Expandable material with improved thermal insulation properties and use thereof
A thermally expandable composition includes at least one polymer P, at least one chemical blowing agent CBA, at least one physical blowing agent PBA composed of expandable microspheres, and at least one filler F. A damping element includes a first layer composed of an expansion material and a second layer composed of an acoustic damping material. The damping element is suitable for providing vibration and/or noise damped systems.
1 . A thermally expandable composition comprising:
a1) at least one polymer P,
a2) at least one chemical blowing agent CBA,
a3) at least one physical blowing agent PBA, and
a4) at least one filler F,
wherein the at least one physical blowing agent PBA is composed of expandable microspheres, and
wherein the thermally expandable composition is essentially free of epoxy resins having an average of more than one epoxy group per molecule.
2 . The thermally expandable composition according to claim 1 , wherein the at least one physical blowing agent PBA is composed of expandable polymer microspheres.
3 . The thermally expandable composition according to claim 1 , wherein the weight ratio of the amount of at least one chemical blowing agent CBA to the amount of the at least physical blowing agent PBA is in the range of 5:1 to 1:5.
4 . The thermally expandable composition according to claim 1 , wherein the at least one physical blowing agent PBA has an initiation expansion temperature in the range of 75-185° C.
5 . The thermally expandable composition according to claim 1 , wherein the at least one polymer P comprises 5-85 wt.-% of the total weight of the thermally expandable composition.
6 . The thermally expandable composition according to claim 1 , wherein the at least one filler F comprises 1.5-75 wt.-% of the total weight of the thermally expandable composition.
7 . The thermally expandable composition according to claim 1 , wherein the at least one filler F comprises at least one mineral filler MF and/or at least one cellulose-containing filler FW.
8 . The thermally expandable composition according to claim 1 , wherein the composition contains less than 0.25 wt.-% of epoxy resins having an average of more than one epoxy group per molecule, based on the total weight of the thermally expandable composition.
9 . The thermally expandable composition according to claim 1 , wherein the at least one polymer P is selected from the group consisting of ethylene vinyl acetate copolymers, polyolefins, olefin (meth)acrylate copolymers, olefin alkyl (meth)acrylate copolymers, and olefin (meth)acrylic acid copolymers.
10 . A damping element comprising a first layer composed of an expansion material and a second layer composed of an acoustic damping material,
wherein the expansion material has an expansion rate of at least 100%, and
wherein the acoustic damping material comprises:
b1) a bitumen component BC or a polymer component PC,
b2) at least one hydrocarbon resin HR,
b3) optionally at least one wax W,
b4) optionally at least one plasticizer PL, and
b5) At least 25 wt.-% based on the total weight of the acoustic damping material, of at least one solid particulate filler PF.
11 . The damping element according to claim 10 , wherein the expansion material in its non-expanded state is thermally activatable and has an activation temperature in the range of 85-225° C.
12 . The damping element according to claim 10 , wherein the expansion material comprises 5-85 wt.-% based on the total weight of the expansion material, of at least one polymer.
13 . The damping element according to claim 10 , wherein the expansion material comprises 1.5-70 wt.-% based on the total weight of the expansion material, of at least one filler.
14 . The damping element according to claim 10 , wherein the expansion material comprises in its non-expanded state at least one chemical foaming agent and/or at least one physical foaming agent.
15 . The damping element according to claim 10 , wherein the expansion material is composed of the thermally expandable composition in its expanded or non-expanded state.
16 . The damping element according to claim 15 , wherein the thermally expandable composition comprises:
a1) at least one polymer P,
a2) at least one chemical blowing agent CBA,
a3) at least one physical blowing agent PBA, and
a4) at least one filler F,
wherein the at least one physical blowing agent PBA is composed of expandable microspheres, and
wherein the thermally expandable composition is essentially free of epoxy resins having an average of more than one epoxy group per molecule.
17 . The damping element according to claim 10 , wherein the acoustic damping material comprises:
b1) 20-65 wt.-% of the bitumen component BC,
b2) 0.1-10 wt.-% of the at least one hydrocarbon resin HR, and
b3) 0-10 wt.-% of the at least one wax W, all the proportions being based on the total weight of the acoustic damping material.
18 . A transportation vehicle comprising the damping element according to claim 10 .
19 . A method for preparing a vibration and/or noise damped system comprising a structure having a noise emitting surface, the method comprising steps of:
I) providing a damping element according to claim 8 ,
II) applying the damping element to the noise emitting surface such that the first layer is arranged between the noise emitting surface and the second layer of the damping element.
20 . The method according to claim 19 , wherein the expansion material is in its non-expanded state and the method comprises a further step of expanding the first layer of the damping element by heating.
21 . The method according to claim 20 , wherein first layer of the damping element is expanded before or after the damping element has been applied to the noise emitting surface.
22 . The method according to claim 19 , wherein the structure is part of a transportation vehicle or a white good.
23 . A vibration and/or noise damped system comprising a structure having a noise emitting surface and a damping element according to claim 10 , wherein least a portion of the first major surface of the first layer is directly adhered to the noise emitting surface.
24 . A method for reinforcing a structure of a transportation vehicle, the method comprising steps of:
I′) providing an expansion material,
II′) applying the expansion material with a reinforcing layer to a surface of the structure such that the expansion material is arranged between the surface of the structure and the reinforcing layer, wherein
the expansion material is composed of the thermally expandable composition according to claim 1 in its expanded or non-expanded state.
25 . The method according to claim 24 , wherein the structure of the transportation vehicle is a roof element.