IP Library › Granted Patent US 12,364,990
Granted Patent B2
US 12,364,990 · App. 17/643,477 · Granted Jul 22, 2025

MySx/ZSH mixture as sulfidizing agent

Inventors: Matthias Folchnandt (Cologne, DE); Olaf Klobes (Greiz, DE); Ulises Picardi (El Prat de Llobregat, ES); Rodrigo M. Giménez (Santiago, CL); Leandro Prats (Santa Fe, AR)
Assignee: NOURYON CHEMICALS INTERNATIONAL B.V.
B03B1/04B03D1/002C01B17/22B03D1/008B03D1/012B03D1/014B03D1/018B03D2201/02B03D2203/025C02F1/24
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 12,364,990
App. No.
17/643,477
Granted
Jul 22, 2025
Kind
B2
Abstract

The disclosure is directed to a sulfidizing agent obtainable by mixing M y S x and ZSH in a weight ratio of from about 90:10 to about 10:90, wherein M is chosen from Li + , Na + , K + , Rb + , Cs + , NH 4 + , Mg 2+ and Ca 2+ , y is about 1 or about 2, x is from about 1.1 to about 5, and Z is independently chosen from Li + , Na + , K + , Rb + , Cs + and NH 4 + , and a process for using the sulfidizing agent in the recovery of one or more metal ores and/or polymetallic minerals from gangue.

Claims (29)

1. A process for recovering one or more metal ores and/or polymetallic minerals from gangue, said process comprising:

(i) treating the one or more metal ores and/or polymetallic minerals with a sulfidizing agent; and

(ii) separating the treated metal ores and/or polymetallic minerals using a sulfide floatation process;

wherein the sulfidizing agent is obtained by mixing M y S x and ZSH in a weight ratio of from about 90:10 to about 10:90, wherein M is chosen from Li + , Na + , K + , Rb + , Cs + , NH 4 + , Mg 2+ and Ca 2+ , y is about 1 or about 2, x is from about 2.1 to about 5, and Z is independently chosen from Li + , Na + , K + , Rb + , Cs + and NH 4 + ;

wherein the treatment in (i) is performed by adding a first portion of sulfidizing agent to the one or more metal ores and/or polymetallic minerals in a rougher floatation stage of the sulfide floatation process and adding a further portion of sulfidizing agent to the one of metal ores and/or polymetallic minerals in at least one cleaning stage of the sulfide floatation process; and

wherein the sulfidizing agent is added to the rougher floatation stage in an amount of from about 10 to about 70 g/ton and to the at least one cleaning stage in an amount of from about 3 to about 15 g/ton, based on a dose of grams of agent per ton of dry ore/dry mineral.

2. The process as claimed in claim 1 , wherein x is from about 2.1 to about 4.5.

3. The process as claimed in claim 2 , wherein M and/or Z is chosen from Li + , Na + , K + , Rb + and Cs + .

4. The process as claimed in claim 2 , wherein the weight ratio M y S x to ZSH is from about 90:10 to about 30:70.

5. The process as claimed in claim 2 , wherein the sulfidizing agent comprises a dithiophosphate or a monothiophosphate-based collector and/or a polyglycol-based foaming agent.

6. The process as claimed in claim 2 , wherein the one or more metal ores is chosen from ores of copper (Cu), molybdenum (Mo), gold (Au), silver (Ag), lead (Pb), Nickel (Ni) and Cobalt (Co) and/or the one or more polymetallic minerals is chosen from Cu—Mo, Cu—Au, Pb—Zn—Cu, Ag—Cu, Zn—Pb—Ag, Cu—Zn—Pb—Ag, Sn—Cu and Zn—Pb minerals.

7. The process as claimed in claim 2 , wherein the sulfidizing agent is added to the rougher floatation stage after a delay of at least about 3 minutes after the flotation process begins.

8. The process as claimed in claim 2 , wherein M and/or Z is Na + .

9. The process as claimed in claim 1 , wherein M and/or Z is chosen from Li + , Na + , K + , Rb + and Cs + .

10. The process as claimed in claim 1 , wherein the weight ratio M y S x to ZSH is from about 90:10 to about 30:70.

11. The process as claimed in claim 1 , wherein the sulfidizing agent comprises a dithiophosphate or a monothiophosphate-based collector and/or a polyglycol-based foaming agent.

