IP Library › Granted Patent US 12,125,915
Granted Patent B2
US 12,125,915 · App. 17/581,300 · Granted Oct 22, 2024

Source/drain features of multi-gate devices

Inventors: Shahaji B. More (Hsinchu, TW); Cheng-Han Lee (New Taipei, TW)
Assignee: TAIWAN SEMICONDUCTOR MANUFACTURING COMPANY, LTD.
H01L29/78618H01L21/02532H01L21/0259H01L29/0665H01L29/42392H01L29/66545H01L29/66553H01L29/66742H01L29/78696
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 12,125,915
App. No.
17/581,300
Granted
Oct 22, 2024
Kind
B2
Abstract

Methods and semiconductor structures are provided. A method according to the present disclosure includes forming, over a substrate, a fin-shaped structure that includes a plurality of channel layers interleaved by a plurality of sacrificial layers, recessing a source/drain region of the fin-shaped structure to form a source/drain recess that extends into the substrate and exposes a portion of the substrate, selectively and partially recessing sidewalls of the plurality of sacrificial layers to form inner spacer recesses, forming inner spacers in the inner spacer recesses, selectively forming a buffer semiconductor layer on the exposed portion of the substrate, selectively depositing a first epitaxial layer on sidewalls of the plurality of channel layer and the buffer semiconductor layer such that a top surface of the buffer semiconductor layer is completely covered by the first epitaxial layer, and depositing a second epitaxial layer over the first epitaxial layer and the inner spacers.

Claims (66)

1. A method, comprising:

forming a fin-shaped structure over a substrate, the fin-shaped structure comprising a plurality of channel layers interleaved by a plurality of sacrificial layers;

recessing a source/drain region of the fin-shaped structure to form a source/drain recess that extends into the substrate and exposes a portion of the substrate;

selectively and partially recessing sidewalls of the plurality of sacrificial layers to form inner spacer recesses;

forming inner spacers in the inner spacer recesses;

selectively forming a buffer semiconductor layer on the exposed portion of the substrate;

selectively depositing a first epitaxial layer on sidewalls of the plurality of channel layer and the buffer semiconductor layer such that a top surface of the buffer semiconductor layer is completely covered by the first epitaxial layer; and

depositing a second epitaxial layer over the first epitaxial layer and the inner spacers.

2. The method of claim 1 ,

wherein, after the selectively depositing of the first epitaxial layer, the first epitaxial layer comprises a bottom portion disposed on the buffer semiconductor layer,

wherein the bottom portion comprises a cone-like profile.

3. The method of claim 1 ,

wherein, after the selectively depositing of the first epitaxial layer, the first epitaxial layer comprises a bottom portion that completely covers sidewalls of bottommost ones of the inner spacers,

wherein the bottom portion comprises a top surface that is substantially flat.

4. The method of claim 1 ,

wherein the first epitaxial layer comprises a first dopant,

wherein the second epitaxial layer comprises a second dopant different from the first dopant.

5. The method of claim 4 ,

wherein the first dopant comprises arsenic,

wherein the second dopant comprises phosphorus.

6. The method of claim 4 , wherein the buffer semiconductor layer comprises an undoped semiconductor material.

7. The method of claim 1 , wherein the selectively depositing of the first epitaxial layer comprises an etch component and a deposition component.

8. The method of claim 1 , wherein the selectively depositing of the first epitaxial layer comprises a process pressure between about 10 Torr and about 300 Torr.

9. The method of claim 1 , wherein the selectively depositing of the first epitaxial layer comprises a process temperature between about 600° C. and about 700° C.

10. The method of claim 1 , further comprising:

after the depositing of the second epitaxial layer, depositing a third epitaxial layer on the second epitaxial layer.

