IP Library Granted Patent US 12,266,798
Granted Patent B2
US 12,266,798 · App. 18/724,930 · Granted Apr 1, 2025

Negative electrode plate, a method for manufacturing thereof, and a lithium battery

Inventors: Kai Yang (Changzhou, CN); Jing Liu (Changzhou, CN); Shuaibin Lou (Changzhou, CN); Hongxin Yang (Changzhou, CN)
Assignee: SVOLT ENERGY TECHNOLOGY CO., LTD.
H01M4/583H01M4/0435H01M4/0471H01M4/133H01M4/1393H01M4/623H01M4/625H01M4/626H01M10/0525H01M2004/027
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 12,266,798
App. No.
18/724,930
Granted
Apr 1, 2025
Kind
B2
Abstract

A negative electrode plate comprising a substrate, which comprises a current collector and negative electrode active material bonded on the current collector; first lithium bands arranged on a front surface of the substrate; second lithium bands arranged on a back surface of the substrate; the first lithium bands and the second lithium bands are mutually staggered; adjacent ones of the first lithium bands are spaced apart and adjacent ones of the second lithium bands are spaced apart, respectively.

Claims (16)

1. A negative electrode plate, comprising:

a substrate, which comprises a current collector and negative electrode active material bonded on the current collector;

first lithium bands arranged on a front surface of the substrate;

second lithium bands arranged on a back surface of the substrate; and

the first lithium bands and the second lithium bands are mutually staggered; adjacent ones of the first lithium bands are spaced apart and adjacent ones of the second lithium bands are spaced apart, respectively; interval c 1 between two adjacent first lithium bands and width b 1 of each first lithium band meet the following relational expression: c 1 =b 1 ; interval c 2 between two adjacent second lithium bands and width b 2 of each second lithium band meet the following relational expression: c 2 =b 2 ; a distance between the midline of one first lithium band and the midlines of its two adjacent second lithium bands are respectively d 1 and d 2 , d 1 =d 2 ; the negative electrode active material comprises, by weight, 94-97.5 parts of carbon material, lithium titanate, or silicon monoxide, 0.5-1.5 parts of conductive agent, 1-2 parts of binder, 0.5-1.5 parts of thickener and 0.5-1.5 parts of lithium-containing additive; and the carbon material is selected from at least one of graphite, mesophase carbon microspheres and silicon-carbon composite material.

2. The negative electrode plate according to claim 1 , wherein, the conductive agent is at least one selected from the group consisting of carbon black, carbon nanotube and graphene; or,

the lithium-containing additive is at least one selected from the group consisting of lithium acetate, lithium thiosulfate, lithium benzoate, lithium alkyl sulfate and lithium cellulose; or,

the thickener is at least one selected from the group consisting of sodium carboxymethyl cellulose, hydroxyethyl cellulose and hydroxypropyl methyl cellulose; or

the binder is at least one selected from the group consisting of polyvinylidene fluoride, sodium carboxymethyl cellulose, polytetrafluoroethylene, polypropylene, polyacrylonitrile, styrene-butadiene rubber and polybutadiene.

3. A method for manufacturing the negative electrode plate according to claim 1 , comprising the following steps:

arranging the first lithium bands and the second lithium bands on the front surface and the back surface of the substrate, respectively, in such a way that the first lithium bands and the second lithium bands are mutually staggered, adjacent ones of the first lithium bands are spaced apart, and adjacent ones of the second lithium bands are spaced apart, respectively, and performing press-fitting to produce a negative electrode plate.

4. The method according to claim 3 , wherein, the step of press-fitting is carried out by single or multiple rolling.

5. A lithium battery, comprising the negative electrode plate according to claim 1 .

6. The method according to claim 3 , wherein, a first heating is performed before the step of press-fitting, and the first heating comprises standing in a vacuum environment at 42-48° C. for 2-4 h, heating to 62-68° C. and then standing for 3-5 h, heating to 82-88° C. and then standing for 9-11 h.

7. The method according to claim 6 , wherein, a second heating is performed after the step of press-fitting, and the second heating comprises standing in a vacuum environment at 82-88° C. for 3-5 h.

8. The method according to claim 4 , wherein, an interval time of multiple rolling is 1-2 h.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jul 1, 2024
From: YANG, KAI; LIU, JING; LOU, SHUAIBIN; YANG, HONGXIN
To: SVOLT ENERGY TECHNOLOGY CO., LTD.
Reel/Frame 067886/0892 →
Priority Claims (1)
CN 202210199929.6 · Mar 2, 2022 · national
Continuity (1)
Related Publication 20240421307A1 · Dec 19, 2024
References Cited (17)
US 6001139A · Asanuma et al. · 1999 [cited by applicant]
US 10505182B2 · Zhong · 2019 [cited by examiner]
US 11515526B2 · Chae · 2022 [cited by examiner]
US 20220069284A1 · Yang et al. · 2022 [cited by applicant]
CN 1177417A · 1998 [cited by applicant]
CN 102544578A · 2012 [cited by applicant]
CN 105390298A · 2016 [cited by applicant]
CN 105513828A · 2016 [cited by applicant]
CN 105869898A · 2016 [cited by applicant]
CN 106602133A · 2017 [cited by applicant]
CN 111384405A · 2020 [cited by applicant]
CN 113851603A · 2021 [cited by applicant]
CN 113889600A · 2022 [cited by applicant]
CN 114551796A · 2022 [cited by applicant]
JP 2014146475A · 2014 [cited by applicant]
Chinese Office action dated Jul. 4, 2023 as received in application No. 202210199929.6. [cited by applicant]
Chinese Office action dated Dec. 29, 2023 as received in application No. 202210199929.6. [cited by applicant]