12. The process as claimed in claim 1 , wherein the one or more metal ores is chosen from ores of copper (Cu), molybdenum (Mo), gold (Au), silver (Ag), lead (Pb), Nickel (Ni) and Cobalt (Co) and/or the one or more polymetallic minerals is chosen from Cu—Mo, Cu—Au, Pb—Zn—Cu, Ag—Cu, Zn—Pb—Ag, Cu—Zn—Pb—Ag, Sn—Cu and Zn—Pb minerals.

13. TheA process as claimed in claim 1 , wherein the sulfidizing agent is added to the rougher floatation stage after a delay of at least about 3 minutes after the flotation process begins.

14. The process as claimed in claim 1 , wherein M and/or Z is Na + .

15. The process as claimed in claim 1 , wherein the weight ratio M y S x to ZSH is from about 90:10 to about 50:50.

16. The process as claimed in claim 1 , wherein the weight ratio M y S x to ZSH is from about 70:30 to about 50:50.

17. The process as claimed in claim 6 wherein the sulfidizing agent is for recovering copper, gold, silver, and/or molybdenum, and/or combinations thereof, from gangue, wherein the sulfidizing agent is obtained by mixing M y S x and ZSH in a weight ratio of about 50:50, wherein M is Na + , y is about 2, x is from about 1.2 to about 2.2, and Z is Na + .

18. The process as claimed in claim 1 , wherein:

x is from about 2.1 to about 4.5;

M and/or Z is chosen from Li + , Na + , K + , Rb + and Cs + so long as at least one of M or Z is Na + ;

the weight ratio M y S x to ZSH is from about 90:10 to about 30:70;

the sulfidizing agent comprises a dithiophosphate or a monothiophosphate-based collector and/or a polyglycol-based foaming agent;

the one or more metal ores is chosen from ores of copper (Cu), molybdenum (Mo), gold (Au), silver (Ag), lead (Pb), Nickel (Ni) and Cobalt (Co) and/or the one or more polymetallic minerals is chosen from Cu—Mo, Cu—Au, Pb—Zn—Cu, Ag—Cu, Zn—Pb—Ag, Cu—Zn—Pb—Ag, Sn—Cu and Zn—Pb minerals; and

the sulfidizing agent is added to the rougher floatation stage after a delay of at least about 3 minutes after the flotation process begins.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Mar 9, 2022
From: FOLCHNANDT, MATTHIAS; KLOBES, OLAF; PICARDI, ULISES; GIMÉNEZ, RODRIGO M.; PRATS, LEANDRO
To: NOURYON CHEMICALS INTERNATIONAL B.V.
Reel/Frame 059202/0630 →
Priority Claims (1)
EP 20383076 · Dec 10, 2020 · regional
Continuity (1)
Related Publication 20220184630A1 · Jun 16, 2022
References Cited (16)
US 2811255A · Nokes · 1957 [cited by examiner]
US 4684459A · Klimpel · 1987 [cited by examiner]
US 20130025410A1 · Saez Navarrete · 2013 [cited by examiner]
US 20190256950A1 · Horn · 2019 [cited by examiner]
CA 2782436A1 · 2011 [cited by examiner]
CL 201800471A · 2018 [cited by applicant]
CN 107790292A · 2018 [cited by examiner]
CN 111530636A · 2020 [cited by examiner]
JP 2009202065A · 2009 [cited by examiner]
JP 2010285639A · 2010 [cited by examiner]
WO WO2015157498A1 · 2015 [cited by examiner]
Le-ming Ou, Bing-yi Yin; A Floatation Technique for a Sulfide-Oxidized Cu-Co Mixed Ore; Nov. 22, 2011; Advanced Materials Research; ISSN 1662-8985, vol. 402, pp. 564-571 (Year: 2011). [cited by examiner]
Wikipedia—http://en.wikipedia.org/wiki/Sodium_polysulfide Aug. 24, 2023 (Year: 2023). [cited by examiner]
Osserov et al. (Non-ferrous Metals, 2017, 2, 3-8). (Year: 2017). [cited by examiner]
Machine translation of CN-111530636-A., pp. 1-9. (Year: 2020). [cited by examiner]
Extended European Search Report dated May 10, 2022, issued in respect of European Patent Application No. EP21210991.2. [cited by applicant]