Polyamide-based film, preparation method thereof, and cover window and display device comprising the same

Inventors: Dae Seong Oh (Gyeonggi-do, KR); Sun Hwan Kim (Gyeonggi-do, KR); Jin Woo Lee (Gyeonggi-do, KR)
Assignee: Microworks Solutions Co., Ltd.
C08G69/32B32B7/12B32B27/06B32B27/20B32B27/34B32B2307/4026B32B2307/414B32B2307/54B32B2307/732B32B2457/20
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 12,583,970
App. No.
17/852,006
Granted
Mar 24, 2026
Kind
B2
Abstract

The embodiments provide a polyamide-based film, which comprises a polyamide-based polymer and has an RSR A value of 3.4 m/N to 5.0 m/N as represented by the following Equation 1 based on the thickness of the film of 50 μm, and which is excellent in loop stiffness, static flexural characteristics, and folding characteristics while securing mechanical and optical properties at least a certain level, a process for preparing the same, and a cover window and a display device comprising the same. <Equation 1> RSR A =(RSR MD +RSR TD )/2 In Equation 1, RSR MD is the loop stiffness value measured with the MD direction of the film as the longitudinal direction at room temperature, and RSR TD is the loop stiffness value measured with the TD direction of the film as the longitudinal direction at room temperature.

Claims (35)

1 . A polyamide-based film, which comprises a polyamide-based polymer and has an RSR A value of 3.6 m/N to 5.0 m/N as represented by the following Equation 1 and an RSL A value of 3.7 m/N to 5.0 m/N as represented by the following Equation 2 based on the thickness of the film of 50 μm:

RSR A =(RSR MD +RSR TD )/2  <Equation 1>

in Equation 1, RSR MD is the loop stiffness value measured with the MD direction of the film as the longitudinal direction at room temperature, and RSR TD is the loop stiffness value measured with the TD direction of the film as the longitudinal direction at room temperature, wherein RSR MD is 3.35 m/N to 5.0 m/N, and RSR TD is 3.3 m/N to 5.0 m/N,

RSL A =(RSL MD +RSL TD )/2  <Equation 2>

in Equation 2, RSL MD is the loop stiffness value measured with the MD direction of the film as the longitudinal direction within 1 minute after the film is left at −20° C. for 2 hours, and RSL TD is the loop stiffness value measured with the TD direction of the film as the longitudinal direction within 1 minute after the film is left at −20° C. for 2 hours,

wherein the polyamide-based polymer comprises an imide-based repeat unit and an amide-based repeat unit at a molar ratio of 0:100 to 7:93,

wherein the film is manufactured by a method comprising,

polymerizing a diamine compound, a dicarbonyl compound, and, optionally, a dianhydride compound in an organic solvent to prepare a polyamide-based polymer solution;

casting the solution and then drying it to prepare a gel sheet; and

thermally treating the gel sheet,

wherein the step of thermally treating the gel sheet is carried out by fixing both ends of the gel sheet in the transverse direction with a fixing part, and thermally treating it while the width of the fixed gel sheet is changed,

wherein the step of thermally treating the gel sheet comprises first thermal treatment through hot air supplied by at least one hot air blower; and second thermal treatment through at least one heater, and

wherein when the section in which the first thermal treatment step is carried out is referred to as a first thermal treatment section,

the section in which the second thermal treatment step is carried out is referred to as a second thermal treatment section,

the maximum width of the gel sheet in the first thermal treatment section is referred to as Wa,

the minimum width of the gel sheet is in the first thermal treatment section is referred to as Wb,

the minimum width of the gel sheet in the first thermal treatment section and the second thermal treatment section is referred to as Wc, and

the Wb/Wa value is 0.955 to 0.990, and the Wc/Wa value is 0.950 to 0.990.

2 . The polyamide-based film of claim 1 , wherein when the film based on a thickness of 50 μm is folded to have a radius of curvature of 2 mm, which is then left at 25° C. for 24 hours, and the force applied to the film is released, the inner angle of the film is 140° or more.

3 . The polyamide-based film of claim 1 , which has a modulus of 5 GPa or more.

4 . The polyamide-based film of claim 1 , which has a transmittance of 80% or more, a haze of 1% or less, and a yellow index or 5 or less.

5 . The polyamide-based film of claim 1 , which further comprises at least one selected from the group consisting of a filler, a blue pigment, and a UVA absorber.

6 . A cover window, which comprises a polyamide-based film according to claim 1 and a functional layer, wherein the polyamide-based film comprises a polyamide-based polymer and has an RSR A value of 3.6 m/N to 5.0 m/N as represented by the following Equation 1 and an RSL A value of 3.7 m/N to 5.0 m/N as represented by the following Equation 2 based on the thickness of the film of 50 μm:

RSR A =(RSR MD +RSR TD )/2  <Equation 1>

in Equation 1, RSR MD is the loop stiffness value measured with the MD direction of the film as the longitudinal direction at room temperature, and RSR TD is the loop stiffness value measured with the TD direction of the film as the longitudinal direction at room temperature, wherein RSR MD is 3.35 m/N to 5.0 m/N, and RSR TD is 3.3 m/N to 5.0 m/N,

RSL A =(RSL MD +RSL TD )/2  <Equation 2>

in Equation 2, RSL MD is the loop stiffness value measured with the MD direction of the film as the longitudinal direction within 1 minute after the film is left at −20° C. for 2 hours, and RSL TD is the loop stiffness value measured with the TD direction of the film as the longitudinal direction within 1 minute after the film is left at −20° C. for 2 hours,

wherein the polyamide-based polymer comprises an imide-based repeat unit and an amide-based repeat unit at a molar ratio of 0:100 to 7:93.

