IP Library › Granted Patent US 12,522,891
Granted Patent B2
US 12,522,891 · App. 17/939,543 · Granted Jan 13, 2026

Method of recycling a component with rare earth element recovery

Inventor: Chuanbing Rong (Canton, MI)
Assignee: Ford Global Technologies, LLC
C22B59/00C22B7/006
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 12,522,891
App. No.
17/939,543
Granted
Jan 13, 2026
Kind
B2
Abstract

A method of recycling a component having a base structure and at least one body coupled to the base structure, wherein the body includes a rare earth element, includes positioning a mask over the component to produce a masked component. The mask is a material that is resistant to a liquid. The liquid is an acid or solvent and configured to dissolve the rare earth element. The mask covers the base structure to inhibit exposure of the base structure to the liquid. The mask defines at least one window aligned with the at least one body to expose the body to the liquid. The method includes dissolving the rare earth element into a solution by exposing the masked component to the liquid such that the liquid contacts the at least one body through the at least one window. The method further includes recovering the rare earth element from the solution.

Claims (33)

1 . A method of recycling a component that includes a base structure and at least one body coupled to the base structure, the at least one body comprising a rare earth element, the method comprising:

positioning a mask over the component to produce a masked component, the mask being a material that is resistant to a liquid, the liquid being an acid or solvent and configured to dissolve the rare earth element, wherein the mask covers the base structure to inhibit exposure of the base structure to the liquid, wherein the mask defines at least one window aligned with the at least one body to expose the body to the liquid;

dissolving the rare earth element into a solution by exposing the masked component to the liquid such that the liquid contacts the at least one body through the at least one window; and

recovering the rare earth element from the solution,

wherein the mask comprises at least one of Polytetrafluoroethylene, Polyvinyl chloride, and Polypropylene.

2 . The method according to claim 1 , wherein the component is a rotor or a stator of an electric motor and the at least one body includes a plurality of bodies disposed about a rotational axis of the component.

3 . The method according to claim 2 , wherein the base structure includes a plurality of laminated metal layers that cooperate to define a plurality of pockets, wherein each body of the plurality of bodies is a rare earth element magnet disposed within a corresponding one of the pockets.

4 . The method according to claim 3 , wherein the pockets are open to an exterior of the base structure through an axial end face of the base structure.

5 . The method according to claim 1 , wherein the base structure is steel.

6 . The method according to claim 1 , wherein the rare earth element is praseodymium, neodymium, samarium, terbium, dysprosium, holmium, lanthanum, or cerium.

7 . The method according to claim 1 , wherein the liquid has a pH that is less than or equal to 6.

8 . The method according to claim 7 , wherein the pH of the liquid is greater than or equal to 3.

9 . The method according to claim 1 , wherein the liquid comprises at least one of 0.1 M hydrochloric acid, 15 M nitric acid, 0.1 M to 1.0 M oxalic acid, and Di-(2-ethylhexyl) phosphoric acid.

10 . The method according to claim 1 , wherein exposing the masked component includes submerging at least a portion of the masked component in bath of the liquid.

11 . The method according to claim 10 , wherein exposing the masked component includes directing at least one jet of the liquid toward the at least one window to directly impinge on the at least one body.

12 . The method according to claim 11 , wherein the at least one jet is submerged in the bath.

13 . The method according to claim 1 , wherein exposing the masked component includes directing at least one jet of the liquid toward the at least one window to directly impinge on the at least one body.

14 . The method according to claim 1 , wherein recovering the rare earth element from the solution includes performing a reduction process.

15 . A method of recycling a component that includes a base structure and at least one body coupled to the base structure, the at least one body comprising a rare earth element, the method comprising:

positioning a mask over the component to produce a masked component, the mask being a material that is resistant to a liquid, the liquid being an acid or solvent and configured to dissolve the rare earth element, wherein the mask covers the base structure to inhibit exposure of the base structure to the liquid, wherein the mask defines at least one window aligned with the at least one body to expose the body to the liquid;

dissolving the rare earth element into a solution by directing at least one jet of the liquid toward the at least one window to directly impinge on the at least one body through the at least one window; and

recovering the rare earth element from the solution,

wherein the mask comprises at least one of Polytetrafluoroethylene, Polyvinyl chloride, and Polypropylene.

16 . The method according to claim 15 , wherein the at least one jet is submerged in a bath of the liquid.

17 . The method according to claim 15 , wherein the component is a rotor or a stator of an electric motor and the at least one body includes a plurality of bodies disposed about a rotational axis of the component.

18 . A method of recycling a component that includes a base structure and at least one body coupled to the base structure, the at least one body comprising a rare earth element, the method comprising:

positioning a mask over the component to produce a masked component, the mask being a material that is resistant to a liquid, the liquid being an acid or solvent and configured to dissolve the rare earth element, wherein the mask covers the base structure to inhibit exposure of the base structure to the liquid, wherein the mask defines at least one window aligned with the at least one body to expose the body to the liquid;

dissolving the rare earth element into a solution by exposing the masked component to the liquid such that the liquid contacts the at least one body through the at least one window; and

recovering the rare earth element from the solution,

wherein the component is a rotor or a stator of an electric motor and the at least one body includes a plurality of bodies disposed about a rotational axis of the component,

wherein the base structure includes a plurality of laminated metal layers that cooperate to define a plurality of pockets, wherein each body of the plurality of bodies is a rare earth element magnet disposed within a corresponding one of the pockets, and

wherein the mask comprises at least one of Polytetrafluoroethylene, Polyvinyl chloride, and Polypropylene.

19 . The method according to claim 18 , wherein exposing the masked component includes directing at least one jet of the liquid toward the at least one window to directly impinge on the at least one body.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Sep 14, 2022
From: RONG, CHUANBING
To: FORD GLOBAL TECHNOLOGIES, LLC
Reel/Frame 061089/0151 →
Continuity (1)
Related Publication 20240076760A1 · Mar 7, 2024
References Cited (9)
US 3749314A · Robinson · 1973 [cited by examiner]
US 10648063B2 · Mudring et al. · 2020 [cited by applicant]
US 11118245B2 · Berggren et al. · 2021 [cited by applicant]
US 11148957B2 · Le Breton et al. · 2021 [cited by applicant]
US 20150056427A1 · Guillemette · 2015 [cited by examiner]
US 20180119251A1 · Fox · 2018 [cited by examiner]
JP 2000324738A · 2000 [cited by examiner]
JP 2000-324738A Translation (Year: 2000). [cited by examiner]