11. A method, comprising:

forming a stack over a substrate, the stack comprising a plurality of channel layers interleaved by a plurality of sacrificial layers;

patterning the stack and the substrate into a fin-shaped structure;

forming a dummy gate stack over a channel region of the fin-shaped structure;

recessing a source/drain region of the fin-shaped structure to expose a portion of the substrate, the source/drain region being adjacent the channel region;

after the recessing of the source/drain region, selectively and partially recessing sidewalls of the plurality of sacrificial layers to form inner spacer recesses;

forming inner spacers in the inner spacer recesses;

selectively forming an undoped semiconductor layer on the exposed portion of the substrate;

selectively depositing a shielding epitaxial layer on sidewalls of the plurality of channel layer and surfaces of the undoped semiconductor layer;

depositing a heavily doped epitaxial layer over the shielding epitaxial layer and the inner spacers such that the heavily doped epitaxial layer is spaced apart from the undoped semiconductor layer by the shielding epitaxial layer; and

depositing a capping epitaxial layer over the heavily doped epitaxial layer.

12. The method of claim 11 , wherein the undoped semiconductor layer comprises undoped silicon or undoped silicon germanium.

13. The method of claim 11 ,

wherein the shielding epitaxial layer is doped with arsenic,

wherein the heavily doped epitaxial layer is doped with phosphorus.

14. The method of claim 13

wherein a concentration of arsenic in the shielding epitaxial layer is between about 5×10 20 atoms/cm 3 and about 2×10 21 atoms/cm 3 ,

wherein a concentration of phosphorus in the heavily doped epitaxial layer is between about 1×10 21 atoms/cm 3 and about 4×10 22 atoms/cm 3 .

15. The method of claim 11 ,

wherein the selectively depositing of the shielding epitaxial layer comprises a process pressure between about 10 Torr and about 300 Torr,

wherein the selectively depositing of the shielding epitaxial layer comprises a process temperature between about 600° C. and about 700° C.

16. A method, comprising:

forming a fin-shaped structure over a substrate, the fin-shaped structure comprising a plurality of channel layers interleaved by a plurality of sacrificial layers;

recessing a source/drain region of the fin-shaped structure to form a source/drain recess that extends into the substrate and exposes a portion of the substrate;

selectively and partially recessing sidewalls of the plurality of sacrificial layers to form inner spacer recesses;

forming inner spacers in the inner spacer recesses;

selectively forming an undoped semiconductor layer on the exposed portion of the substrate;

selectively depositing a first epitaxial layer on sidewalls of the plurality of channel layer and the undoped semiconductor layer; and

depositing a second epitaxial layer over the first epitaxial layer and the inner spacers,

wherein the selectively forming of the undoped semiconductor layer is performed in a first process chamber,

wherein the selectively depositing the first epitaxial layer and the depositing of the second epitaxial layer are performed in a second process chamber different from the first process chamber.

17. The method of claim 16 , wherein the selectively depositing of the first epitaxial layer comprises a growth-etch deposition process.

18. The method of claim 17 , wherein the growth-etch deposition process comprises between about 2 and about 5 growth cycles and between about 2 and about 5 etch cycles.

19. The method of claim 16 ,

wherein the first epitaxial layer comprises a bottom portion disposed on the undoped semiconductor layer and a sidewall portion disposed on sidewalls of the plurality of channel layers,

wherein the bottom portion comprises a thickness between about 5 nm and about 20 nm,

wherein the sidewall portion comprises a thickness between about 2 nm and about 5 nm.

20. The method of claim 19 ,

wherein the plurality of channel layers extend lengthwise along a first direction,

wherein, when viewed along a second direction perpendicular to the first direction, the bottom portion comprises a cone-like profile.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jan 21, 2022
From: MORE, SHAHAJI B.; LEE, CHENG-HAN
To: TAIWAN SEMICONDUCTOR MANUFACTURING COMPANY, LTD.
Reel/Frame 058726/0915 →
Continuity (2)
Provisional Application 63255200 · Oct 13, 2021
Related Publication 20230114789A1 · Apr 13, 2023