IP Library › Granted Patent US 12,595,217
Granted Patent B2
US 12,595,217 · App. 18/367,926 · Granted Apr 7, 2026

Thermite block for stored-data destruction

Inventor: Carlo Scevola (Santo Domigo, DO)
C06B33/14C06B21/0033C06B31/02C06B33/02
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 12,595,217
App. No.
18/367,926
Granted
Apr 7, 2026
Kind
B2
Abstract

The invention is a multi-layer thermite block, encased in an exterior protective shield with one face exposed. The exposed face is carved out to accommodate a target device such that the block encompasses the target device when placed atop the device. When receiving a data-destruction signal, the block is ignited producing a short-duration blast of heat sufficient to severely damage or destroy all physical data-storing facilities of the target device.

Claims (50)

1 . A multi-layer thermite block comprising:

at least one ignition layer;

mixtures of constituent materials of the at least one ignition layer are bonded to form a solid slab of constituent ignition material;

a thermite layer;

mixtures of constituent materials in the thermite layer are bonded to form a solid slab of constituent thermite material;

layers interface via physical contact of slab faces;

interfacing layers are bonded to one another;

the multi-layer thermite block comprises a rectangular three-dimensional structure;

the rectangular three-dimensional structure is encased in an exterior protective shell;

wherein the exterior protective shell covers a top and all side faces of the multi-layer thermite block;

wherein the bottom face of the multi-layer thermite block, which is one face of the thermite layer, is exposed; and

a conducting wire is embedded in the at least one ignition layer with each end protruding from at least one edge of the at least one ignition layer.

2 . A claim as in claim 1 wherein:

the multi-layer thermite block comprises a single ignition layer and a two-layer-based thermite layer;

the single ignition layer comprises Potassium Nitrate (KNO 3 ) and powdered sugar (C 6 H 12 O 6 ) wherein constituent proportions, by percentage of single-ignition-layer weight, have a range of 55-70 percent and 30-45 percent, respectively;

the two-layer-based thermite layer comprises Vanadium (V) Oxide (V 2 O 5 ), Magnesium, and Barium Nitrate [Ba(NO 3 ) 2 ] wherein constituent proportions, by percentage of thermite layer weight, have a range of 40-55 percent, 25-35 percent and 10-30 percent, respectively;

the proportions, by weight, of the single ignition layer and single thermite layer to the multi-layer thermite block have a range of 4-10 percent and 90-96 percent; and

the conducting wire is embedded in the single ignition layer.

3 . A claim as in claim 1 wherein:

the multiple-layer thermite block comprises a first ignition layer, a second ignition layer, and a three-layer-based thermite layer:

the first ignition layer comprises Potassium Nitrate (KNO 3 ) and powdered sugar (C 6 H 12 O 6 ) wherein constituent proportions, by percentage of first-ignition-layer weight, have a range of 55-70 percent and 30-45 percent, respectively;

the second ignition layer comprises Barium Peroxide, Aluminum powder, and Magnesium powder wherein constituent proportions, by percentage of second-ignition-layer weight, have a range of 70-80 percent, 18-26 percent, and 2-12 percent, respectively;

the three-layer-based thermite layer comprises Iron (III) Oxide (Fe 2 O 3 ), Aluminum, and Barium Nitrate [(BaNO 3 ) 2 ] wherein constituent proportions, by percentage of thermite layer weight, have a range of 53 to 66 percent, 17-24 percent and 10-30 percent, respectively;

the proportions, by weight, of the first ignition layer, the second ignition layer, and the single thermite layer to the weight of the multi-layer thermite block have the range 3-5 percent, 2-4 percent and 91-95 percent, respectively; and

the conducting wire is embedded in the first ignition layer.

4 . A claim as in claim 1 wherein:

the conducting wire has a resistance range of 5-15 ohms.

5 . A claim as in claim 1 wherein:

the exterior protective shell's material comprises metal.

6 . A claim as in claim 1 wherein:

the exterior protective shell's material comprises ceramic.

7 . A claim as in claim 1 wherein:

the exterior protective shell's material comprises carbon fiber.

8 . A claims as in claim 1 wherein:

the exterior protective shell's material comprises graphite.

9 . A claim as in claim 1 further comprising:

the bottom face the multi-layer thermite block has a carve out operative to enable the multi-layer thermite block to encompass a target device such that the bottom face's periphery can make contact with a surface below the target device.

10 . A claim as in claim 1 further comprising:

an ignition controller subsystem.

11 . A claim as in claim 10 wherein:

the ignition controller subsystem operative to produce an output voltage sufficient to cause ignition when a destruct signal of logic 1 has been conveyed to the ignition controller's input.

12 . A claim as in claim 11 further comprising:

three redundant input gates conveying outputs to a three-input gate such that the output voltage sufficient to cause ignition will only be generated when two out of three inputs are logic 1 thereby enabling a triple-redundancy protection against single input-gate failure.

13 . A method of use comprising:

carving out a space from a bottom face of a multi-layer thermite block sufficient to encompass a target device;

applying a waterproofing adhesive to the bottom face's periphery operative to adhere to a surface below the target device so as to affix the block to the surface and provide protection against water intrusion;

placing the multi-layer thermite block atop the target device such that the target device is encompassed and the bottom face's periphery is in contact with the surface below the target device; and

allowing the waterproofing adhesive to cure.

14 . A method as in claim 13 further comprising:

attaching both ends of an embedded conductor protruding from at least one edge of an ignition layer to both output nodes of an ignition controller subsystem.

Continuity (1)
Related Publication 20250084011A1 · Mar 13, 2025
References Cited (14)
US 1082474A · Colman · 1913 [cited by applicant]
US 1148002A · Anderson · 1915 [cited by applicant]
US 6627013B2 · Carter, Jr. · 2003 [cited by examiner]
US 6928551B1 · Lee et al. · 2005 [cited by applicant]
US 8255620B2 · Frost et al. · 2012 [cited by applicant]
US 8461863B2 · Pedersen et al. · 2013 [cited by applicant]
US 8816717B2 · Fritz et al. · 2014 [cited by applicant]
US 8864924B2 · Coffey et al. · 2014 [cited by applicant]
US 9021333B1 · Northcott · 2015 [cited by applicant]
US 9471512B2 · Frost et al. · 2016 [cited by applicant]
US 9573858B1 · Brothers · 2017 [cited by examiner]
US 10724320B2 · Huang et al. · 2020 [cited by applicant]
US 20040205352A1 · Ohyama · 2004 [cited by applicant]
US 20090220088A1 · Lu et al. · 2009 [cited by applicant]