium rich solution further comprises adding a basic solution.

5. The method according to claim 4 , wherein the lithium rich solution is modified to attain the pH in a range between 5 to 13.

6. The method according to claim 1 further comprising achieving a concentration of 0.3-3.0 M of the oxidizing agent to a concentration of the LiFePO 4 .

7. The method according to claim 1 further comprising achieving a concentration of 0.5-2.2M of the oxidizing agent to a concentration of the LiFePO 4 .

8. The method according to claim 1 , wherein adding an oxidizing agent further comprises adding an acid solution.

9. The method according to claim 8 , wherein the acid solution is selected from an inorganic acid or an organic acid.

10. The method according to claim 9 , wherein the inorganic acid is at least one selected from: sulfuric acid, hydrochloric acid, nitric acid, and phosphoric acid.

11. The method according to claim 9 , wherein the organic acid is at least one selected from: acetic acid, formic acid, propionic acid, butyric acid, oxalic acid, malonic acid, succinic acid, and adipic acid.

12. The method according to claim 1 , wherein the precipitant is at least one selected from: sodium carbonate, sodium phosphate, phosphoric acid, oxalic acid, and sodium oxalate.

13. The method according to claim 1 , wherein the lithium compound is at least one selected from lithium carbonate (Li 2 CO 3 ), lithium phosphate (Li 3 PO 4 ), and lithium oxalate (Li 2 C 2 O 4 ).

14. The method according to claim 1 further comprising maintaining pH of the leach solution in a range between 1-6.

15. The method according to claim 1 , wherein the oxidizing agent is at least one selected from: a peroxide (O 2 2− ), a persulfate (S 2 O 8 2− ), a sulfate (SO 4 2 —), a hypoclorite (ClO − ), a chlorite (ClO 2 − ), a chlorate (ClO 3 − ), a perchlorate (ClO 4 − ), a nitrate (NO 3 − ), a nitrous oxide (N 2 O), a nitrogen dioxide (NO 2 ), and a halogen.

16. The method according to claim 1 , wherein the oxidizing agent is at least one selected from: hydrogen peroxide, sodium persulfate, and ammonium persulfate.

17. The method of claim 1 wherein the lithium products are lithium phosphate or lithium oxalate.

18. The method of claim 1 wherein the impurities are other than Ni, Mn and Co.

19. The method of claim 1 wherein the recycling stream includes cathode materials and anode materials, the lithium iron phosphate included in the cathode materials.

20. The method of claim 1 further comprising modifying pH of the lithium rich solution by raising the pH to 11-13 for filtering impurities.

21. A method for recycling lithium iron phosphate batteries, the method comprising:

shredding the lithium iron phosphate batteries to obtain a recycling stream of a granular powder comprising cathodes and anodes and including lithium iron phosphate;

adding at least one of: an oxidizing agent, and an acid, to the granular powder of lithium iron phosphate (LiFePO 4 ) batteries to form a leach solution;

maintaining the temperature of the leach solution from 20° C. to 100° C.;

filtering the leach solution to remove graphite and FePO 4 to obtain a lithium rich solution;

modifying pH of the lithium rich solution from 11 to 13 for filtering impurities and obtaining a purified Li solution;

adding a precipitant to the purified Li solution thereby precipitating a lithium compound; and

after filtering, purifying the graphite by at least one process selected from acid leaching and froth flotation.

22. A method for recycling lithium iron phosphate batteries, the method comprising:

shredding a recycling stream of lithium iron phosphate batteries to obtain granular powder comprising cathodes and anodes of the batteries including lithium iron phosphate;

adding an acid to the recycling stream of powdered lithium iron phosphate (LiFePO 4 ) batteries to form a leach solution;

maintaining the temperature of the leach solution from 20° C. to 100° C.;

filtering the leach solution to remove graphite and FePO 4 to obtain a lithium rich solution;

modifying pH of the lithium rich solution from 11 to 13 for filtering impurities and obtaining a purified Li solution;

adding a precipitant to the purified Li solution thereby precipitating a lithium compound; and

after filtering, purifying the graphite by at least one process selected from acid leaching and froth flotation.

Assignments (4)
TERMINATION AND RELEASE OF INTELLECTUAL PROPERTY SECURITY AGREEMENT Recorded Dec 12, 2025
From: AVENUE CAPITAL MANAGEMENT II, L.P.
To: ASCEND ELEMENTS, INC.
Reel/Frame 073935/0873 →
INTELLECTUAL PROPERTY SECURITY AGREEMENT Recorded Jun 13, 2025
From: ASCEND ELEMENTS, INC.
To: ALTER DOMUS (US) LLC
Reel/Frame 071564/0618 →
SECURITY INTEREST Recorded May 16, 2025
From: ASCEND ELEMENTS, INC.
To: AVENUE CAPITAL MANAGEMENT II, L.P.
Reel/Frame 071147/0634 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Sep 13, 2023
From: GRATZ, ERIC; KIM, KEE-CHAN
To: ASCEND ELEMENTS, INC.
Reel/Frame 064885/0140 →
Continuity (2)
Provisional Application 63228331 · Aug 2, 2021
Related Publication 20230038978A1 · Feb 9, 2023