7 . A display device, which comprises a display unit; and a cover window disposed on the display unit, wherein the cover window comprises a polyamide-based film according to claim 1 and a functional layer, and the polyamide-based film comprises a polyamide-based polymer and has an RSR A value of 3.6 m/N to 5.0 m/N as represented by the following Equation 1 and an RSL A value of 3.7 m/N to 5.0 m/N as represented by the following Equation 2 based on the thickness of the film of 50 μm:

RSR A =(RSR MD +RSR TD )/2  <Equation 1>

in Equation 1, RSR MD is the loop stiffness value measured with the MD direction of the film as the longitudinal direction at room temperature, and RSR TD is the loop stiffness value measured with the TD direction of the film as the longitudinal direction at room temperature, wherein RSR MD is 3.35 m/N to 5.0 m/N, and RSR TD is 3.3 m/N to 5.0 m/N,

RSL A =(RSL MD +RSL TD )/2  <Equation 2>

in Equation 2, RSL MD is the loop stiffness value measured with the MD direction of the film as the longitudinal direction within 1 minute after the film is left at −20° C. for 2 hours, and RSL TD is the loop stiffness value measured with the TD direction of the film as the longitudinal direction within 1 minute after the film is left at −20° C. for 2 hours,

wherein the polyamide-based polymer comprises an imide-based repeat unit and an amide-based repeat unit at a molar ratio of 0:100 to 7:93,

wherein RSR MD is 3.35 m/N to 5.0 m/N, and RSR TD is 3.3 m/N to 5.0 m/N.

Assignments (5)
CHANGE OF NAME Recorded Jan 15, 2026
From: SK MICROWORKS SOLUTIONS CO., LTD.
To: MICROWORKS SOLUTIONS CO., LTD.
Reel/Frame 074078/0923 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Apr 24, 2025
From: SK MICROWORKS CO., LTD.
To: SK MICROWORKS SOLUTIONS CO., LTD.
Reel/Frame 070929/0875 →
CORRECTIVE ASSIGNMENT TO CORRECT THE THE ASSIGNMENT DOCUMENT PREVIOUSLY RECORDED AT REEL: 063240 FRAME: 0192. ASSIGNOR(S) HEREBY CONFIRMS THE ASSIGNMENT. Recorded Dec 8, 2023
From: SKC CO., LTD.
To: SK MICROWORKS CO., LTD.
Reel/Frame 065841/0822 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Apr 3, 2023
From: SKC CO., LTD.
To: SK MICROWORKS CO., LTD.
Reel/Frame 063240/0192 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jun 28, 2022
From: OH, DAE SEONG; KIM, SUN HWAN; LEE, JIN WOO
To: SKC CO., LTD.
Reel/Frame 060341/0311 →
Priority Claims (1)
KR 10-2021-0115982 · Aug 31, 2021 · national
Continuity (1)
Related Publication 20230090709A1 · Mar 23, 2023
References Cited (18)
US 20190359772A1 · Kim · 2019 [cited by examiner]
US 20200407506A1 · Kim · 2020 [cited by examiner]
US 20200407519A1 · Ki · 2020 [cited by examiner]
US 20200407521A1 · Oh · 2020 [cited by examiner]
US 20200407522A1 · Choi · 2020 [cited by examiner]
US 20200409413A1 · Kim et al. · 2020 [cited by applicant]
US 20210246265A1 · Lee · 2021 [cited by examiner]
US 20210341971A1 · Park · 2021 [cited by examiner]
US 20220315702A1 · Park · 2022 [cited by examiner]
JP 2020003781A · 2020 [cited by applicant]
KR 1020190043458A · 2019 [cited by applicant]
KR 102147342B1 · 2020 [cited by examiner]
KR 1020210001845A · 2021 [cited by applicant]
WO WO2017200042A1 · 2017 [cited by examiner]
Dong, Yao, “The Effects of Processing Techniques on Mechanical Properties of Selected Polymers”, pp. 1-124, May 2013. [cited by examiner]
Office Action issued to the corresponding Japanese Patent Application No. 2022-115155, of which mailing date is Jul. 4, 2023. [cited by applicant]
Extended European Search Report for the European Patent Application No. 22192303.0 issued by the European Patent Office on Jan. 24, 2023. [cited by applicant]
Office Action for Korean Patent Application No. 10-2021-0115982 issued by the Korean Patent Office on Mar. 15, 2023. [cited by applicant]